Materials and Corrosion in Light Water Reactors

被引:0
|
作者
Feron, Damien [1 ]
机构
[1] Univ Paris Saclay, CEA, Serv Rech Corros & Comportement Mat, Gif Sur Yvette, France
来源
CHALLENGES AND RECENT ADVANCEMENTS IN NUCLEAR ENERGY SYSTEMS, SCOPE 2023 | 2024年
关键词
Light Water Reactor; Zirconium; Carbon Steel; Stainless Steel; Nickel Base Alloy; Flow-Accelerated Corrosion; Stress Corrosion Cracking;
D O I
10.1007/978-3-031-64362-0_20
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
Since the beginning of nuclear industry, corrosion issues have been a major concern. Less than two years after start-up, stress corrosion cracking occurred on the stainless steel tubing of the steam generator of the prototype for the Nautilus in USA (1953); more recently, in 2022, several French Pressurized Water Reactors were shut down due to stress corrosion cracking of stainless steels pipes in a safety injection circuit. We propose to underline the complex corrosion mechanisms linked to the nuclear reactor environments (high temperature and high-pressure water environments) and to present briefly the three main corrosion phenomena occurring in Light Water Reactors (LWRs), after a short overview of the LWR materials: (i) general corrosion of zirconium cladding which limits the life-time of fuel elements to generally 3 cycles; (ii) flow-accelerated corrosion (FAC) of carbon steel components, which is the only corrosion phenomenon that has led to several deaths in LWRs; (iii) stress corrosion cracking (SCC) of nickel base alloys ("the Coriou effect") and of stainless steels including irradiation-assisted stress corrosion cracking; SCC of nickel base alloys has led to the replacement of major components like steam generators or pressurized vessel heads. Finally, the corrosion future will be discussed as LWRs are extending their period of operation up to 60 / 80 years, and even more.
引用
收藏
页码:187 / 197
页数:11
相关论文
共 50 条
  • [21] CORROSION IN PRESSURIZED-WATER REACTORS
    SAINTPAUL, P
    JOURNAL DE PHYSIQUE IV, 1993, 3 (C9): : 707 - 717
  • [22] Prediction of materials damage history from stress corrosion cracking in boiling water reactors
    Balachov, I
    Macdonald, D
    Stellwag, B
    Henzel, N
    Kilian, R
    JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 2000, 122 (01): : 45 - 49
  • [23] Uniform corrosion of FeCrAl cladding tubing for accident tolerant fuels in light water reactors
    Yin, Liang
    Jurewicz, T. B.
    Larsen, M.
    Drobnjak, M.
    Graff, C. C.
    Lutz, D. R.
    Rebak, R. B.
    JOURNAL OF NUCLEAR MATERIALS, 2021, 554
  • [24] IRRADIATION AND CORROSION BEHAVIOR OF CADMIUM ALUMINATE, A BURNABLE POISON FOR LIGHT WATER-REACTORS
    HATTENBACH, K
    AHLF, J
    HILGENDORFF, W
    ZIMMERMANN, HU
    ATOMKERNENERGIE, 1979, 33 (01): : 26 - 30
  • [26] IRRADIATION AND CORROSION BEHAVIOR OF CADMIUM ALUMINATE, A BURNABLE POISON FOR LIGHT WATER-REACTORS
    HATTENBACH, K
    AHLF, J
    HILGENDORFF, W
    ZIMMERMANN, HU
    ATOMKERNENERGIE-KERNTECHNIK, 1979, 33 (01): : 26 - 30
  • [27] Initial experimental evaluation of crud-resistant materials for light water reactors
    Dumnernchanvanit, I.
    Zhang, N. Q.
    Robertson, S.
    Delmore, A.
    Carlson, M. B.
    Hussey, D.
    Short, M. P.
    JOURNAL OF NUCLEAR MATERIALS, 2018, 498 : 1 - 8
  • [28] ENVIRONMENT SENSITIVE CRACKING IN PRESSURE BOUNDARY MATERIALS OF LIGHT WATER-REACTORS
    HANNINEN, H
    AHOMANTILA, I
    TORRONEN, K
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 1987, 30 (04) : 253 - 291
  • [29] REQUIREMENTS ON MATERIALS OF PRIMARY-CIRCUIT COMPONENTS OF LIGHT-WATER REACTORS
    ERNST, KR
    ATOMKERNENERGIE-KERNTECHNIK, 1980, 35 (03): : 225 - 227
  • [30] VALVES FOR LIGHT WATER REACTORS
    MORSDORF, S
    NUCLEAR ENGINEERING INTERNATIONAL, 1973, 18 (207): : 617 - 620