Microstructure and corrosion behavior of CrAl-coated 316L steel in static and flowing liquid lead-bismuth eutectic

被引:0
|
作者
Wang, Da [1 ]
Sun, Bihan [1 ]
Zhuo, Weiqian [2 ]
Ma, Xianfeng [1 ]
Zhu, Fei [1 ]
He, Xiujie [1 ]
Liang, Ruixian [3 ]
Liu, Sirui [1 ]
Xiao, Changquan [1 ]
Zhu, Wenjian [1 ]
机构
[1] Sun Yat Sen Univ, Sino French Inst Nucl Engn & Technol, Zhuhai 519082, Peoples R China
[2] Nucl Power Inst China, Sci & Technol Reactor Fuel & Mat Lab, Chengdu 610213, Peoples R China
[3] North China Elect Power Univ, Sch Nucl Sci & Engn, Beijing 102206, Peoples R China
关键词
CrAl coating; LBE; Corrosion resistance; Interface structure; TEM; MECHANICAL-PROPERTIES; OXIDATION RESISTANCE; T91; STEEL; COATINGS; SURFACE;
D O I
10.1016/j.vacuum.2025.114021
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To mitigate the corrosion issue of 316 L steel in lead-bismuth eutectic (LBE) cooled fast reactors, CrAl alloy coating was prepared on 316 L steel by multi-arc ion plating. Its corrosion behavior and microstructure evolution were examined in static and flowing LBE at different temperatures. The results show that the coating exhibited good bonding strength and corrosion resistance in LBE. The microstructure of coating experienced transformation in LBE at 550 degrees C while maintained stable at 350 degrees C. Under 550 degrees C, the coating transformed from Al3Cr7 with columnar grains to AlCr2 with refined equiaxed grains. Meanwhile, the enhanced element interdiffusion at interface of coating and steel also resulted in formation of B2-NiAl, Fe-Cr solid solution, Cr23C6 and (Al0.5Cr0.5)Fe. Although the CrAl coating has good anti-corrosion performance, the phase structure instability might limit its potential application.
引用
收藏
页数:15
相关论文
共 50 条
  • [21] Corrosion behavior of 410 stainless steel in flowing lead-bismuth eutectic alloy at 550 °C
    Chen, Gang
    Ju, Na
    Lei, Yucheng
    Wang, Dan
    Zhu, Qiang
    Li, Tianqing
    JOURNAL OF NUCLEAR MATERIALS, 2019, 522 : 168 - 183
  • [22] Corrosion Behavior of T91/316L Weld Seams with Different Chemical Compositions in 550℃ High-speed Flowing Liquid Lead-bismuth Eutectic Alloy
    Xiao L.
    Lei Y.
    Zhu Q.
    Li T.
    Chen G.
    Luo M.
    Zhao J.
    Chen W.
    Cailiao Daobao/Materials Reports, 2019, 33 (06): : 1805 - 1812
  • [23] Oxygen-enhanced dissolution corrosion of austenitic stainless steel 316 L in static lead-bismuth eutectic at 500 °C
    Maia, Eloa Lopes
    Tsybanev, Aleksandr
    Gavrilov, Serguei
    Tsisar, Valentyn
    Lim, Jun
    De Graeve, Iris
    CORROSION SCIENCE, 2024, 236
  • [24] Spectroscopic and microscopic investigation of the corrosion of 316/316L stainless steel by lead-bismuth eutectic (LBE) at elevated temperatures: importance of surface preparation
    Johnson, AL
    Parsons, D
    Manzerova, J
    Perry, DL
    Koury, D
    Hosterman, B
    Farley, JW
    JOURNAL OF NUCLEAR MATERIALS, 2004, 328 (2-3) : 88 - 96
  • [25] Corrosion behavior of steels in flowing lead-bismuth
    Barbier, F
    Rusanov, A
    JOURNAL OF NUCLEAR MATERIALS, 2001, 296 : 231 - 236
  • [26] Atomic-scale dissolution corrosion mechanism of additively-manufactured 316L steels in liquid lead-bismuth eutectic
    Gong, Xing
    Wan, Li
    Gao, Mingxin
    Auger, Thierry
    Chen, Kaiyun
    Wang, Pei
    Short, Michael P.
    Liu, Jing
    Luo, Jian
    ACTA MATERIALIA, 2025, 290
  • [27] Statistical analysis of the effect of lead-bismuth eutectic on fatigue resistance of 316L
    Solis, Noelia Olivia Fuentes
    Gavrilov, Serguei
    Stergar, Erich
    Seefeldt, Marc
    Wevers, Martine
    Marmy, Pierre
    NUCLEAR ENGINEERING AND DESIGN, 2023, 407
  • [28] Revealing fretting corrosion synergistic mechanism of 316 stainless steel in liquid lead-bismuth eutectic (LBE)
    Hua, Ke
    Cao, Yue
    Li, Na
    Tong, Yanlin
    Song, Yifan
    Zhang, Fan
    Li, Xiaolin
    Wu, Hongxing
    Wang, Haifeng
    CORROSION SCIENCE, 2023, 215
  • [29] Performance of the new ferritic/martensitic steel SIMP against liquid lead-bismuth eutectic corrosion: Comparison with T91 and 316L steels
    Ma, Zhiwei
    Shen, Tielong
    Zhou, Ting
    Wang, Zhiguang
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2023, 74 (02): : 221 - 232
  • [30] Analysis of 316L stainless steel pipe of lead-bismuth eutectic cooled thermo-hydraulic loop
    Rao, V. Shankar
    Lim, Jun
    Hwang, I. L. Soon
    ANNALS OF NUCLEAR ENERGY, 2012, 48 : 40 - 44