Stage division and discharge mechanism characterization of micro-arc oxidation based on acoustic emission

被引:0
|
作者
Bao, Fengyuan [1 ,3 ]
Li, Feng [1 ]
Bashkov, Oleg [2 ]
Wang, Zhiyuan [1 ]
Sun, Ling [4 ]
机构
[1] Harbin Univ Sci & Technol, Sch Mat Sci & Chem Engn, Harbin 150040, Peoples R China
[2] Komsomolsk Na Amure State Tech Univ, Komsomolsk On Amur 681013, Russia
[3] Weihai Zhenyu Intelligent Technol Co Ltd, Weihai 264204, Peoples R China
[4] Heilongjiang Polytech, Sch Informat Engn, Harbin 150080, Peoples R China
来源
基金
俄罗斯科学基金会;
关键词
Micro-arc oxidation; Acoustic emission; Aluminum alloy; T-SNE; Discharge; PLASMA ELECTROLYTIC OXIDATION; GROWTH; ALLOY; COATINGS; MICROSTRUCTURE; PEO;
D O I
10.1016/j.surfcoat.2025.131964
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Acoustic emission monitoring was conducted on the micro-arc oxidation process of the D16AT aluminum alloy plate with double-sided rolled pure aluminum in a silicate system electrolyte. Using the t-SNE algorithm, the recorded signals were classified based on the parameters of the acoustic emission signals. The analysis examined the regularities of the micro-arc oxidation stages under different current density conditions and their correspondence with signal characteristics and categories. Further discussion was held on the passivation and film formation mechanisms during the early, middle, and late stages of micro-arc oxidation. The effective film formation process of MAO was divided into four main stages: initial stage, weak micro-arc discharge, stable microarc discharge, and large arc discharge. Additionally, it included five sub-stages: conventional anodizing, weak glow discharge, transition from weak to strong glow discharge, transition from strong glow discharge to weak micro-arc discharge, and weak micro-arc discharge. The transition moments of these stages can be identified and determined by the frequency distribution of AE signals. As the current density increases, the discharge mechanism undergoes stage-wise changes. At different current densities, type-a signals primarily originate from gas glow discharge, while type-b signals are caused by breakdown at the bottom of the passivation film pores. Type-c signals mainly result from stable micro-arc discharge, and the increase in type-d signals marks the transition to a penetration-type strong discharge mechanism.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Characterization and corrosion behavior of ceramic coating on magnesium by micro-arc oxidation
    Durdu, Salih
    Aytac, Aylin
    Usta, Metin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (34) : 8601 - 8606
  • [32] Preparation and Characterization of Micro-Arc Oxidation Coating and Carbon Film on Titanium
    Yang Xiaokang
    Luo Binli
    Cai Jun
    Shuang Yixiang
    Wang Kuaishe
    RARE METAL MATERIALS AND ENGINEERING, 2020, 49 (08) : 2875 - 2879
  • [33] Micro-arc oxidation of β-titanium alloy: Structural characterization and osteoblast compatibility
    Chen, Hsien-Te
    Hsiao, Ching-Hung
    Long, Han-Yun
    Chung, Chi-Jen
    Tang, Chih-Hsin
    Chen, Keh-Chang
    He, Ju-Liang
    SURFACE & COATINGS TECHNOLOGY, 2009, 204 (6-7): : 1126 - 1131
  • [34] Optical emission spectroscopic determination of the optimum regions for micro-arc oxidation of titanium
    Chu, Hou Jen
    Liang, Chen-Jui
    Chen, Chien-Hui
    He, Ju-Liang
    SURFACE & COATINGS TECHNOLOGY, 2017, 325 : 166 - 173
  • [35] Characterization of Micro-arc Oxidized Titanium
    Inho Han
    Jai Hyuk Choi
    Hong Koo Baik
    In-Seop Lee
    JournalofWuhanUniversityofTechnology-MaterialsScience, 2005, (S1) : 178 - 180
  • [36] Effect of Electrolyte on Micro-arc Oxidation Discharge Mode and Wear Resistance of Titanium Alloy
    Zhang H.
    Xie F.-K.
    Liu Q.
    Surface Technology, 2023, 52 (08): : 216 - 225and236
  • [37] Influence of micro-arc oxidation discharge sparks on the surface roughness of aluminum alloy coating
    Liu, Xinghua
    Zhu, Liqun
    Liu, Huicong
    Li, Weiping
    Harbin Gongcheng Daxue Xuebao/Journal of Harbin Engineering University, 2014, 35 (04): : 510 - 515
  • [38] Recent Patents of Micro-arc Oxidation Technology
    Yuan M.
    Li Z.
    Recent Patents on Engineering, 2024, 18 (06) : 83 - 96
  • [39] Micro-arc oxidation of magnesium alloys: A review
    Yao, Wenhui
    Wu, Liang
    Wang, Jingfeng
    Jiang, Bin
    Zhang, Dingfei
    Serdechnova, Maria
    Shulha, Tatsiana
    Blawert, Carsten
    Zheludkevich, Mikhail L.
    Pan, Fusheng
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 118 : 158 - 180
  • [40] Electrophysical Model of the Micro-Arc Oxidation Process
    P. E. Golubkov
    E. A. Pecherskaya
    D. V. Artamonov
    T. O. Zinchenko
    Yu. E. Gerasimova
    N. V. Rozenberg
    Russian Physics Journal, 2020, 62 : 2137 - 2144