Stage division and discharge mechanism characterization of micro-arc oxidation based on acoustic emission

被引:0
|
作者
Bao, Fengyuan [1 ,3 ]
Li, Feng [1 ]
Bashkov, Oleg [2 ]
Wang, Zhiyuan [1 ]
Sun, Ling [4 ]
机构
[1] Harbin Univ Sci & Technol, Sch Mat Sci & Chem Engn, Harbin 150040, Peoples R China
[2] Komsomolsk Na Amure State Tech Univ, Komsomolsk On Amur 681013, Russia
[3] Weihai Zhenyu Intelligent Technol Co Ltd, Weihai 264204, Peoples R China
[4] Heilongjiang Polytech, Sch Informat Engn, Harbin 150080, Peoples R China
来源
基金
俄罗斯科学基金会;
关键词
Micro-arc oxidation; Acoustic emission; Aluminum alloy; T-SNE; Discharge; PLASMA ELECTROLYTIC OXIDATION; GROWTH; ALLOY; COATINGS; MICROSTRUCTURE; PEO;
D O I
10.1016/j.surfcoat.2025.131964
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Acoustic emission monitoring was conducted on the micro-arc oxidation process of the D16AT aluminum alloy plate with double-sided rolled pure aluminum in a silicate system electrolyte. Using the t-SNE algorithm, the recorded signals were classified based on the parameters of the acoustic emission signals. The analysis examined the regularities of the micro-arc oxidation stages under different current density conditions and their correspondence with signal characteristics and categories. Further discussion was held on the passivation and film formation mechanisms during the early, middle, and late stages of micro-arc oxidation. The effective film formation process of MAO was divided into four main stages: initial stage, weak micro-arc discharge, stable microarc discharge, and large arc discharge. Additionally, it included five sub-stages: conventional anodizing, weak glow discharge, transition from weak to strong glow discharge, transition from strong glow discharge to weak micro-arc discharge, and weak micro-arc discharge. The transition moments of these stages can be identified and determined by the frequency distribution of AE signals. As the current density increases, the discharge mechanism undergoes stage-wise changes. At different current densities, type-a signals primarily originate from gas glow discharge, while type-b signals are caused by breakdown at the bottom of the passivation film pores. Type-c signals mainly result from stable micro-arc discharge, and the increase in type-d signals marks the transition to a penetration-type strong discharge mechanism.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Micro-arc oxidation mechanism and electrical discharge model
    Chen, Hong
    Hao, Jian-Min
    Feng, Zhong-Xu
    Chang'an Daxue Xuebao (Ziran Kexue Ban)/Journal of Chang'an University (Natural Science Edition), 2008, 28 (05): : 116 - 119
  • [2] Discharge mechanism of ultrasound micro-arc oxidation on magnesium alloy
    李慕勤
    曲立杰
    马春力
    马臣
    王晶彦
    李海涛
    China Welding, 2015, 24 (02) : 30 - 34
  • [3] Discharge mechanism of ultrasound micro-arc oxidation on magnesium alloy
    State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, Harbin, China
    不详
    China Weld Eng Ed, 2 (30-34):
  • [5] Large-Arc Discharge Mechanism and Avoidance in Micro-Arc Oxidation of Magnesium Alloy
    Guan, Ke-Xin
    Yao, Jian-Tao
    Wang, Li-Shuang
    Dong, Hui
    METALS, 2022, 12 (06)
  • [6] Formation Mechanism of the Spark Discharge Plasma Source about Micro-Arc Oxidation
    Pan Mingqiang
    Di Shichun
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 : 333 - 338
  • [7] Local arc discharge mechanism and requirements of power supply in micro-arc oxidation of magnesium alloy
    Chen M.
    Ma Y.
    Hao Y.
    Frontiers of Mechanical Engineering in China, 2010, 5 (1): : 98 - 105
  • [8] Discharge characteristics of confined cathode micro-arc oxidation
    Zhang Xin-Meng
    Tian Xiu-Bo
    Gong Chun-Zhi
    Yang Shi-Qin
    ACTA PHYSICA SINICA, 2010, 59 (08) : 5613 - 5619
  • [9] Micro-arc oxidation
    Malyschev, V.
    Metalloberflache, 1995, 49 (08):
  • [10] Formation mechanism of HA-based coatings by micro-arc oxidation
    Han, Yong
    Sun, Jifeng
    Huang, Xin
    ELECTROCHEMISTRY COMMUNICATIONS, 2008, 10 (04) : 510 - 513