Optimized Laser Surface Remelting of 3D-Printed Ti6Al4V Manufactured Through Electron Beam MeltingOptimized Laser Surface Remelting of 3D-Printed Ti6Al4V Manufactured Through Electron Beam MeltingChen, Tsai, and Ou

被引:0
|
作者
Yi-Cheng Chen [1 ]
Meng-Hsiu Tsai [2 ]
Shih-Fu Ou [3 ]
机构
[1] Metal Industries Research & Development Centre,Department of Micro/Meso Mechanical Manufacturing R&D
[2] National Kaohsiung University of Science and Technology,Department of Mold and Die Engineering
[3] Kaohsiung Medical University,School of Dentistry, College of Dental Medicine
关键词
D O I
10.1007/s11837-024-06870-2
中图分类号
学科分类号
摘要
Laser surface remelting (LSR) has been employed to reduce the surface roughness of these 3D-printed products. However, the influences of LSR parameters such as defocus distance, stripe width, scanning number, and hatch distance on surface roughness have not been extensively investigated. Therefore, this study used the Taguchi method to identify optimized parameter settings for minimizing roughness of 3D-printed Ti6Al4V plates using LSR. In the initial phase of the Taguchi method, defocus distance, stripe width, and scanning number were considered. Among these factors, defocus distance had the strongest effect on reducing roughness, contributing 43.9%, followed by stripe width (21.6%) and scanning number (12.4%). The subsequent phase of analysis, which was conducted at a defocus distance of − 10 mm, included stripe width, scanning number, and hatch distance, which contributed 18.2%, 44.4%, and 25.5% of the surface roughness, respectively. The optimal conditions, namely a scanning number of 25, a defocus distance of − 10 mm, and a hatch distance of 0.004, resulted in the lowest surface roughness (Ra2.8 ± 0.3 μm), which was 86.6% lower than that observed for the as-received Ti6Al4V substrate (Ra20.95 ± 4.14 μm).
引用
收藏
页码:481 / 493
页数:12
相关论文
共 50 条
  • [31] Biotribocorrosion of 3D-printed silica-coated Ti6Al4V for load-bearing implants
    Ali Afrouzian
    Jose D. Avila
    Amit Bandyopadhyay
    Journal of Materials Research, 2021, 36 : 3974 - 3984
  • [32] 3D-printed Ti6Al4V scaffolds combined with pulse electromagnetic fields enhance osseointegration in osteoporosis
    Ye, Mingfu
    Liu, Wenjun
    Yan, Lihui
    Cheng, Shaolong
    Li, Xiaoxiong
    Qiao, Shichong
    MOLECULAR MEDICINE REPORTS, 2021, 23 (06)
  • [33] Performance of laser surface preparation of Ti6Al4V
    Cherif, M.
    Loumena, C.
    Jumel, J.
    Kling, R.
    3RD CIRP CONFERENCE ON SURFACE INTEGRITY, 2016, 45 : 311 - 314
  • [34] Laser Remelting of Ti6Al4V using High Power Diode Lasera
    Amaya-Vazquez, M. R.
    Sanchez-Amaya, J. M.
    Boukha, Z.
    El Amrani, K.
    Botana, F. J.
    4TH MANUFACTURING ENGINEERING SOCIETY INTERNATIONAL CONFERENCE (MESIC 2011), 2012, 1431 : 568 - 574
  • [35] Application of Laser Remelting Treatments to Improve the Properties of Ti6Al4V Alloy
    Amaya-Vazquez, M. R.
    Sanchez-Amaya, J. M.
    Boukha, Z.
    El Amrani, K.
    Botana, F. J.
    ADVANCES IN NON CONVENTIONAL MATERIALS PROCESSING TECHNOLOGIES, 2012, 713 : 25 - +
  • [36] Laser polishing of additive manufactured Ti6Al4V alloy: a review
    Li, Jiejing
    Zuo, Dunwen
    OPTICAL ENGINEERING, 2021, 60 (02)
  • [37] The effect of electron beam surface remelting on the wear behavior of Ti-6Al-4V by EBF3
    Sun, Shihao
    Qian, Ning
    Yao, Zhengjun
    Su, Honghua
    MATERIALS RESEARCH EXPRESS, 2022, 9 (12)
  • [38] Length scale parameters to estimate fatigue lifetime of 3D-printed titanium alloy Ti6Al4V containing notches in the as-manufactured condition
    Razavi, Nima
    Askes, H.
    Berto, F.
    Susmel, L.
    INTERNATIONAL JOURNAL OF FATIGUE, 2023, 167
  • [39] Effect Of Surface Roughness On The Fatigue Life Of Laser Additive Manufactured Ti6al4v Alloy
    Bača, Adrián
    Konečná, Radomila
    Nicoletto, Gianni
    Kunz, Ludvík
    Manufacturing Technology, 2015, 15 (04): : 4 - 4
  • [40] Fracture toughness of electron beam welded Ti6Al4V
    Rao, K. Prasad
    Angamuthu, K.
    Srinivasan, P. Bala
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2008, 199 (1-3) : 185 - 192