The 40Cr surface hardening mechanism by pre-stressed dry grinding

被引:0
|
作者
Chao, Caixia [1 ]
Zhang, He [2 ]
Sun, Cong [2 ]
Lin, Kaiyuan [2 ]
Wang, Xin [2 ]
Wang, Guanlong [2 ]
机构
[1] Quzhou Coll Technol, Quzhou 324002, Peoples R China
[2] Northeastern Univ, Sch Mech Engn & Automat, Shenyang 110819, Peoples R China
关键词
40Cr; Pre-stressed dry grinding; Non-Gaussian random function; High-performance manufacturing; SIMULATION; STEEL;
D O I
10.1007/s00170-025-15244-0
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
40Cr steel is one of the most widely used steels in machinery manufacturing. After tempering treatment, it has good mechanical properties and low-temperature impact toughness. In order to effectively improve the machining quality and surface integrity of the parts, a new machining technology, pre-stressed dry grinding, is proposed. The technology combines pre-stress grinding and hardened grinding technology in one, reasonable control of the surface stress state of the processed parts. It can change the sub-temperature quenching organization of the surface layer. Meanwhile, it has the characteristics of reducing energy consumption and conforming to green processing. In this paper, ANSYS software is used to analyze the specimen's temperature field simulation. Based on MATLAB, a non-Gaussian random function simulation is used to obtain the grinding wheel's surface with the final simulation of the surface trajectory model. The results show that with the increase of pre-stress, the surface quality of the specimen improved, and the defects, such as cracks and burns on the material's surface, are gradually reduced. Compared with the 45# steel, the Cr element hinders the growth of austenite grains and the transformation of austenite to large-grained pearlite. The metallographic organization of the hardened layer is refined and dense, and the surface roughness decreased by 38%. The study's results deepen the understanding of material removal and damage under the action of pre-stressed dry grinding technology, but the proposed method can also help realize high-performance manufacturing of 40Cr steel substrate surfaces.
引用
收藏
页码:1281 / 1292
页数:12
相关论文
共 50 条
  • [41] Effect of laser hardening modes on the hardening zone geometric parameters and tribological properties of 40Cr steel
    Starostin, D. A.
    Biryukov, V. P.
    Klevetov, D. V.
    Yudkin, V. F.
    INTERNATIONAL CONFERENCE OF YOUNG SCIENTISTS AND STUDENTS: TOPICAL PROBLEMS OF MECHANICAL ENGINEERING 2018, 2019, 489
  • [42] Experimental Investigation on High-speed Grinding of 40Cr Steel with Vitrified CBN Grinding Wheel
    Yu, Jianwu
    Chen, Tao
    Shang, Zhentao
    Sheng, Xiaomin
    Xie, Guizhi
    ADVANCES IN ABRASIVE TECHNOLOGY XIII, 2010, 126-128 : 154 - 158
  • [43] ON SURFACE-WAVES AND DEFORMATIONS IN A PRE-STRESSED INCOMPRESSIBLE ELASTIC SOLID
    DOWAIKH, MA
    OGDEN, RW
    IMA JOURNAL OF APPLIED MATHEMATICS, 1990, 44 (03) : 261 - 284
  • [44] Concrete beams strengthened with pre-stressed near surface mounted reinforcement
    Nordin, H
    Täljsten, B
    FIBRE-REINFORCEMENT POLYMER: REINFORCEMENT FOR CONCRETE STRUCTURES, VOLS 1 AND 2, PROCEEDINGS, 2003, : 1077 - 1086
  • [45] Effects of surface nanocrystallization pre-treatment on gas-nitriding behavior of 40Cr steel
    Ge, Li-Ling
    Lu, Cai-Hong
    Jing, Xiao-Tian
    Lu, Zheng-Xin
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2008, 29 (05): : 155 - 159
  • [46] The Vertical Bearing Mechanism of Hybrid Bored Pre-stressed Concrete Cased Piles
    Tang, Mengxiong
    Hu, Hesong
    Cui, Jie
    Yang, Xiaosong
    Hu, Han
    Chen, Hang
    INTERNATIONAL JOURNAL OF CIVIL ENGINEERING, 2020, 18 (3A) : 293 - 302
  • [47] PRE-STRESSED PLATES AS A MECHANISM TO PROVIDE ADDITIONAL UNDER BELLY BLAST PROTECTION
    Darrock, Louis
    Manning, Ashley
    Caine, Joe
    Beadle, James
    Peare, Alan
    Horsfall, Ian
    29TH INTERNATIONAL SYMPOSIUM ON BALLISTICS, VOLS 1 AND 2, 2016, : 1189 - 1194
  • [48] Effect of grinding wheel characteristics on the grind-hardened layer of 40Cr steel
    School of Mechanical Engineering, Jimei University, Xiamen 361021, China
    不详
    不详
    Jinshu Rechuli, 2006, 12 (56-58):
  • [49] Piezoelectric Pre-Stressed Bending Mechanism for Impact-Driven Energy Harvester
    Abdal, A. M.
    Leong, K. S.
    INTERNATIONAL TECHNICAL POSTGRADUATE CONFERENCE, 2017, 2017, 210
  • [50] Investigation on grinding-induced dynamic recrystallization behavior of 40Cr alloy steel
    Yao, Yunlong
    Xiu, Shichao
    Sun, Cong
    Kong, Xiangna
    Hong, Yuan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 867