Infrared spectroscopic study on residual chitosan-based composite seed coating in kaolin
被引:0
|作者:
Huang, Lanchun
[1
,2
]
Wu, Qian
[1
,2
]
Huang, Teng
[3
,4
]
Wang, Enwen
[1
,2
]
Kong, Desong
[3
]
Wang, Hai
[1
,2
]
机构:
[1] Anshun Univ, Sch Resources & Environm Engn, Anshun 561000, Peoples R China
[2] Anshun Univ, Res Ctr Rural Revitalizat, Anshun 561000, Peoples R China
[3] Southwest Univ Sci & Technol, Sch Environm & Resource, Mianyang 621010, Peoples R China
[4] Southwest Univ Sci & Technol, Key Lab Solid Waste Treatment & Resource Recycle, Minist Educ, Mianyang 621010, Peoples R China
来源:
关键词:
Chitosan-based composite seed coating;
Infrared spectroscopy;
Residues;
Temperature;
Salinity;
D O I:
10.1038/s41598-025-85805-6
中图分类号:
O [数理科学和化学];
P [天文学、地球科学];
Q [生物科学];
N [自然科学总论];
学科分类号:
07 ;
0710 ;
09 ;
摘要:
The decomposition of residual chitosan-based composite seed coating in kaolin under different temperatures and salinities is analyzed with a Fourier transform infrared spectroscopy (FT-IR). The degradation cycle is 28 days. The results show that a residue of the chitosan-based composite seed coating still exists in the kaolin on Day 7. From Day 7 to Day 14, the degradation rate of the chitosan-based composite seed coating is relatively slow. On Day 21, the chitosan-based composite seed coating is degraded entirely, and the degradation rate is quick during this period. However, the residue of this seed coating after degradation has a chemical action with the kaolin. On Day 28, the chitosan-based composite seed coating and residue aree wholly degraded in the kaolin. The chitosan-based composite seed coating can be completely degraded without residue. When the salinity of the kaolin is less than 1.0% under 0 -30 degrees C, its degradation rate and products will not be affected by temperature and salinity.