Microstructure, Corrosion Resistance and Tensile Properties of Modified Al-0.7Mn Alloy

被引:0
|
作者
Huang, YuanJiu [1 ]
Kang, Tae-Hoon [1 ]
Choi, Ho-Joon [2 ]
Shin, Young-Chul [2 ]
Lee, Seung-Cheol [3 ]
Lee, Kee-Ahn [1 ]
机构
[1] Inha Univ, Dept Mat Sci & Engn, Incheon 22212, South Korea
[2] Korea Inst Ind Technol, Incheon 21999, South Korea
[3] Daehan Air Conditioner Co LTD, Osan 18102, South Korea
来源
KOREAN JOURNAL OF METALS AND MATERIALS | 2024年 / 62卷 / 11期
关键词
Al3102; Modified Al-0.7Mn; Corrosion resistance; Tensile; Microstructure; Corrosion mechanism; ELECTROCHEMICAL-BEHAVIOR; MECHANICAL-PROPERTIES; ALUMINUM-ALLOYS; MN;
D O I
10.3365/KJMM.2024.62.11.886
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A modified alloy (Al-0.7Mn) was designed and fabricated with an increased Mn content up to 0.7wt.% and a controlled Fe content of 0.1wt.% and compared with the conventional Al3102 (Al-0.3Mn) alloy using the air-slip casting process. Both alloys were homogenized at 510 degrees C for 10 hours and then air-cooled. The microstructure, corrosion resistance, and mechanical properties of these materials were investigated. In the modified Al-0.7Mn alloy, the Mn/Fe ratios were found to be higher in both the alpha-Al matrix and the intermetallic compound of Al6(Mn, Fe) compared to those of the Al3102 alloy. Additionally, the size and volume fraction of the Al6(Mn, Fe) phase were relatively larger and higher in the modified Al-0.7Mn alloy, while the grain size of the alpha-Al matrix was significantly smaller. The galvanic corrosion test results indicated that the corrosion potential (E corr ) of the conventional Al3102 alloy was higher than that of the modified Al-0.7Mn alloy (Al-0.7Mn:-682.1mV, Al3102:-652.4mV). In contrast, the corrosion current (I corr ) and corrosion rate were measured to be 49.86 mu A and 0.541 mm/year for the Al-0.7Mn alloy, and 53.91 mu A and 0.585 mm/year for the Al3102 alloy, respectively. Thus, it was confirmed that the corrosion rate of the Al-0.7Mn alloy was slower compared to the conventional alloy, indicating better corrosion resistance. Room temperature tensile results showed that the tensile strengths of the modified and conventional alloys were 92.55 MPa and 78.39 MPa, respectively, demonstrating that the modified Al-0.7Mn alloy achieved higher strength without a significant decrease in ductility. This improvement is attributed to the higher Mn/Fe wt.% ratio in the Al6(Mn, Fe) phase of the modified Al-0.7Mn alloy, which can reduce the detrimental effect of Fe element and enhance the corrosion resistance. Additionally, the larger size and higher volume fraction of Al6(Mn, Fe) in the modified alloy, along with the smaller grain size, may contribute to the higher tensile strength. Based on these results, the corrosion mechanisms and deformation behavior of the modified Al0.7Mn alloy were also discussed.
引用
收藏
页码:886 / 896
页数:11
相关论文
共 50 条
  • [41] Effect of Mn-Bearing Dispersoids on Tensile Properties and Recrystallization Resistance of Al-3Mg-0.8Mn Rolled Alloy
    Algendy, Ahmed Y.
    Liu, Kun
    Chen, X. -Grant
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (19)
  • [42] Microstructure and mechanical properties of Al-Mg-Mn alloy with erbium
    Wang Xudong
    Lin Shuangping
    Yang Junjun
    Tang Zhenlei
    Nie Zuoren
    RARE METALS, 2012, 31 (03) : 237 - 243
  • [43] Microstructure and mechanical properties of Al-Mg-Mn alloy with erbium
    WANG Xudong a
    RareMetals, 2012, 31 (03) : 237 - 243
  • [44] Microstructure and mechanical properties of Al-Mg-Mn alloy with erbium
    Xudong Wang
    Shuangping Lin
    Junjun Yang
    Zhenlei Tang
    Zuoren Nie
    Rare Metals, 2012, 31 : 237 - 243
  • [45] Microstructure and tensile properties of magnesium alloy modified by Si/Ca based refiner
    Duan, ZC
    Sun, YS
    Wei, Y
    Du, WW
    Xue, F
    Zhu, TB
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2005, 15 (04) : 878 - 883
  • [46] Densification, microstructure and properties of Sc and Zr modified Al-Mn alloy prepared by selective laser melting
    Du, Lei
    Ke, Linda
    Xiao, Meili
    Dou, Enhui
    Luo, Zhiqiang
    Chen, Yi
    Lai, Caifang
    OPTICS AND LASER TECHNOLOGY, 2022, 148
  • [47] Microstructure and tensile properties of magnesium alloy modified by Si/Ca based refiner
    段志超
    孙扬善
    魏宇
    杜温文
    薛烽
    诸天柏
    TransactionsofNonferrousMetalsSocietyofChina, 2005, (04) : 878 - 883
  • [48] Effects of ultrasonic vibration on the microstructure and corrosion properties of the 7046 Al alloy
    Qiu, Yang
    Li, Xintao
    Huang, Huilan
    Liu, Mingyang
    Xia, Peng
    Luo, Yajun
    Zhou, Nan
    VACUUM, 2022, 205
  • [49] Effects of Al Addition on Tensile Properties and Aqueous Corrosion Behavior of Cantor Alloy
    Baolin Pang
    Man Wang
    Tanying Liu
    Xiaoli Xi
    Journal of Materials Engineering and Performance, 2022, 31 : 5602 - 5610
  • [50] Effects of Al Addition on Tensile Properties and Aqueous Corrosion Behavior of Cantor Alloy
    Pang, Baolin
    Wang, Man
    Liu, Tanying
    Xi, Xiaoli
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (07) : 5602 - 5610