Research on Failure Pressure of API 5L X100 Pipeline with Single Defect

被引:0
|
作者
Wang Z. [1 ]
Duan W. [1 ]
Long M. [1 ]
Wang A. [1 ]
Li X. [2 ]
机构
[1] Shaanxi Key Laboratory of Low Metamorphic Coal Clean Utilization, Yulin University, Yulin
[2] Key Laboratory of Fluid Transmission Technology of Zhejiang Province, Zhejiang Sci-Tech University, Hangzhou
基金
中国国家自然科学基金;
关键词
anti-corrosion layer; corrosiveness; exactitude; failure pressure; Single defect; stress cloud diagram;
D O I
10.2174/0124055204294716240306065810
中图分类号
学科分类号
摘要
Background: With the continuous application of API 5L X100 high-strength grade steel pipeline and the development trend of increasing pipeline diameter and design pressure in China's long natural gas and petroleum pipeline, API 5L X100 high-strength grade steel pipeline steel is bound to become the aorta in long-distance pipeline construction in the future. Studying the failure pressure of API 5L X100 high-strength grade steel pipeline has high economic and social benefits. Objective: Exploring the corrosion mechanism of the two single corroded pipeline models with outer defect and inner defect. Methods: Using ANSYS Workbench 15.0 software to explore the two single corroded pipeline models with outer defect and inner defect and the influence of geometric parameters such as defect depth, defect length, defect width, etc., on the maximum equivalent stress and failure pressure investigated. Based on the finite element analysis database, the failure pressures of two single corroded pipeline models were fitted using Matlab software and the fitting formulas. Results: In the corrosion defect area of the pipeline, stress concentration occurs; Far away from the corrosion defect area, the stress distribution is uniform. For the pipeline model with outer defect and inner defect, as the defect depth and length increases, failure pressure shows a decreasing trend and is almost unaffected by defect width; As the ratio of diameter to thickness increases, failure pressure shows a decreasing trend; By fitting failure pressure formula of the pipeline models with outer defect and inner defect, a multivariate fitting function formula of failure pressure is obtained, with high fitting exactitude. Conclusion: The conclusion obtained have certain guiding values for the normal and stable operation of natural gas and petroleum transportation pipelines. © 2024 Bentham Science Publishers.
引用
收藏
页码:134 / 155
页数:21
相关论文
共 50 条
  • [31] INFLUENCE OF SANDBLASTING AND HYDROGEN ON TENSILE AND FATIGUE PROPERTIES OF PIPELINE API 5L X52 STEEL
    Alhussein, Akram
    Capelle, Julien
    Gilgert, Joseph
    Dominiak, Serge
    Azari, Zitouni
    STRUCTURAL INTEGRITY AND LIFE-INTEGRITET I VEK KONSTRUKCIJA, 2011, 11 (03): : 195 - 204
  • [32] Influence of sandblasting and hydrogen on tensile and fatigue properties of pipeline API 5L X52 steel
    Alhussein, A.
    Capelle, J.
    Gilgert, J.
    Dominiak, S.
    Azari, Z.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2011, 36 (03) : 2291 - 2301
  • [33] EBSD Microstructural studies on quenched-tempered API 5L X65 pipeline steel
    Ohaeri, Enyinnaya G.
    Jack, Tonye
    Yadav, Sandeep
    Szpunar, Jerzy
    Zhang, Jiming
    Qu, Jinbo
    PHILOSOPHICAL MAGAZINE, 2021, 101 (17) : 1895 - 1912
  • [34] SURFACE MORPHOLOGY OF API 5L X65 PIPELINE STEEL PROCESSED BY ULTRASONIC IMPACT PEENING
    Haque, M. Merajul
    Yeh, Li-Hsin
    Zhang, Xing
    Li, Beiwen
    Liao, Yiliang
    PROCEEDINGS OF ASME 2023 18TH INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE, MSEC2023, VOL 2, 2023,
  • [35] Inhibition of corrosion on API 5L X52 pipeline steel in acid media by Tradescantia spathacea
    Rodriguez-Torres, Adriana
    Valladares-Cisneros, Maria Guadalupe
    Chavez-Diaz, German
    Martinez-Calzada, Victor
    Saldana-Heredia, Alonso
    FRONTIERS IN CHEMISTRY, 2024, 12
  • [36] Microstructural Evaluation of API 5L X80 Pipeline Steels Submitted to Different Cooling Rates
    Bott, I. S.
    Vieira, A. A. H.
    de Souza, L. F. G.
    Rios, P. R.
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 3146 - +
  • [37] Development of an API 5L X-70 grade steel for sour gas resistance pipeline application
    Mendoza, R
    Huante, J
    Camacho, V
    Alvarez-Fregoso, O
    Juarez-Islas, JA
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1999, 8 (05) : 549 - 555
  • [38] Development of an API 5L X-70 grade steel for sour gas resistance pipeline application
    Mendoza R.
    Huante J.
    Camacho V.
    Alvarez-Fregoso O.
    Juarez-Islas J.A.
    Journal of Materials Engineering and Performance, 1999, 8 (5) : 549 - 555
  • [39] Effects of alternating current interference on the cathodic protection for API 5L X60 pipeline steel
    Guo, Yanbao
    Tan, Hai
    Meng, Tao
    Wang, Deguo
    Liu, Shuhai
    JOURNAL OF NATURAL GAS SCIENCE AND ENGINEERING, 2016, 36 : 414 - 423
  • [40] Static, dynamic and fatigue characteristics of the pipeline API 5L X52 steel after sandblasting
    Alhussein, A.
    Capelle, J.
    Gilgert, J.
    Tidu, A.
    Hariri, S.
    Azari, Z.
    ENGINEERING FAILURE ANALYSIS, 2013, 27 : 1 - 15