Unveiling the Degradation Mechanism of Polymer-Based Thermal Interface Materials Under Thermo-Oxidative Condition

被引:0
|
作者
Wu, Yongdong [1 ]
He, Bin [2 ]
Fang, Jingyuan [3 ]
Hu, Yuqi [2 ]
Zeng, Xiaoliang [1 ]
Ren, Linlin [1 ]
Sun, Rong [1 ]
机构
[1] Chinese Acad Sci, Shenzhen Inst Adv Elect Mat, Shenzhen Inst Adv Technol, Shenzhen 518055, Peoples R China
[2] Chinese Acad Sci, Shenzhen Inst Adv Elect Mat, Shenzhen 518055, Peoples R China
[3] Guilin Univ Technol, Key Lab Nonferrous Mat & New Proc Technol, Guilin 541004, Peoples R China
基金
中国国家自然科学基金;
关键词
Aging; Degradation; Thermal degradation; Thermal conductivity; Polymers; Young's modulus; Temperature; Thermal interface materials; thermo-oxidative aging mechanism; thermal conductivity; aging; PERFORMANCE;
D O I
10.1109/TDMR.2024.3442781
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
With the growing power density and miniaturization of electronic devices, their thermal management and reliability are becoming more and more important. Polymer-based thermal interface materials, which are used to fill the gap between chip and heat sink, play an important role for the heat dissipation, but their reliability is rarely studied in academia, especially under thermo-oxidative condition. Here, a polymer-based thermal interface material, highly filled thermal conductive gel, is used as a model to study the degradation mechanism under thermo-oxidative condition. The results show that aging mainly deteriorates the mechanical performance instead of its intrinsic thermal conductivity. The elongation at break of aged sample is reduced and the corresponding modulus is increased as a function of aging time. Relaxation spectra indicate that the relaxation time of aged sample increases. The longer relaxation time of aged sample is attributed to the chain scission and oxidation of alky chain at interface and the depolymerization of polydimethylsiloxane chain, resulting in a more crosslinked polymer network. Thus, both interfacial aging and depolymerization of polymers contribute to the slowdown of polymer chain dynamics and degradation of mechanical properties. This work provides an insight into the degradation mechanism of thermal interface materials and guides the development of high-reliability thermal interface materials.
引用
收藏
页码:514 / 521
页数:8
相关论文
共 50 条
  • [21] Thermal and thermo-oxidative degradation of polystyrene in the presence of ammonium sulfate
    Zhu, XS
    Elomaa, M
    Sundholm, F
    Lochmuller, CH
    MACROMOLECULAR CHEMISTRY AND PHYSICS, 1997, 198 (10) : 3137 - 3148
  • [22] Understanding of thermal/thermo-oxidative degradation kinetics of polythiophene nanoparticles
    Omid Zabihi
    Aminreza Khodabandeh
    Journal of Thermal Analysis and Calorimetry, 2013, 112 : 1507 - 1513
  • [23] Structural effects of phenols on the thermal and thermo-oxidative degradation of polybenzoxazines
    Low, HY
    Ishida, H
    POLYMER, 1999, 40 (15) : 4365 - 4376
  • [24] An assessment of the role of morphology in thermal/thermo-oxidative degradation mechanism of PP/EVA/clay nanocomposites
    Goodarzi, Vahabodin
    Jafari, Seyed Hassan
    Khonakdar, Hossein Ali
    Monemian, Seyed Ali
    Mortazavi, Mehdi
    POLYMER DEGRADATION AND STABILITY, 2010, 95 (05) : 859 - 869
  • [25] MECHANISM OF INHIBITION OF THERMAL AND THERMO-OXIDATIVE DEGRADATION OF POLYMERS BY POLYARYLENE ALKYLENES AND POLYMERIC HYDROCARBONS.
    Shopov, I.
    Polymer science USSR, 1985, 27 (01): : 213 - 219
  • [26] Rheological Characterization of Thermal, Thermo-Oxidative and Photo-Oxidative Degradation of LDPE
    Rolon-Garrido, Victor Hugo
    Wagner, Manfred Hermann
    NOVEL TRENDS IN RHEOLOGY VI, 2015, 1662
  • [27] Thermal interface polymer-based composites materials: a critical review
    Abbas, Mesum
    Septevani, Athanasia Amanda
    Yurid, Fitra
    Joshi, Ankit
    Gupta, Madhulika
    Rangappa, Sanjay Mavinkere
    Madhu, G. M.
    Sriariyanun, Malinee
    Siengchin, Suchart
    Baranitharan, P.
    MULTISCALE AND MULTIDISCIPLINARY MODELING EXPERIMENTS AND DESIGN, 2025, 8 (03)
  • [28] Thermal extraction combined with thermal desorption: A powerful tool to investigate the thermo-oxidative degradation of polyamide 66 materials
    Duemichen, E.
    Braun, U.
    Kraemer, R.
    Deglmann, P.
    Senz, R.
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2015, 115 : 288 - 298
  • [29] Kinetics of the thermal and thermo-oxidative degradation of a polystyrene-clay nanocomposite
    Vyazovkin, S
    Dranca, I
    Fan, XW
    Advincula, R
    MACROMOLECULAR RAPID COMMUNICATIONS, 2004, 25 (03) : 498 - 503
  • [30] Kinetic analysis of thermal and thermo-oxidative degradation of polyethylene (nano)composites
    Siročić, A.P. (apticek@fkit.hr), 1600, Taylor and Francis Ltd. (21):