KINETICS OF THE REDUCTION OF FeO IN CaO-SiO2 SLAG WITH SOLID CARBON.

被引:0
|
作者
Sasaki, Yasushi
Soma, Tanekazu
机构
关键词
D O I
10.2355/tetsutohagane1955.64.3_376
中图分类号
TF [冶金工业]; TG14 [金属材料];
学科分类号
0806 ;
摘要
The testing temperature ranged from 1400 degree C to 1600 degree C and basicity (CaO/SiO//2) from 0. 5 to 2. 0. The reduction rate is independent of the FeO concentration in the range of reduction of 30% to 80%. Reduction takes place in the form of indirect reduction in which CO as reductant is consumed and regenerated by solid carbon. The controlling step is gasification. CaO increases the reduction rate.
引用
收藏
页码:376 / 384
相关论文
共 50 条
  • [31] RATE OF FEO REDUCTION FROM A CAO-SIO2-AL2O3 SLAG BY CARBON-SATURATED IRON
    PHILBROOK, WO
    KIRKBRIDE, LD
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1956, 206 (03): : 351 - 356
  • [32] Oxidation Kinetics and Mechanism of Boron in Metallurgical-Grade Silicon Melt by CaO-SiO2 Slag Refining
    He, Qian
    He, Naiyong
    Yang, Ding
    Wu, Jijun
    Wei, Kuixian
    Ma, Wenhui
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2022, 53 (03): : 1841 - 1850
  • [33] Oxidation Kinetics and Mechanism of Boron in Metallurgical-Grade Silicon Melt by CaO-SiO2 Slag Refining
    Qian He
    Naiyong He
    Ding Yang
    Jijun Wu
    Kuixian Wei
    Wenhui Ma
    Metallurgical and Materials Transactions B, 2022, 53 : 1841 - 1850
  • [34] Reduction smelting on bismuth oxide residue in FeO-SiO2-CaO ternary slag system
    Zhang Du-chao
    Zhang Xin-wang
    Yang Tian-zu
    Wen Jian-feng
    Liu Wei-feng
    Chen Lin
    Rao Shuai
    Xiao Qing-kai
    Hao Zhan-dong
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2016, 23 (06) : 1326 - 1331
  • [35] Reduction smelting on bismuth oxide residue in FeO-SiO2-CaO ternary slag system
    Du-chao Zhang
    Xin-wang Zhang
    Tian-zu Yang
    Jian-feng Wen
    Wei-feng Liu
    Lin Chen
    Shuai Rao
    Qing-kai Xiao
    Zhan-dong Hao
    Journal of Central South University, 2016, 23 : 1326 - 1331
  • [36] Reduction smelting on bismuth oxide residue in FeO-SiO2-CaO ternary slag system
    张杜超
    张新望
    杨天足
    文剑锋
    刘伟锋
    陈霖
    饶帅
    肖庆凯
    郝占东
    Journal of Central South University, 2016, 23 (06) : 1326 - 1331
  • [37] Measurement of hydrogen reduction rates of FeO in 2FeO•SiO2 and CaO•FeO•SiO2
    Ono-Nakazato, H
    Tsubone, Y
    Takaki, Y
    Usui, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (05): : 320 - 326
  • [38] THERMODYNAMICS OF THE CAO-SIO2 SYSTEM
    LEE, YE
    CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 1982, 6 (04): : 283 - 291
  • [39] KINETICS OF WATER VAPOR DISSOLUTION IN LIQUID CaO-SiO2 AND CaO-SiO2-TiO2 SLAGS.
    Ban-Ya, Shiro
    Iguchi, Yasutaka
    Yamamoto, Seiji
    Kang T'ieh/Iron and Steel (Peking), 1985, 20 (10): : 31 - 37
  • [40] AN ASSESSMENT OF THE CAO-SIO2 SYSTEM
    HILLERT, M
    SUNDMAN, B
    WANG, XZ
    METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1990, 21 (02): : 303 - 312