STRAIN AND FRACTURE OF LIQUID-PHASE SINTERED ALLOY 90W-7Ni-3Fe.

被引:0
|
作者
Du, Jiaju
Shi, Yuanlong
机构
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
It was found that the matrix of the alloy is the first to yield and to undergo plastic deformation. Cracks may be initiated along the W grain/matrix interfaces as the bonding force there is weak. While the bonding force is strengthened to a greater extent than the cleavage failure stress of W, the transgranular cleavage cracking of W grains and the plastic tearing of the matrix may happen simultaneously. Hydrogen is shown as one of the main sources of the interfacial embrittlement of as-sintered specimens. The removal of the hydrogen both stored in the voids and dissolved in metals of the W grain/matrix interfaces is easily done by heat treatment under vacuum.
引用
收藏
相关论文
共 50 条
  • [32] Transient Liquid-Phase Sintering Characteristic of W-Ni-Fe Alloy via Microwave-Assisted Heating
    Ma Yunzhu
    Zhang Jiajia
    Liu Wensheng
    Zhao Yaxu
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (09) : 2108 - 2111
  • [33] Preparation of 90W-7Ni-3Fe Heavy Alloy Sheet by Tape-casting
    Li Bangyi
    Wu Fang
    Zhang Jing
    Feng Jian
    Shao Jiajun
    Zhu Yubin
    RARE METAL MATERIALS AND ENGINEERING, 2019, 48 (08) : 2616 - 2622
  • [34] Preparation of 90W-7Ni-3Fe Heavy Alloy Sheet by Tape-casting
    Li, Bangyi
    Wu, Fang
    Zhang, Jing
    Feng, Jian
    Shao, Jiajun
    Zhu, Yubin
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2019, 48 (08): : 2616 - 2622
  • [35] Densification behaviour, microstructural characteristics and mechanical properties of liquid phase sintered W-2Ni-1Fe alloy
    Majumdar, Sanjib
    Kishor, Jugal
    Paul, Bhaskar
    Kain, Vivekanand
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 818
  • [36] HIGH-STRAIN RATE PROPERTIES OF 3 LIQUID-PHASE SINTERED TUNGSTEN ALLOYS
    CIMPOERU, SJ
    WOODWARD, RL
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1990, 9 (02) : 187 - 191
  • [37] Effect of Fe7W6 Phase (μ-phase) on Mechanical Properties of W-Ni-Fe Heavy Alloy
    Jeon, Yong Jin
    Kim, Se Hoon
    Kim, Young Do
    KOREAN JOURNAL OF METALS AND MATERIALS, 2011, 49 (09): : 720 - 725
  • [38] INFLUENCE OF THE SINTERING TIME ON PROPERTIES AND FRACTURE-BEHAVIOR OF LIQUID-PHASE SINTERED W-HEAVY METALS
    DANNINGER, H
    PISAN, W
    JANGG, G
    LUX, B
    ZEITSCHRIFT FUR METALLKUNDE, 1983, 74 (03): : 151 - 155
  • [39] Substitution of Ni with NiB prevents shape distortion of liquid phase sintered 90W-6Ni-2Fe-2Co heavy alloys
    Sengupta, P.
    Panigrahi, A.
    Indoria, B.
    Meher, P.
    Acharya, T. S.
    Basu, S.
    Debata, M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 840
  • [40] Dynamic Strength of Heavy 90W-7Ni-3Fe Alloy Produced by Spark Plasma Sintering
    Bragov, A. M.
    Chuvildeev, V. N.
    Melekhin, N. V.
    Filippov, A. R.
    Konstantinov, A. Yu.
    Sakharov, N. V.
    PHYSICAL MESOMECHANICS, 2019, 22 (04) : 307 - 312