ELASTIC/PLASTIC INDENTATION IN CERAMICS: A FRACTURE TOUGHNESS DETERMINATION METHOD.

被引:84
|
作者
Miranzo, P. [1 ]
Moya, J.S. [1 ]
机构
[1] Inst de Ceramica y Vidrio, Madrid, Spain, Inst de Ceramica y Vidrio, Madrid, Spain
关键词
MATERIALS TESTING - Notched Bar;
D O I
10.1016/0272-8842(84)90005-1
中图分类号
学科分类号
摘要
An extensive literature survey of the evolution of the indentation technique is made. The elastic/plastic solution for the spherical cavity expansion is used to obtain a physical explanation for the quantitative measurement of the radial cracks that occur at the indentation impression corners. Finally an expression based on the mentioned theory is given. Experimental data from a series of brittle materials are well fitted by this expression.
引用
收藏
页码:147 / 152
相关论文
共 50 条
  • [41] Determination of Interfacial Fracture Toughness of Thermal Spray Coatings by Indentation
    Yasuhiro Yamazaki
    Masayuki Arai
    Yukio Miyashita
    Hiroyuki Waki
    Masato Suzuki
    Journal of Thermal Spray Technology, 2013, 22 : 1358 - 1365
  • [42] Determination of Interfacial Fracture Toughness of Thermal Spray Coatings by Indentation
    Yamazaki, Yasuhiro
    Arai, Masayuki
    Miyashita, Yukio
    Waki, Hiroyuki
    Suzuki, Masato
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2013, 22 (08) : 1358 - 1365
  • [43] Elastic modulus, indentation pressure and fracture toughness of hybrid coatings on glass
    Malzbender, J
    de With, G
    den Toonder, JMJ
    THIN SOLID FILMS, 2000, 366 (1-2) : 139 - 149
  • [44] Determination of fracture toughness of zirconia ceramics with different yttria concentrations by SEVNB method
    Liu, Hao
    Zhao, Wei
    Ji, Yi
    Cui, Jinping
    Chu, Yanhui
    Rao, Pinggen
    CERAMICS INTERNATIONAL, 2017, 43 (13) : 10572 - 10575
  • [45] Fracture sequences during elastic–plastic indentation of brittle materials
    Robert F. Cook
    Journal of Materials Research, 2019, 34 : 1633 - 1644
  • [46] Determination of dynamic fracture initiation toughness of elastic-plastic materials at intermediate strain rates
    Fernández-Sáez, J
    de Luna, S
    Rubio, L
    Pérez-Castellanos, JL
    Navarro, C
    REVISTA DE METALURGIA, 2001, 37 (03) : 459 - 469
  • [47] FRACTURE TOUGHNESS DETERMINATIONS BY INDENTATION
    EVANS, AG
    CHARLES, EA
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1976, 59 (7-8) : 371 - 372
  • [48] METHOD FOR DETERMINATION THE TOUGHNESS OF PLASTIC PRODUCTS
    SON, AT
    KUNSTSTOFFE-GERMAN PLASTICS, 1980, 70 (12): : 844 - 849
  • [49] Dual-tip elastic indentation:: A new technique for controlled crack growth and brittle fracture toughness determination
    Martín-Meizoso, A
    Martínez-Esnaola, JM
    Gil-Sevillano, J
    INTERNATIONAL JOURNAL OF FRACTURE, 2001, 110 (02) : L17 - L22
  • [50] Preparation and elastic-plastic indentation response of MgAlON transparent ceramics
    Zhang, Wei
    Wang, Yuezhong
    Chen, Jian
    Jiang, Ruomei
    Shi, Zitao
    Yang, Guojian
    Hu, Weiyin
    Xu, Qiang
    Xie, Xiumin
    Tan, Yang
    Huang, Shuai
    Zhang, Zhibin
    Song, Hai-Zhi
    CERAMICS INTERNATIONAL, 2022, 48 (01) : 855 - 863