Development of ultra-clean plasma deposition process

被引:0
|
作者
Kamei, Toshihiro [1 ]
Matsuda, Akihisa [1 ]
机构
[1] Thin Film Silicon Solar Cells Superlab, Electroteclmical Laboratory, 1-1-4 Umezono Tsukuba 3058568, Japan
关键词
Amorphous silicon - Degassing - Degradation - Grain size and shape - Hydrogenation - Partial pressure - Photochemical reactions - Purification - Secondary ion mass spectrometry;
D O I
暂无
中图分类号
学科分类号
摘要
We have developed a new type of ultra-high vacuum plasma-enhanced chemical vapor deposition (UHV/PECVD) system. According to high sensitivity secondary ion mass spectrometry, device quality hydrogenated amorphous silicon (a-Si:H) films deposited at 250°C at a deposition rate of 1 angstrom/s contains 1015 cm-3 of O, 1015 cm-3 of C, and 1014 cm-3 of N impurities, while low defect hydrogenated microcrystalline silicon (μc-Si:H) films deposited at 200°C at a very low rate of 0.1 angstrom/s include 1016 cm-3 of O, 1015 cm-3 of C and 1016 cm-3 of N. These are the lowest concentrations of atmospheric contaminants for these kinds of materials observed so far. The essential features of the present UHV/PECVD system are an extremely low outgassing rate of 8 × 10-9 Torr·l/s, extremely low partial pressure of contaminant gas species -12 Torr, and purification of feed gas SiH4 at 'point of use'. These efforts are quite important not only for clarifying the microscopic mechanism of photo-induced degradation in a-Si:H, but also for enlarging the crystalline grain size in μc-Si:H. μc-Si:H with a grain size of ≈ 1000 angstrom as determined by Scherrer's formula can be obtained at the higher rate of 1.5 angstrom/s by utilizing a VHF (Very High Frequency) plasma. The specific origins of impurities in the films are also discussed.
引用
收藏
页码:19 / 24
相关论文
共 50 条
  • [42] Denveloping efficient charges for making ultra-clean steel
    Zhul'ev, SI
    Guzenkov, SA
    Sergeev, VI
    Bod, KY
    METALLURGIST, 2003, 47 (9-10) : 401 - 404
  • [43] Thermodynamics on control of inclusions composition in ultra-clean steels
    Suito, H
    Inoue, R
    ISIJ INTERNATIONAL, 1996, 36 (05) : 528 - 536
  • [44] Advanced cleaning strategies for ultra-clean silicon surfaces
    Heyns, M
    Bearda, T
    Cornelissen, I
    De Gendt, S
    Loewenstein, L
    Mertens, P
    Mertens, S
    Meuris, M
    Schaekers, M
    Teerlinck, I
    Vos, R
    Wolke, K
    CLEANING TECHNOLOGY IN SEMICONDUCTOR DEVICE MANUFACTURING, 2000, 99 (36): : 3 - 16
  • [45] Preparation of advanced activated carbon with ultra-clean coals
    Yang, QW
    Zhu, SQ
    Liu, LJ
    Wang, ZN
    PROSPECTS FOR COAL SCIENCE IN THE 21ST CENTURY, 1999, : 1045 - 1048
  • [47] State-of-the-art evaluation of ultra-clean ULSI processes
    FischerColbrie, A
    Laderman, SS
    Brennan, S
    Ghosh, S
    Takaura, N
    Pianetta, P
    Shimazaki, A
    Waldhauer, A
    Wherry, D
    Barkan, S
    SCIENCE AND TECHNOLOGY OF SEMICONDUCTOR SURFACE PREPARATION, 1997, 477 : 403 - 407
  • [48] Polishing of ultra-clean inner surfaces using magnetic force
    Kim, J.-D. (jdkim@sejong.ac.kr), 1600, Springer-Verlag London Ltd (21):
  • [49] Polishing of ultra-clean inner surfaces using magnetic force
    Kim, JD
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2003, 21 (02): : 91 - 97
  • [50] Evaluation of the mechanical properties and corrosion behaviour of ultra-clean steels
    Mendoza, R
    Alanis, M
    Huante, J
    Gonzalez-Rivera, G
    Juarez-Islas, JA
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2000, 101 (1-3) : 238 - 244