The room temperature tensile and fracture behaviour of super α2 have been assessed as a function of a range of thermomechanical treatments. It has been shown that the best properties are obtained in samples which have been forged in the β phase field using cool dies, followed by aging at 800 °C for 2 h. These property measurements have been correlated with the microstructural changes caused by the various heat treatments. It has been found that the highest strength is associated with a two-phase structure of transformed β phase containing about 17% primary α2 and that improved fracture behaviour is associated with a transformed fine Windmanstatten structure. It is concluded that the room temperature tensile ductility improved by aging at 800 °C for 2 h, which reduces the dislocation density and the stress concentration caused by the heavy forging deformation within the α2 and B2 grains. Grain boundary α2 films and the high Nb interface α2 phases at primary α2 and B2 matrix interfaces form after high temperature solution treatments. Also, these two kinds of α2 phase result in low room temperature tensile ductility. Grain boundary strengthening plays a dominant role in super α2, and transgranular fracture is the main failure feature of this alloy.
引用
收藏
页码:23 / 35
相关论文
共 50 条
  • [41] A comparative study of the strain rate and temperature dependent compression behavior of Ti-46.5Al-3Nb-2Cr-0.2W and Ti-25Al-10Nb-3V-1Mo intermetallic alloys
    Vaidya, RU
    Jin, Z
    Cady, C
    Gray, GT
    Butt, DP
    SCRIPTA MATERIALIA, 1999, 41 (06) : 569 - 574
  • [42] MECHANICAL-PROPERTIES OF POWDER-METALLURGY TI-829 AND TI-25AL-10NB-3V-1MO PRODUCED BY RAPID OMNIDIRECTIONAL COMPACTION
    OSBORNE, NR
    PORTER, WJ
    EYLON, D
    SAMPE QUARTERLY-SOCIETY FOR THE ADVANCEMENT OF MATERIAL AND PROCESS ENGINEERING, 1991, 22 (04): : 21 - 28
  • [43] Ti-25Al-10Nb-3V-1Mo合金的高周疲劳性能及断裂特征
    曹京霞
    孙福生
    曹春晓
    高扬
    材料工程, 1997, (05) : 12 - 14
  • [44] Effect of Cooling Rate on Microstructure of Alloy Ti3Al-10Nb-3V-1Mo
    张启海
    周光爵
    邬彦如
    RareMetals, 1997, (04) : 48 - 53
  • [45] 渗氢对Ti-25Al-10Nb-3V-1Mo锻态合金显微组织的影响
    董林
    董林
    张彩碚
    张彩碚
    丁桦
    孙伟
    赵志
    材料研究学报, 2000, (S1) : 63 - 67
  • [46] TEM investigations of the fibre/matrix interface in SCS-6 Sic/Ti-25Al-10Nb-3V-1Mo composites
    Yang, YQ
    Dudek, HJ
    Kumpfert, J
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1998, 29 (9-10) : 1235 - 1241
  • [47] Microstructures and High Temperature Tensile Properties of Ti-43Al-4Nb-1.5Mo Alloy in the Canned Forging and Heat Treatment Process
    Li Tianrui
    Liu Guohuai
    Xu Mang
    Niu Hongzhi
    Fu Tianliang
    Wang Zhaodong
    Wang Guodong
    ACTA METALLURGICA SINICA, 2017, 53 (09) : 1055 - 1064
  • [48] 锻造Ti-25Al-10Nb-3V-1Mo(超α2)合金的塑变特征及显微组织发展
    张廷杰
    钛工业进展, 1995, (05) : 39 - 39
  • [49] 氢对锻态Ti-25Al-10Nb-3V-1Mo合金热压缩行为的影响
    张勇,张少卿,陶春虎
    中国有色金属学报, 1996, (01) : 84 - 88