PROPERTIES OF WELDED JOINTS IN LOW-CARBON AND LOW-ALLOY STEELS PRODUCED BY CO2 PLASMA WELDING.

被引:0
|
作者
Shepelev, A.F.
Bozhenko, B.L.
Akulov, A.I.
机构
关键词
WELDING - Steel - WELDS - Mechanical Properties;
D O I
暂无
中图分类号
学科分类号
摘要
In CO//2 plasma welding with filler wire, the high losses of deoxidizing elements may cause the formation, on the surface of the weld metal, of a slag with a high content of iron oxides which impairs the separability of the slag crust. The main losses of alloying elements in CO//2 plasma welding occur in the droplet formation stage. In comparison with consumable electrode welding, the role of the pool stage is considerably more important. To produce sound alloyed welded joints, welding should be carried out at a speed of more than 30 m/hr at a ratio of the plasma arc current to the cross-sectional area of the shaping nozzle of less than 8 multiplied by 10**6 A/m**2, and the filler wire should be fed in the directions in which its melting takes place in the pool within the limits of the current-conducting channel of the arc column.
引用
收藏
页码:23 / 26
相关论文
共 50 条
  • [31] DEPENDENCE OF THE STRENGTH OF LOW-CARBON LOW-ALLOY STEELS ON THE COOLING RATE
    BANNYKH, OA
    ONUCHIN, LG
    RUSSIAN METALLURGY, 1984, (01): : 72 - 77
  • [32] MORPHOLOGY OF CARBONITRIDES AND HOT DUCTILITY OF LOW-CARBON LOW-ALLOY STEELS
    MAEHARA, Y
    YASUMOTO, K
    TOMONO, H
    OHMORI, Y
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 27 (03) : 222 - 228
  • [33] EFFECT OF STRUCTURE ON FRACTURE CHARACTERISTICS OF LOW-CARBON, LOW-ALLOY STEELS
    FRIDMAN, ZG
    GORITSKII, VM
    KHROMOV, DP
    LOBZOV, MG
    RUSSIAN METALLURGY, 1986, (01): : 155 - 159
  • [34] HARDENABILITY OF BORON-TREATED LOW-CARBON LOW-ALLOY STEELS
    OHMORI, Y
    YAMANAKA, K
    JOURNAL OF METALS, 1979, 31 (08): : F30 - F31
  • [35] EFFECT OF NIOBIUM ON COLD RESISTANCE OF LOW-CARBON AND LOW-ALLOY STEELS
    NIKITIN, VN
    YAKOVLEVA, EF
    METAL SCIENCE AND HEAT TREATMENT, 1978, 20 (1-2) : 15 - 18
  • [36] Some Features of Sulfide Cracking of Low-Alloy and Low-Carbon Steels
    Melekhov, R. K.
    Smiyan, O. D.
    Karvats'kyi, L. M.
    Kapinos, L. V.
    Materials Science, 31 (02):
  • [37] Influence of Nanomodification on the Microstructure of the Metal of Welded Joints of Low-Alloy Steels
    Golovko, V. V.
    Kostin, V. A.
    Zhukov, V. V.
    MATERIALS SCIENCE, 2024, 59 (06) : 762 - 769
  • [38] MULTIPLE REPAIR OF WELDED-JOINTS IN LOW-CARBON STEELS
    KOZULIN, MG
    WELDING PRODUCTION, 1977, 24 (06): : 52 - 54
  • [39] Effect of Ce on the microstructure, mechanical properties and dislocation state in low-carbon low-alloy steels
    Song, Chenghao
    Xie, Zongzheng
    Zhang, Zhenshan
    Wang, Haoliang
    Sun, Zhenzhong
    Yang, Yuhui
    Yu, Hao
    Cheng, Jun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 927
  • [40] Changes in the structure and properties of low-carbon low-alloy pipe steels upon inoculation with REM
    Denisova, T. V.
    Vyboishchik, M. A.
    Tetyueva, T. V.
    Ioffe, A. V.
    METAL SCIENCE AND HEAT TREATMENT, 2013, 54 (9-10) : 530 - 534