MICROSTRUCTURE OF Fe-Cr-C HARDFACING ALLOYS WITH ADDITIONS OF Nb, Ti AND, B.

被引:0
|
作者
Berns, H. [1 ]
Fischer, A. [1 ]
机构
[1] Ruhr Univ, Bochum, West Ger, Ruhr Univ, Bochum, West Ger
来源
Metallography | 1987年 / 20卷 / 04期
关键词
BORIDES - CARBIDES - Microstructure - IRON AND ALLOYS - Abrasion Resistance - PROTECTIVE COATINGS - WELDING;
D O I
暂无
中图分类号
学科分类号
摘要
The abrasive wear of machine parts and tools used in the mining, earth moving, and transporting of mineral materials can be lowered by filler wire welding of hardfacing alloys. In this paper, the microstructures of Fe-Cr-C and Fe-Cr-C-Nb/Ti hardfacing alloys and deposits and those of newly developed Fe-Cr-C-B and Fe-Ti-Cr-C-B ones are described. They show up to 85 vol. % of primarily solidified coarse hard phases; i. e. , carbides of MC-, M//7C//3-, M//3C-type and borides of MB//2-, M//3B//2-, M//2B-, M//3B-, M//2//3B//6-type, which are embedded in a hard eutectic. This itself consists of eutectic hard phases and a martensitic or austenitic metal matrix. The newly developed Fe-Cr-C-B alloys reach hardness values of up to 1200 HV and are harder than all purchased ones. The primary solidification of the MB//2-type phase of titanium requires such high amounts of titanium and boron that these alloys are not practical for manufacture as commercial filler wires.
引用
收藏
页码:401 / 429
相关论文
共 50 条
  • [21] The Effect of Microstructure on Properties of Fe-Cr-C-Nb/Ti Hardfacing Alloy
    Tang, Wenbo
    Guo, Yungang
    Wang, Hongrui
    MECHANICS, SOLID STATE AND ENGINEERING MATERIALS, 2011, 279 : 126 - 131
  • [22] The Microstructure and Abrasive Wear Resistance of Fe-Cr-C Hardfacing Alloys with the Composition of Hypoeutectic, Eutectic, and Hypereutectic at Cr/C=6
    Sabet, H.
    Khierandish, Sh
    Mirdamadi, Sh
    Goodarzi, M.
    TRIBOLOGY LETTERS, 2011, 44 (02) : 237 - 245
  • [23] Microstructure and wear resistance of Fe-Cr-B-C hardfacing alloys
    Gong, Jian-Xun
    Li, Dan
    Xiao, Yi-Feng
    Zhang, Qing-Hui
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2010, 31 (03): : 136 - 141
  • [24] Effect of TiN on microstructure and wear resistance of Fe-Cr-C hardfacing alloy
    Liu Z.
    Li D.
    Wang W.
    Su Y.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (10): : 15 - 19
  • [25] Optimal Design for Fe-Cr-C Hardfacing Alloys with Anti-Wearing
    Yuan, Tao
    Luo, Zhen
    Wang, Rui
    MANUFACTURING PROCESS TECHNOLOGY, PTS 1-5, 2011, 189-193 : 3545 - +
  • [26] Wear Regimes of Fe-Cr-C Hardfacing Alloys in Microscale Abrasion Tests
    Colaco, Fernando H. G.
    Pintaude, Giuseppe
    TRIBOLOGY LETTERS, 2022, 70 (02)
  • [27] Microstructures and properties of Fe-Cr-C hardfacing alloys with high carbon content
    Wang, Qing-Bao
    Wang, Zhi-Hui
    Li, Shi-Min
    Hanjie Xuebao/Transactions of the China Welding Institution, 2004, 25 (06): : 119 - 123
  • [28] Effects of B contents on the microstructure and wear resistance of hypereutectic Fe-Cr-C hardfacing alloy coating
    Wang, Jibo
    Lu, Jianxiang
    Xing, Xiaolei
    Zhou, Yefei
    Liu, Shaocun
    Qi, Xiaowen
    Yang, Qingxiang
    MATERIALS RESEARCH EXPRESS, 2019, 6 (10)
  • [29] Effects of Graphite Additions on Microstructures and Wear Resistance of Fe-Cr-C-Nb Hardfacing Alloys
    Huang, Fei
    Ren, Zhen'an
    Liu, Wumu
    Chen, Hanlin
    Zheng, Siqiang
    MATERIALS SCIENCE-MEDZIAGOTYRA, 2017, 23 (03): : 233 - 237
  • [30] Influence of microstructure on micro-abrasive wear resistance of alloys Fe-Cr-C and Fe-Cr-C-Nb
    de Oliveira, Tatiane Gabi
    da Costa, Adilson Rodrigues
    MATERIA-RIO DE JANEIRO, 2019, 24 (01):