Microstructure characteristics of high undercooled bulk nanocrystalline Fe-B-Si eutectic alloy

被引:0
|
作者
Zhang, Zhenzhong
Song, Guangsheng
Yang, Gencang
Zhou, Yaohe
机构
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
By applying cyclical superheating incorporated with glass fluxing denucleation method, the maximum undercooling of 367 K was obtained for 6 - 20 g Fe76B12Si12 eutectic bulk liquid alloy. Using high undercooling and quenching the high undercooled alloy into water, nanocrystalline bulk Fe76B12Si12 eutectic alloy with 11 mm in diameter, 10 mm in height and average particles size of about 200 nm has been prepared. It has been found that the microstructures vary with preparing conditions. For the sample triggered at 367 K undercooling after recalescence by the cooling rate of 4 K/s cooling to room temperature and for the sample triggered at 329 K undercooling after recalescence and quenching, the microstructure consists of 30 - 400 nm α-Fe(Si) particles distributed uniformly in the refined Fe2B(Si) matrix, whereas for the sample triggered at 354 K undercooling in the process of recalescence and quenching, the microstructure consists of 30 - 350 nm Fe2B(Si) particles distributed uniformly in the α-Fe(Si) matrix. The radial microstructure difference can be improved by increasing the initial undercooling and cooling rate. The reasons of microstructure refined to nanometer level were discussed.
引用
收藏
页码:693 / 697
相关论文
共 50 条
  • [31] RECALESCENCE EFFECT SIMULATION AND MICROSTRUCTURE EVOLUTION OF UNDERCOOLED Fe82B17Si1 ALLOY
    Chen Zheng
    Yang Yanan
    Chen Qiang
    Xu Junfeng
    Tang Yueyue
    Liu Feng
    ACTA METALLURGICA SINICA, 2014, 50 (07) : 795 - 801
  • [32] Characteristics of Fe-Si-B-P-Cu Nanocrystalline Soft Magnetic Alloy Powders With High Bs
    Chiba, Miho
    Urata, Akiri
    Matsumoto, Hiroyuki
    Yoshida, Shigeyoshi
    Makino, Akihiro
    IEEE TRANSACTIONS ON MAGNETICS, 2011, 47 (10) : 2845 - 2847
  • [33] Effect of Microadditional Cerium on Annealing Embrittlement of Fe-B-Si Amorphous Alloy
    曹兴国
    车晓舟
    戴礼智
    JOURNAL OF RARE EARTHS, 1996, (01) : 30 - 35
  • [34] Competitions incorporated in rapid solidification of the bulk undercooled eutectic Ni78.6Si21.4 alloy
    Liu, Feng
    Chen, Yuzeng
    Yang, Gencang
    Lu, Yiping
    Chen, Zheng
    Zhou, Yaohe
    JOURNAL OF MATERIALS RESEARCH, 2007, 22 (10) : 2953 - 2963
  • [35] Competitions incorporated in rapid solidification of the bulk undercooled eutectic Ni78.6Si21.4 alloy
    Feng Liu
    Yuzeng Chen
    Gencang Yang
    Yiping Lu
    Zheng Chen
    Yaohe Zhou
    Journal of Materials Research, 2007, 22 : 2953 - 2963
  • [36] JOULE HEATING ANNEALING OF AMORPHOUS FE-B-SI ALLOY DOPED WITH CERIUM
    HUANG, DR
    TSAI, CL
    LI, JCM
    JOURNAL OF METALS, 1988, 40 (07): : A62 - A62
  • [37] Growth morphology of Ni3Si in high undercooled Ni-Si eutectic alloy
    Xi, Zengzhe
    Yang, Gencang
    Zhou, Yaohe
    Progress in Natural Science, 1997, 7 (05): : 630 - 631
  • [38] Growth morphology of Ni3Si in high undercooled Ni-Si eutectic alloy
    惠增哲
    杨根仓
    周尧和
    ProgressinNaturalScience, 1997, (05) : 114 - 121