Friction and wear behavior of electrodeposited amorphous Fe-Co-W alloy deposits

被引:0
|
作者
He, Feng-Jiao [1 ]
Lei, Jing-Tian [1 ]
Lu, Xin [2 ]
Huang, Yu-Ning [2 ]
机构
[1] Coll. of Chem. and Chem. Eng., Hunan Univ., Changsha 410082, China
[2] Yingcai Technol. Co. Ltd., Changsha 410006, China
来源
Transactions of Nonferrous Metals Society of China (English Edition) | 2004年 / 14卷 / 05期
关键词
Amorphous alloys - Chromium alloys - Cobalt alloys - Electrodeposition - Friction - Heat treatment - Tungsten alloys - Wear of materials - Wear resistance;
D O I
暂无
中图分类号
学科分类号
摘要
The microstructures, friction and wear behavior under dry sliding condition of electrodeposited amorphous Fe-Co-W alloy deposits heat treated at different temperatures were studied. A comparative study of hard chrome deposit under the same testing condition was also made. The experimental results show that the hardness and wear resistance of amorphous Fe-Co-W alloy deposits are improved with the increasing of heat treatment temperature, and reach the maximum value at 800°C, then decrease above 800°C. Under 40 N load, the wear resistance properties of the alloy deposits heat treated at 800°C are superior to those of hard chrome deposit. The main wear mechanisms of amorphous Fe-Co-W alloy deposits heat treated below 600°C are peeling, plastic and flowing deformation; when the deposits are heat treated above 700°C, they are plastic and flowing deformation. While the main wear mechanisms of hard chrome are abrasive wear, fatigue and peeling.
引用
收藏
页码:901 / 906
相关论文
共 50 条
  • [21] Composition, Morphology, and Topography of Galvanic Coatings Fe-Co-W and Fe-Co-Mo
    Yermolenko, Iryna Yu.
    Ved, Maryna V.
    Sakhnenko, Nykolay D.
    Sachanova, Yulya I.
    NANOSCALE RESEARCH LETTERS, 2017, 12
  • [22] Friction and wear properties of HVAF sprayed Fe-based amorphous alloy coatings
    Wei, Xian-Shun, 2018, Chongqing Wujiu Periodicals Press (47):
  • [23] Coupled Electrodeposition of Fe-Co-W Alloys: Thin Films and Nanowires
    Maliar, Tatjana
    Cesiulis, Henrikas
    Podlaha, Elizabeth J.
    FRONTIERS IN CHEMISTRY, 2019, 7
  • [24] EFFECT OF CARBON ON PHASE COMPOSITION AND PROPERTIES OF FE-CO-W ALLOYS
    BROSTREM, VA
    KREMNEV, LS
    METAL SCIENCE AND HEAT TREATMENT, 1974, 16 (9-10) : 750 - 754
  • [25] AMORPHIZATION OF ELECTRODEPOSITED FE-W ALLOY-FILMS AND ELECTROCHEMICAL-BEHAVIOR
    RUAN, YF
    YAO, SW
    KOWAKA, M
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 1990, 117 : 752 - 755
  • [26] EFFECT OF COBALT ON AGING OF MARTENSITE AND FERRITE IN FE-CO-W AND FE-CO-MO ALLOYS
    EDNERAL, AF
    ZHUKOV, OP
    PERKAS, MD
    METAL SCIENCE AND HEAT TREATMENT, 1974, 16 (9-10) : 840 - 843
  • [27] Improvement in the Wear Resistance under Dry Friction of Electrodeposited Fe-W Coatings through Heat Treatments
    Mulone, Antonio
    Nicolenco, Aliona
    Imaz, Naroa
    Martinez-Nogues, Vanesa
    Tsyntsaru, Natalia
    Cesiulis, Henrikas
    Klement, Uta
    COATINGS, 2019, 9 (02):
  • [28] Development of Fe-Co-W alloys as cathode materials for fuel cell application
    Ramesh, L
    Sheshadri, BS
    Mayanna, SM
    TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 1998, 76 : 101 - 104
  • [29] KINETICS AND MECHANISM OF DISPERSION HARDENING OF DEPOSITED METAL OF SYSTEMS FE-CO-W AND FE-CO-MO
    DEMYANTSEVICH, VP
    KRYZHANOVSKII, AS
    WELDING PRODUCTION, 1975, 22 (03): : 11 - 15
  • [30] Wear mechanism of electrodeposited amorphous Ni-Fe-P alloys
    高诚辉
    赵源
    TransactionsofNonferrousMetalsSocietyofChina, 2004, (02) : 255 - 259