LIPSIE device: Pb-17Li irradiation in water loop with on-line tritium measurements

被引:0
|
作者
Thevenot, G. [1 ]
Lefevre, F. [1 ]
Estrade, J. [1 ]
Roche, M. [1 ]
Flament, T. [1 ]
Terlain, A. [1 ]
机构
[1] Cent d'Etudes de Saclay, Saclay, France
关键词
Breeding blankets - Diffusion in solids - Lithium alloys - Measurements - Mechanical permeability - Pressurized water reactors - Radiation effects - Scintillation counters - Stainless steel - Walls (structural partitions) - Water cooled reactors;
D O I
10.1016/0022-3115(92)90759-E
中图分类号
学科分类号
摘要
Due to the low solubility and high diffusivity of tritium in Pb-17Li, tritium permeation through the walls of a water-cooled Pb-17Li blanket has to be investigated. This has been done in Lipsie irradiation performed by CEA in the OSIRIS reactor. The Isabelle 4 PWR loop, in the OSIRIS reactor pool, has been adapted to allow us to irradiate in demineralized water at 15 MPa and 300°C a 316L stainless steel capsule of 0.025 m diameter, containing about 0, 450 kg of Pb-17Li manufactured with natural lithium. Two tritium measurements systems have been specially developed around radioactivity scintillation counting devices: one for tritium in cooling water out of the capsule and one for tritium in helium gas after sweeping or sparging in Pb-17Li inside the capsule. This paper describes the loop used for this irradiation and the tritium measurement systems. The experiment will enable us to estimate tritium permeation rate through the capsule wall in Demo-representative conditions of tritium in Pb-17Li and also study the effect of oxidation of the external capsule wall on tritium permeation by oxygen injection near the capsule.
引用
收藏
页码:226 / 230
相关论文
共 45 条
  • [41] Formation of Al2O3/FeAl coatings on a 9Cr-1 Mo steel, and corrosion evaluation in flowing Pb-17Li loop
    Majumdar, Sanjib
    Paul, Bhaskar
    Chakraborty, Poulami
    Kishor, Jugal
    Kain, Vivekanand
    Dey, Gautam Kumar
    JOURNAL OF NUCLEAR MATERIALS, 2017, 486 : 60 - 65
  • [42] TRITIUM RECYCLING, PERMEATION AND INVENTORY IN A SELF-COOLED FUSION-REACTOR BLANKET USING PB-17LI OR FLIBE AS A BREEDER AND V OR FE AS A 1ST WALL MATERIAL
    GERVASINI, G
    REITER, F
    VACUUM, 1989, 39 (7-8) : 839 - 842
  • [43] DIFFUSION-COEFFICIENT OF TRITIUM IN MOLTEN LITHIUM LEAD ALLOY (LI17PB83) UNDER NEUTRON-IRRADIATION AT ELEVATED-TEMPERATURES
    TERAI, T
    NAGAI, S
    YONEOKA, T
    TAKAHASHI, Y
    JOURNAL OF NUCLEAR MATERIALS, 1992, 187 (03) : 247 - 253
  • [44] The engineering sizing of the packed desorption column of hydrogen isotopes from Pb-17Li eutectic alloy. A rate based model using experimental mass transfer coefficients from a Melodie loop
    Linek, V.
    Kosek, L.
    Moucha, T.
    Rejl, F. J.
    Kordac, M.
    Valenz, L.
    Opletal, M.
    FUSION ENGINEERING AND DESIGN, 2014, 89 (11) : 2504 - 2515
  • [45] MASS-TRANSFER COEFFICIENT OF TRITIUM FROM MOLTEN LITHIUM LEAD ALLOY (LI-17 PB-83) TO ENVIRONMENTAL GAS UNDER NEUTRON-IRRADIATION
    TERAI, T
    NAGAI, S
    YONEOKA, T
    TAKAHASHI, Y
    FUSION ENGINEERING AND DESIGN, 1991, 17 : 237 - 241