Hot tearing behavior of AZ91D magnesium alloy

被引:11
|
作者
Zhong, Honggang [1 ]
Lin, Zenghuang [1 ]
Han, Qingyou [2 ,3 ]
Song, Jiangfeng [4 ]
Chen, Meicheng [1 ]
Chen, Xiangru [1 ]
Li, Lijuan [1 ]
Zhai, Qijie [1 ]
机构
[1] Shanghai Univ, Ctr Adv Solidificat Technol, Shanghai 200072, Peoples R China
[2] Purdue Univ, Sch Engn Technol, W Lafayette, IN 47906 USA
[3] Southeast Univ, Sch Mech Engn, Nanjing 211189, Peoples R China
[4] Chongqing Univ, Natl Engn Res Ctr Magnesium Alloys, Chongqing 400044, Peoples R China
关键词
Hot tearing; AZ91D Magnesium alloy; Mechanical behavior; Strain rate; MECHANICAL-PROPERTIES; MUSHY ZONES; STEEL; SOLIDIFICATION; CRITERION; CRACKING;
D O I
10.1016/j.jma.2023.02.010
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Hot tearing is a serious destructive solidification defect of magnesium alloys and other casting metals. Quantitative and controllable measurements on the thermal and the mechanical behavior of an alloy during its solidification process are crucial for the understanding of hot tearing formation. We developed a new experimental method and setup to characterize hot tearing behavior via controlled cooling and active loading to force hot hearing formation on cooling at selected fractions of solid. The experimental setup was fully instrumented so that stress, strain, strain rate, and temperature can be measured in-situ while hot tearing was developing. An AZ91D magnesium alloy, which is prone to hot tearing, was used in this study. Results indicate that when hot hearing occurred, the local temperature, critical stress, and cumulative strain were directly affected by strain rate. Depending on the applied strain rate, hot tearing of the AZ91D magnesium alloy could occur in two solidification stages: one in the dendrite solidification stage ( fS similar to 0.81-0.82) and the other in the eutectic solidification stage ( fS similar to 0.99). AZ91D alloy exhibited distinct mechanical behaviors in these two ranges of fraction solid. (c) 2023 Chongqing University. Publishing services provided by Elsevier B.V. on behalf of KeAi Communications Co. Ltd. This is an open access article under the CC BY-NC-ND license ( http://creativecommons.org/licenses/by-nc-nd/4.0/ ) Peer review under responsibility of Chongqing University
引用
收藏
页码:3431 / 3440
页数:10
相关论文
共 50 条
  • [31] Influence of Surface Nanocrystallization on Aluminizing Behavior of AZ91D Magnesium Alloy
    Zhang Conghui
    Song Guodong
    Wang Jing
    Zhao Xu
    RARE METAL MATERIALS AND ENGINEERING, 2020, 49 (02) : 447 - 453
  • [32] Influence of Surface Nanocrystallization on Aluminizing Behavior of AZ91D Magnesium Alloy
    Zhang, Conghui
    Song, Guodong
    Wang, Jing
    Zhao, Xu
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2020, 49 (02): : 447 - 453
  • [33] Thixotropic behavior of semi-solid AZ91D magnesium alloy
    Mao, WM
    Zhen, ZS
    Yan, SJ
    Zhong, XY
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2004, 14 (02) : 297 - 301
  • [34] Effect of applied stress on precipitation behavior in AZ91D magnesium alloy
    Na, YG
    Yim, CD
    Park, SC
    Shin, KS
    MAGNESIUM ALLOYS 2003, PTS 1 AND 2, 2003, 419-4 : 285 - 290
  • [35] Thixotropic behavior of semi-solid AZ91D magnesium alloy
    毛卫民
    甄子胜
    闫时建
    钟雪友
    Transactions of Nonferrous Metals Society of China, 2004, (02) : 297 - 301
  • [36] Corrosion behavior of AZ91D magnesium alloy in sodium sulfate solution
    Chen, J.
    Wang, J.
    Han, E.
    Dong, J.
    Ke, W.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2006, 57 (10): : 789 - 793
  • [37] Corrosion behavior of microarc oxidation film on AZ91D magnesium alloy
    Zhi Qing
    Gao Jin
    Dong Chaofang
    Li Xiaogang
    ACTA METALLURGICA SINICA, 2008, 44 (08) : 986 - 990
  • [38] Hot cracking in tungsten inert gas welding of magnesium alloy AZ91D
    Zhou, W.
    Long, T. Z.
    Mark, C. K.
    MATERIALS SCIENCE AND TECHNOLOGY, 2007, 23 (11) : 1294 - 1299
  • [39] WEAR BEHAVIOR OF AZ91D MAGNESIUM COMPOSITE
    Erarslan, Yaman
    Akca, Cem
    SIGMA JOURNAL OF ENGINEERING AND NATURAL SCIENCES-SIGMA MUHENDISLIK VE FEN BILIMLERI DERGISI, 2015, 33 (03): : 465 - 471
  • [40] Novel Fabrication of a TiB2 Grain Refiner and its Effect on Reducing Hot Tearing in AZ91D Magnesium Alloy
    T. A. Davis
    L. Bichler
    Journal of Materials Engineering and Performance, 2018, 27 : 4444 - 4452