Microstructure and properties of PAN-based carbon fiber with different graphitization temperature (up to 3000 °C)

被引:0
|
作者
Jiang, Zhenyu [1 ]
Chen, Qiufei [1 ]
Fan, Baolin [5 ]
He, Jian [1 ]
Malik, Hamza [1 ]
Zhang, Hui [1 ,2 ,3 ]
Liu, Yong [1 ,2 ,3 ]
Yu, Jianyong [4 ]
机构
[1] Donghua Univ, Coll Mat Sci & Engn, State Key Lab Modificat Chem Fibers & Polymer Mat, Shanghai 201620, Peoples R China
[2] Donghua Univ, Coll Mat Sci & Engn, Key Lab High Performance Fiber & Prod, Minist Educ, Shanghai 201620, Peoples R China
[3] Donghua Univ, Shanghai High Performance Fibers & Composites Ctr, Prov Minist Joint, Shanghai 201620, Peoples R China
[4] Donghua Univ, Innovat Ctr Text Sci & Technol, Shanghai 201620, Peoples R China
[5] Zhongfu Shenying Carbon Fiber Co Ltd, Lianyungang 222000, Peoples R China
关键词
Carbon fiber; Graphitization; High modulus; Microstructure; HEAT-TREATMENT; ELECTRICAL-CONDUCTIVITY; EVOLUTION; POLYACRYLONITRILE; CARBONIZATION; BEHAVIOR; MODULUS;
D O I
10.1016/j.diamond.2025.111953
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Understanding and regulating the graphitization process are critical to high-modulus carbon fiber production technologies. In this work, a series of high modulus polyacrylonitrile (PAN)-based carbon fibers (CFs) were prepared via the graphitization process at different temperatures up to 3000 degrees C in a continuous production line, and the evolution mechanism of the microstructures was investigated. The results showed that the primary reaction at the temperature of 2300-2600 degrees C is the condensation between graphite molecules, and over 2700 degrees C is mainly the growth and accumulating of crystallite. Moreover, due to the difference in graphitization difficulty between the skin and core layer of the CFs, the degree of graphitization at the surface is higher than that in the core. SAXS analysis suggests that the transition of amorphous carbon may begin near the micropores due to the sufficient space to rearrangement, and the amorphous carbon can more easily convert to graphite carbon above 2700 degrees C. Additionally, the optimization of CF microstructures leads to an increase in both tensile strength and elastic modulus with rising graphitization temperatures above 2700 degrees C.
引用
收藏
页数:10
相关论文
共 50 条
  • [33] Catalytic graphitization of PAN-based carbon fibers by spontaneously deposited manganese oxides
    Shoujun Yi
    Chao Wu
    Zhen Fan
    Yafei Kuang
    Jinhua Chen
    Transition Metal Chemistry, 2009, 34 : 559 - 563
  • [34] Physical Properties and Electrical Conductivity of PAN-based Carbon Fiber Reinforced Paper
    Jang, Joon
    Lee, Chang-Ho
    Park, Kwan-Ho
    Ryu, Seung-Kon
    KOREAN CHEMICAL ENGINEERING RESEARCH, 2006, 44 (06): : 602 - 608
  • [35] Pores in PAN-based carbon fiber and effects of pore defects on mechanical properties
    Hua, Zhong
    Zhong, Ya-juan
    Li, Dong-feng
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 1665 - +
  • [36] Thermoelectric power and AC electrical properties of PAN-based carbon fiber composites
    S. Saq’an
    A. M. Zihlif
    S. R. Al-Ani
    G. Ragosta
    Journal of Materials Science: Materials in Electronics, 2008, 19 : 1079 - 1085
  • [37] PAN fiber diameter effect on the structure of PAN-based carbon fibers
    Lingqiang Kong
    Hui Liu
    Weiyu Cao
    Lianghua Xu
    Fibers and Polymers, 2014, 15 : 2480 - 2488
  • [38] PAN fiber diameter effect on the structure of PAN-based carbon fibers
    Kong, Lingqiang
    Liu, Hui
    Cao, Weiyu
    Xu, Lianghua
    FIBERS AND POLYMERS, 2014, 15 (12) : 2480 - 2488
  • [39] Thermoelectric power and AC electrical properties of PAN-based carbon fiber composites
    Saq'an, S.
    Zihlif, A. M.
    Al-Ani, S. R.
    Ragosta, G.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2008, 19 (11) : 1079 - 1085
  • [40] A study on the DC electrical properties of PAN-based carbon fiber/polycarbonate composites
    Saq'an, S.
    Zihlif, A. M.
    Al-Ani, R. S.
    Ragosta, G.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2007, 18 (12) : 1203 - 1209