Anisotropy of mechanical properties and influencing factors of hot rolling TC4 titanium alloy

被引:0
|
作者
Luo, Yumeng [1 ]
Liu, Jinxu [1 ]
Li, Shukui [1 ]
Li, Mu [1 ]
Gao, Lingli [1 ]
机构
[1] Beijing Institute of Technology, Beijing,100081, China
关键词
Ductility - Hot rolling - Microstructure - Titanium alloys - Compression testing - Dynamics - Factor analysis;
D O I
暂无
中图分类号
学科分类号
摘要
Anisotropy of mechanical properties and influencing factors of hot rolling TC4 alloy were studied through quasi-static tests, dynamic compression tests, XRD, metallographic study, and electron microscopy analysis. Results indicate that the quasi-static and dynamic compression properties of 930℃ hot rolling TC4 titanium alloy exhibit obvious anisotropy: the rolling direction shows the best ductility and lowest yielding strength, while the transverse direction shows the highest yielding strength and worse ductility. The ductility and strength of the normal direction are both between the rolling direction and the transverse direction. Microstructure analysis results show that there are four factors which are responsible for the anisotropy of the mechanical properties. Firstly, after the hot rolling process, a weak plane texture was formed; secondly, the original grains were deformed into fibrous structure; thirdly the plate-like α clusters' normal axis tended to be parallel to the transverse direction of the rolling sheet; finally, a large amount of dislocations which are distributed in the grain were being parallel to the transverse direction according to the TEM results. The anisotropy of the mechanical properties is attributed to the above four factors. Copyright © 2014, Northwest Institute for Nonferrous Metal Research. Published by Elsevier BV. All rights reserved.
引用
收藏
页码:2692 / 2696
相关论文
共 50 条
  • [21] Phase transformation of TC4 titanium alloy during hot forming
    Jin, Quan-Lin
    Beijing Ligong Daxue Xuebao/Transaction of Beijing Institute of Technology, 2014, 34 : 1 - 9
  • [22] Hot deformation behavior and microstructure evolution of TC4 titanium alloy
    孙圣迪
    宗影影
    单德彬
    郭斌
    TransactionsofNonferrousMetalsSocietyofChina, 2010, 20 (11) : 2181 - 2184
  • [23] Deep Drawing of Titanium Alloy TC4 Sheet at Hot Temperatures
    郭斌
    孙圣迪
    Journal of Wuhan University of Technology(Materials Science), 2009, (S1) : 128 - 131
  • [24] Deep Drawing of Titanium Alloy TC4 Sheet at Hot Temperatures
    郭斌
    孙圣迪
    Journal of Wuhan University of Technology(Materials Science Edition), 2009, 24(S1) (Materials Science Edition) : 128 - 131
  • [25] Effect of Rolling Process on Texture Evolution, Microstructure and Mechanical Properties of TC4 Alloy Plate
    Han Ying
    Yu Wei
    Dong Entao
    Cheng Zhisong
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (10) : 3585 - 3590
  • [26] Study on necking defects, microstructure and mechanical properties of TC4 alloy by cross wedge rolling
    Li, Peiai
    Wang, Baoyu
    Yang, Cuiping
    Zhang, Huibo
    Li, Wei
    Zhou, Jing
    INTERNATIONAL JOURNAL OF MATERIAL FORMING, 2022, 15 (06)
  • [27] Effect of Rolling Process on Texture Evolution, Microstructure and Mechanical Properties of TC4 Alloy Plate
    Han, Ying
    Yu, Wei
    Dong, Entao
    Cheng, Zhisong
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2021, 50 (10): : 3585 - 3590
  • [28] Study on necking defects, microstructure and mechanical properties of TC4 alloy by cross wedge rolling
    Peiai Li
    Baoyu Wang
    Cuiping Yang
    Huibo Zhang
    Wei Li
    Jing Zhou
    International Journal of Material Forming, 2022, 15
  • [29] Dynamic mechanical property and constitutive model for TC4 titanium alloy
    Hui X.
    Mu R.
    Bai C.
    Liu X.
    Shi T.
    Mu, Rangke, 1600, Chinese Vibration Engineering Society (35): : 161 - 168
  • [30] Effect of high pulsed magnetic field on microstructure and mechanical properties of TC4 titanium alloy
    Li, Gui-Rong
    Li, Yue-Ming
    Wang, Fang-Fang
    Wang, Hong-Ming
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2015, 25 (02): : 330 - 337