Corrosion performance of (ZrYTaAlCr)O ceramic coating materials for heated surface tubes

被引:0
|
作者
Chen, Yuhui [1 ,2 ]
Chai, Zonghua [1 ]
Chen, Shiwang [3 ]
Cao, Yang [4 ]
Wu, Tan [1 ,2 ]
Wang, Zihao [1 ]
Zhang, Baiqiang [1 ,2 ]
Wang, Caidong [4 ]
机构
[1] School of Energy and Power Engineering, Zhengzhou University of Light Industry, Zhengzhou,450002, China
[2] Henan International Joint Laboratory of Energy Efficient Conversion and Utilization, Zhengzhou,450002, China
[3] Fujian Special Equipment Inspection and Research Institute, Fuzhou,350008, China
[4] School of Mechanical and Electrical Engineering, Zhengzhou University of Light Industry, Zhengzhou,450002, China
基金
中国国家自然科学基金;
关键词
Aluminum corrosion - Atmospheric corrosion - Boiler corrosion - Boiler firing - Ceramic coatings - Corrosion resistance - Corrosion resistant coatings - Corrosive effects - Waste incineration;
D O I
10.1016/j.ceramint.2024.10.183
中图分类号
学科分类号
摘要
The comprehensive advantages of waste incineration power generation are evident, gradually replacing composting, landfill, and other treatment methods. However, the presence of chlorine, sulfur, heavy metals, and a variety of hazardous elements in the flue gas has led to severe corrosion of the heated surface tubes of the waste incineration boilers and an increase in the failure rate of the boilers, thus restricting the wider application of waste incineration power generation technology. In this study, (ZrYTaAlCr)O high-entropy ceramic materials were synthesized via the solid-phase reaction method and subjected to exposure in a standard corrosive mixture (SCM) simulating the molten salts environment of waste incineration boilers, consisting of NaCl (25 mol%), KCl (25 mol%), Na2SO4 (25 mol%), and K2SO4 (25 mol%). The corrosion behavior of (ZrYTaAlCr)O ceramics with different proportions was studied through visual detection, corrosion kinetics, XRD, and SEM/EDS analysis. The results show that (Zr0.5Y0.125Ta0.125Al0.125Cr0.125)O forms a NaTaO3 tantalate protective layer in the early stages of corrosion, with fewer types of corrosion products. Compared with other compositions, (Zr0.5Y0.125Ta0.125Al0.125Cr0.125)O has good corrosion resistance and is suitable as a corrosion protection material for the heating surface tubes of waste incineration boilers. © 2024 Elsevier Ltd and Techna Group S.r.l.
引用
收藏
页码:53329 / 53341
相关论文
共 50 条
  • [41] The effect of NiCr intermediate layer on corrosion behavior of Cr2O3 ceramic coated materials
    Li, CL
    Zhao, HX
    Matsumura, M
    Takahashi, T
    Asahara, M
    Yamaguchi, H
    SURFACE & COATINGS TECHNOLOGY, 2000, 124 (01): : 53 - 60
  • [42] A study of nano-sized surface coating on LiMn2O4 materials
    Hung, Fei-Yi
    Lui, Truan-Sheng
    Liao, Hung-Chi
    APPLIED SURFACE SCIENCE, 2007, 253 (18) : 7443 - 7448
  • [43] The effect of surface pretreatment on the corrosion performance of Electroless E-coating coated AZ31
    Song, Guang-Ling
    Liu, Minghong
    CORROSION SCIENCE, 2012, 62 : 61 - 72
  • [44] Study on Performance and Corrosion Resistance Mechanism of Rare Earth Metal Conversion Coating on Al Alloy Surface
    Gu Baoshan
    Gong Li
    Yang Peiyan
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (02) : 429 - 434
  • [45] Corrosion performance of chemically polymerized poly(pyrrole-co-o-toluidine) coating on mild steel
    M. Mobin
    Nelofar Tanveer
    Protection of Metals and Physical Chemistry of Surfaces, 2012, 48 : 243 - 250
  • [46] Performance and corrosion resistance mechanism of SA-Al composite hydrophobic coating on electrolytic manganese surface
    Lei, Sihua
    Wang, Shuai
    Zhong, Hong
    Ma, Xin
    Cao, Zhan-fang
    SURFACE & COATINGS TECHNOLOGY, 2021, 419
  • [47] Corrosion performance of chemically polymerized poly(pyrrole-co-o-toluidine) coating on mild steel
    Mobin, M.
    Tanveer, Nelofar
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2012, 48 (02) : 243 - 250
  • [48] Tribological and corrosion performance of electrodeposited Ni-Fe/Al2O3 coating
    Rezayat, Mohammad
    Yazdi, Morteza Saghafi
    Zandi, Mohammad Damous
    Azami, Aref
    RESULTS IN SURFACES AND INTERFACES, 2022, 9
  • [49] Fabrication of calcium phosphate coating on pure magnesium substrate via simple chemical conversion coating: surface properties and corrosion performance evaluations
    Zaludina, Mohd Amin Farhan
    Jamala, Zul Azhar Zahid
    Dermana, Mohd Nazree
    Kasmuina, Mohd Zaheruddin
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (01): : 981 - 987
  • [50] A review of nanostructured surfaces and materials for dental implants: surface coating, patterning and functionalization for improved performance
    Rasouli, Rahimeh
    Barhoum, Ahmed
    Uludag, Hasan
    BIOMATERIALS SCIENCE, 2018, 6 (06) : 1312 - 1338