Fatigue characteristics of a newly developed laser powder bed fused scandium-free Al-Mg-Zr-Mn alloy

被引:1
|
作者
Shakil, Shawkat I. [1 ]
Bednarczyk, Wiktor [2 ]
Gajewska, Marta [3 ]
Mahbooba, Zaynab [4 ]
Saharan, Ankit [4 ]
Tridello, Andrea [5 ]
Paolino, Davide S. [5 ]
Haghshenas, Meysam [1 ]
机构
[1] Univ Toledo, Dept Mech Ind & Mfg Engn MIME, Fatigue Fracture & Failure Lab F3L, Toledo, OH 43606 USA
[2] AGH Univ Krakow, Fac Met Engn & Ind Comp Sci, Krakow, Poland
[3] AGH Univ Krakow, Acad Ctr Mat & Nanotechnol, Krakow, Poland
[4] EOS North Amer Inc, Pflugerville, TX USA
[5] Politecn Torino, Dept Mech & Aerosp Engn, Turin, Italy
关键词
Additive Manufacturing; Laser powder bed fusion; Fatigue; Al-Mg-Zr-Mn; EXTREME-VALUE STATISTICS; DISLOCATION-STRUCTURE; BEHAVIOR; MICROSTRUCTURE; COMPONENTS; INCLUSIONS; STRENGTH; DEFECTS;
D O I
10.1016/j.ijfatigue.2024.108738
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This study investigates the fully reversed force-controlled fatigue response of a newly developed laser powder bed fused (LPBF) Al-Mg-Zr-Mn alloy (EOS Al5X1) in the post-aged condition. The fatigue behavior revealed a defect-driven response with a fatigue strength of approximately 140 MPa at 5 million cycles. Comprehensive microstructural analyses, including grain size, texture, and precipitate characterization, were performed using advanced microscopy techniques. Additionally, X-ray computed micro-tomography (XCT) was employed to assess defect size and distribution, yielding a relative density of 99.93 %. Fracture surfaces of all fatigue-failed specimens were examined using optical and scanning electron microscopy to determine the primary failure mechanisms, with a focus on distinguishing between defect-driven and microstructural causes. The results indicated that nearly all specimens, tested across seven stress levels, exhibited crack initiation from process- induced volumetric defects, such as pores and lack of fusion. At lower stress levels (up to 195 MPa), single crack initiation sites driven by defects were identified at either surface or subsurface locations. In contrast, at higher stress levels (234 to 351 MPa), multiple crack initiation sites were observed, also at the surface or subsurface.
引用
收藏
页数:22
相关论文
共 50 条
  • [21] Microstructure and mechanical properties of Al-Mg-Mn-Er-Zr alloys fabricated by laser powder bed fusion
    Guo, Yanwu
    Wei, Wu
    Shi, Wei
    Zhou, Xiaorong
    Wen, Shengping
    Wu, Xiaolan
    Gao, Kunyuan
    Zhang, Dongyun
    Qi, Peng
    Huang, Hui
    Nie, Zuoren
    MATERIALS & DESIGN, 2022, 222
  • [22] Influence of the Zr content on the processability of a high strength Al-Zn-Mg-Cu-Zr alloy by laser powder bed fusion
    Martin, A.
    Vilanova, M.
    Gil, E.
    Sebastian, M. San
    Wang, C.Y.
    Milenkovic, S.
    Pérez-Prado, M.T.
    Cepeda-Jiménez, C.M.
    Materials Characterization, 2022, 183
  • [23] Influence of the Zr content on the processability of a high strength Al-Zn-Mg-Cu-Zr alloy by laser powder bed fusion
    Martin, A.
    Vilanova, M.
    Gil, E.
    San Sebastian, M.
    Wang, C. Y.
    Milenkovic, S.
    Perez-Prado, M. T.
    Cepeda-Jimenez, C. M.
    MATERIALS CHARACTERIZATION, 2022, 183
  • [24] Effects of powder reuse on the microstructure and mechanical behaviour of Al–Mg–Sc–Zr alloy processed by laser powder bed fusion (LPBF)
    Cordova, Laura
    Bor, Ton
    de Smit, Marc
    Carmignato, Simone
    Campos, Mónica
    Tinga, Tiedo
    Additive Manufacturing, 2020, 36
  • [25] A novel Al-Zn-Mg-Cu-Si-Zr-Er alloy fabricated by laser powder bed fusion
    Li, Dehua
    Li, Shengci
    Chen, Jiqiang
    Zhang, Zhiqian
    Tang, Hui
    MATERIALS CHARACTERIZATION, 2024, 214
  • [26] Investigation and characterization of an Al-Mg-Zr-Sc alloy with reduced Sc content for laser powder bed fusion
    Belelli, F.
    Casati, R.
    Andrianopoli, C.
    Cuccaro, F.
    Vedani, M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 924
  • [27] Comprehensive Characterisation of a Newly Developed Mg-Dy-Al-Zn-Zr Alloy Structure
    Kuncicka, Lenka
    Kocich, Radim
    METALS, 2018, 8 (01):
  • [28] The effect of heat treatment on fatigue response of laser powder bed fused Al-Cu-Mg-Ag-TiB2 (A20X) alloy
    Avateffazeli, Maryam
    Shakil, Shawkat Imam
    Khan, Md Faysal
    Pirgazi, Hadi
    Shamsaei, Nima
    Haghshenas, Meysam
    MATERIALS TODAY COMMUNICATIONS, 2023, 35
  • [29] Effect of minor Sc and Zr on the fatigue properties of Al-Mg-Mn alloy
    Peng, Yong-yi
    Yin, Zhi-min
    Nie, Bo
    Wang, Tao
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 863 - +
  • [30] Laser powder bed fusion of a novel crack-free Al-Mg-Sc-Zr alloy: Printability, microstructure characterization and mechanical performance
    Li, Xiang
    Liu, Yunzhong
    Tan, Chaolin
    Zou, Yongming
    OPTICS AND LASER TECHNOLOGY, 2023, 162