Exploring the ionic conductivity of A2Ti2O7 (A = Y and Gd) pyrochlore: Experimental and DFT approach

被引:0
|
作者
Ajayraj, A. [1 ]
Kumar, B. Navaneeth [1 ]
Baburao, Upare Vishal [1 ]
Amala, J. [1 ]
Kuppusamy, Raghu Raja Pandiyan [1 ]
Suranani, Srinath [1 ]
Anantharaman, Anjana P. [1 ]
机构
[1] Natl Inst Technol, Dept Chem Engn, Warangal 506004, Telangana, India
关键词
Pyrochlore; Superstructure; Defect formation energy; DFT; Ionic conductivity; ELECTRICAL-CONDUCTIVITY; RE2TI2O7; RE; ELECTROLYTES; MIGRATION; CERAMICS; BEHAVIOR; CERIA; TB; CO; LN;
D O I
10.1016/j.ssc.2024.115795
中图分类号
O469 [凝聚态物理学];
学科分类号
070205 ;
摘要
This work investigates the structural and electrical properties of titanate pyrochlore materials, GT (Gd2Ti2O7) and YT (Y2Ti2O7), synthesized using the sol-gel method that can be used as solid electrolytes in intermediate temperature solid oxide fuel cells (IT-SOFCs). Both materials were found to have single-phase pyrochlore structures with cubic lattices and Fd-3m space groups after X-ray diffraction analysis. Rietveld refinement revealed that substituting Gd3+ with lower ionic radii cation of Y 3+ reduced lattice constants, lattice volume, and crystallite size, attributed to differences in ionic radius and potential hybridization effects. The oxygen x parameter that decides the disorder in the structure obtained through Rietveld refinement is higher for GT (0.431) than the recommended range of 0.3125-0.375, along with the presence of superstructure peaks confirms the disordered pyrochlore structure in GT sample. Raman spectroscopy has consistent vibrational modes across both samples, while SEM indicated larger particle sizes for YT. X-ray photoelectron spectroscopy (XPS) analysis clarifies higher surface oxygen ratios in YT (67.6 %), which is crucial for oxygen ion transport. The O1s spectra of both samples show O 48f facilitating conductivity and O 8b corresponding to defect sites. Despite YT having higher dislocation density (0.313) and lattice strain (0.0058), GT exhibited lower defect formation energy (-5.82 eV) based on DFT results, favouring oxygen vacancy formation and enhanced ionic conductivity (2.07 x 10-3) at 700 degrees C. The highest ionic conductivity for YT is obtained at 600 degrees C of 2.33 x 10-3 with defect formation energy of -4.96 eV. The findings emphasize the critical role of structural disorder and defect sites in optimizing ionic conductivity.
引用
收藏
页数:8
相关论文
共 50 条
  • [11] Magnetic resonance in the pyrochlore antiferromagnet Gd2Ti2O7
    Sosin, S. S.
    Smirnov, A. I.
    Prozorova, L. A.
    Balakrishnan, G.
    Zhitomirsky, M. E.
    PHYSICAL REVIEW B, 2006, 73 (21)
  • [12] Adiabatic demagnetization of a pyrochlore antiferromagnet Gd2Ti2O7
    Sosin, SS
    Prozorova, LA
    Smirnov, AI
    Golov, AI
    Berkutov, IB
    Petrenko, OA
    Balakrishnan, G
    Zhitomirsky, ME
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2005, 290 : 709 - 711
  • [13] Thermoelectric performance of Dy/Y co-doped SrTiO3 ceramic composites with submicron A2Ti2O7 (A = Dy, Y) pyrochlore
    Chen, Tingting
    Wang, Hongchao
    Su, Wenbin
    Wang, Xue
    Mehmood, Fahad
    Zhang, Kaiqi
    Huo, Taichang
    Wang, Chunlei
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2021, 54 (15)
  • [14] Preparation and properties of high-entropy pyrochlore A2Ti2O7 with multi-elements at A site
    Guo, Haiyan
    Zhang, Kuibao
    Li, Yuxiang
    Jiang, Xiaoe
    CERAMICS INTERNATIONAL, 2024, 50 (01) : 1 - 8
  • [15] Ionic conduction and disorder in the Gd2Sn2O7 pyrochlore system
    Yu, TH
    Tuller, HL
    SOLID STATE IONICS, 1996, 86-8 : 177 - 182
  • [16] Ionic conduction and disorder in the Gd2Sn2O7 pyrochlore system
    Massachusetts Inst of Technology, Cambridge, United States
    Solid State Ionics, 1996, 86-88 (pt 1): : 177 - 182
  • [17] IONIC-CONDUCTION IN THE GD2TI2O7-GD2ZR2O7 SYSTEM
    MOON, PK
    TULLER, HL
    SOLID STATE IONICS, 1988, 28 : 470 - 474
  • [18] Intermediate temperature ionic conductivity of Sm1.92Ca0.08Ti2O7–δ pyrochlore
    Karinh E. J. Eurenius
    Henrik Karnøe Bentzer
    Nikolaos Bonanos
    Elisabet Ahlberg
    Christopher S. Knee
    Journal of Solid State Electrochemistry, 2011, 15 : 2571 - 2579
  • [19] Energetics and concentration of defects in Gd2Ti2O7 and Gd2Zr2O7 pyrochlore at high pressure
    Wang, Jianwei
    Zhang, Fuxiang
    Lian, Jie
    Ewing, Rodney C.
    Becker, Udo
    ACTA MATERIALIA, 2011, 59 (04) : 1607 - 1618
  • [20] Spin dynamics of the pyrochlore magnets Gd2Ti2O7 and Gd2Sn2O7 in the paramagnetic state
    Sosin, S. S.
    Prozorova, L. A.
    Smirnov, A. I.
    Bonville, P.
    Bras, G. Jasmin-Le
    Petrenko, O. A.
    PHYSICAL REVIEW B, 2008, 77 (10)