Microstructure and high-temperature oxidation resistance of Ti-6Al-4V alloy with in-situ SiC-SiO2 nano-composite coating by LPDS technique

被引:1
|
作者
Wang, Jiacheng [1 ]
Zhang, Liwei [1 ]
Cheng, Jiahao [1 ]
Liu, Jing [1 ]
Qi, Dan [1 ]
Zou, Yongchun [2 ,3 ]
Wei, Daqing [4 ]
Cheng, Su [1 ]
Wang, Yaming [3 ]
机构
[1] Harbin Univ Sci & Technol, Sch Architecture & Civil Engn, Harbin 150080, Peoples R China
[2] Harbin Inst Technol, Ctr Anal & Measurement, Harbin 150001, Peoples R China
[3] Harbin Inst Technol, Inst Adv Ceram, Harbin 150001, Peoples R China
[4] Harbin Engn Univ, Coll Nucl Sci & Technol, Harbin 150001, Peoples R China
关键词
Ti-6Al-4V alloy; SiC nanoparticle; Liquid-plasma-assisted particle deposition and; sintering; High-temperature oxidation resistance; Oxidation resistance mechanisms; PLASMA ELECTROLYTIC OXIDATION; MECHANICAL-PROPERTIES; CERAMIC COATINGS; C/C COMPOSITES; TITANIUM-ALLOY; NANOPARTICLES; PROTECTION; BEHAVIOR;
D O I
10.1016/j.ceramint.2024.08.472
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A SiC-SiO2 nano-composite coating was prepared via a novel liquid-phase plasma-assisted particle deposition and sintering (LPDS) method to enhance the oxidation resistance of the Ti-6Al-4V alloy. For comparison, a conventional plasma electrolytic oxidation (PEO) ceramic coating is fabricated on the Ti-6Al-4V alloy. The microstructure and formation mechanisms of both ceramic coatings were investigated using scanning electron microscopy (SEM), X-ray diffraction (XRD), and transmission electron microscopy (TEM). The results indicated that the thickness of the SiC nano-composite coating (similar to 40 mu m) increased significantly by 285 % compared to the PEO coating (similar to 14 mu m). The microstructural evolution and isothermal oxidation performance of the PEO and SiC-SiO2 nano-composite coating were comparatively investigated at 800 degrees C. After 100 h, the thickness gain of the SiC-SiO2 nano-composite coating (similar to 14 mu m) was lower than that of the PEO coating (similar to 26 mu m). The improved oxidation performance is primarily attributed to the outermost layer containing abundant SiC nanoparticles, which transform into SiO2 during the oxidation process and effectively inhibiting the inward penetration of oxygen.
引用
收藏
页码:46288 / 46299
页数:12
相关论文
共 50 条
  • [31] Effect of SiO2 coating combined with chemical treatment by phosphoric acid on oxidation resistance of Ti-6Al-4V alloy
    Ren, Bao-Yi
    Liu, Zi-Ru
    Gao, Yan-Hui
    Zhang, Xue-Jun
    Cailiao Gongcheng/Journal of Materials Engineering, 2013, (05): : 62 - 66
  • [32] High-temperature creep behavior of TiC particulate reinforced Ti-6Al-4V alloy composite
    Ma, ZY
    Mishra, RS
    Tjong, SC
    ACTA MATERIALIA, 2002, 50 (17) : 4293 - 4302
  • [33] Microstructure and high-temperature oxidation resistance of laser cladding in-situ synthesis Ti-Al-Si composite coatings
    Liu H.-X.
    Zhao Y.-S.
    Zhang X.-W.
    Hao X.-H.
    Zhang L.-L.
    Guangxue Jingmi Gongcheng/Optics and Precision Engineering, 2019, 27 (02): : 316 - 325
  • [34] MECHANICAL PROPERTIES AND HIGH TEMPERATURE OXIDATION BEHAVIOR OF Ti-Al COATING REINFORCED BY NITRIDES ON Ti-6Al-4V ALLOY
    Dai, Jingjie
    Yu, Huijun
    Zhu, Jiyun
    Weng, Fei
    Chen, Chuanzhong
    SURFACE REVIEW AND LETTERS, 2016, 23 (05)
  • [35] High temperature deformation behavior of Ti-6Al-4V alloy with Widmanstaten microstructure
    Kim, JH
    Semiatin, SL
    Lee, CS
    THERMEC'2003, PTS 1-5, 2003, 426-4 : 689 - 694
  • [36] High temperature forming of Ti-6Al-4V alloy considering microstructure evolution
    Hwanlee, Y
    Soolee, C
    RARE METAL MATERIALS AND ENGINEERING, 2006, 35 : 29 - 33
  • [37] Microstructure evolution during high temperature deformation of Ti-6Al-4V alloy
    Luo, Jiao
    Li, Miaoquan
    Yu, Weixin
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2010, 39 (08): : 1323 - 1328
  • [38] Microstructure Evolution during High Temperature Deformation of Ti-6Al-4V Alloy
    Luo Jiao
    Li Miaoquan
    Yu Weixin
    RARE METAL MATERIALS AND ENGINEERING, 2010, 39 (08) : 1323 - 1328
  • [39] Microstructure of ceramic coating formed by microarc oxidation in silicate solution on Ti-6Al-4V alloy
    Xue, Wenbin
    Deng, Zhiwei
    Chen, Ruyi
    Zhang, Tonghe
    Gongye Jianzhu/Industrial Construction, 2000, 30 (02): : 5 - 7
  • [40] Structure and abrasion resistance of MoS2/TiN composite coating on Ti-6Al-4V alloy
    Wang, Lijie
    Tian, Xiaodong
    Yang, Junsheng
    MATERIALS PROCESSING TECHNOLOGIES, PTS 1 AND 2, 2011, 154-155 : 727 - 730