Failure analysis of superheater tubes in an air quenching cooler waste heat boiler

被引:0
|
作者
Li, Yongjun [1 ]
Chen, Hualin [1 ]
Pan, Zhi [1 ]
Liang, Hanzhao [1 ]
Wang, Zhipeng [1 ]
Feng, Zongjian [1 ]
Li, Zhigang [1 ]
Kuang, Yunkun [1 ]
机构
[1] Guangxi Special Equipment Inspection and Research Institute, 25 Renxin Road, Nanning,530299, China
关键词
Heat affected zone - Fracture mechanics - Microhardness - Residual stresses - Waste heat - Cracks - Tensile testing - Failure (mechanical) - Finite element method - Boilers - Textures - Chemical analysis - Optical emission spectroscopy - Failure analysis;
D O I
暂无
中图分类号
学科分类号
摘要
The failure of superheater tubes in an air quenching cooler waste heat boiler from a cement plant is presented in this study. The tubes were composed of material specified to ASTM SA210C. After three months in service, one leak was detected in one of the tubes over its bent section. Subsequently, several leaks also were found in other tubes of the same boiler. In order to find out the root cause of the leaks, the failed tubes were investigated by visual inspection, optical emission spectroscopy, metallographic analysis, tensile test, micro-hardness measurements, and SEM/EDS analysis. Visual inspection revealed that no obvious wall thinning, swelling and mechanical damage were observed in the failure zone. The material met the chemical composition, microstructure, and tensile property requirements, while the micro-hardness far exceeded the requirements as specified by ASTM. It has been found that the fracture surfaces in general exhibited intergranular brittle fracture. Furthermore, the cracks with corrosion products originating on the water side of tubes were branched. According to finite element calculations, the residual stress in the failure zone due to bending confirmed that cracks propagated in a general direction perpendicular to the stresses. Therefore, the failure mechanism of the tubes was identified as stress corrosion cracking. © 2021
引用
收藏
相关论文
共 50 条
  • [21] Catastrophic failure of waste heat boiler
    ElBatahgy, AM
    MATERIALS PERFORMANCE, 1997, 36 (02) : 81 - 83
  • [22] Catastrophic failure of waste heat boiler
    Central Metallurgical R&D Inst, Cairo, Egypt
    Mater Perform, 2 (81-83):
  • [23] Failure analysis and modeling of super heater tubes of a waste heat boiler thermally coupled in ammonia oxidation reactor
    Abbasfard, Hamed
    Ghanbari, Mehdi
    Ghasemi, Amin
    Ghader, Sattar
    Rafsanjani, Hasan Hashemipour
    Moradi, Ali
    ENGINEERING FAILURE ANALYSIS, 2012, 26 : 285 - 292
  • [24] STRESS-DISTRIBUTION IN THE TUBES OF A WASTE HEAT BOILER
    GUDENAU, HW
    DAHL, W
    KOERFER, M
    SCHEIWE, M
    STEEL RESEARCH, 1990, 61 (04): : 164 - 169
  • [25] Analysis of Superheater Boiler Tubes Failed through Non-linear Heating
    Roy, Rajat K.
    Das, Swapan K.
    Panda, Ashis K.
    Mitra, Amitava
    STRUCTURAL INTEGRITY, 2014, 86 : 926 - 932
  • [26] Failure of evaporator tubes initiated by lamellar tearing during the commissioning of a waste heat recovery boiler
    Srikanth, S.
    Das, S. K.
    Sasikumar, C.
    Ravikumar, B.
    ENGINEERING FAILURE ANALYSIS, 2007, 14 (01) : 262 - 278
  • [27] STRESS-CORROSION FAILURE OF WASTE HEAT BOILER TUBES IN AN AMMONIA-SYNTHESIS CONVERTER
    VERMA, KM
    GHOSH, H
    PATTNAIK, KC
    BRITISH CORROSION JOURNAL, 1980, 15 (04): : 175 - 178
  • [28] Failure, repair and replacement of waste heat boiler
    Ahmed, S
    Anwar, Z
    AMMONIA PLANT SAFETY & RELATED FACILITIES, VOL 37, 1997, 37 : 100 - 110
  • [29] Failure analysis of primary waste heat boiler tube in ammonia plant
    Ardy, Husaini
    Putra, Yudhistira Perdana
    Anggoro, Adimas Dwi
    Wibowo, Arie
    HELIYON, 2021, 7 (02)
  • [30] Root Cause Analysis of Failure in Superheater Tubes in a Power Plant
    A. Bahrami
    S. M. Rafiaei
    M. Yazdan Mehr
    Metallography, Microstructure, and Analysis, 2019, 8 : 275 - 280