Microstructure tailoring and impact toughness of a newly developed high strength Ti-5Al-3Mo-3V-2Cr-2Zr-1Nb-1Fe alloy

被引:0
|
作者
Wu, Cong [1 ]
Zhao, Yongqing [2 ]
Huang, Shixing [2 ]
Lei, Lei [2 ]
Zhao, Qinyang [3 ]
Sun, Qiaoyan [1 ]
Zhou, Lian [1 ,2 ]
机构
[1] State Key Laboratory for Mechanical Behavior of Materials, Xi'an Jiaotong University, Xi'an,710049, China
[2] Northwest Institute for Non-ferrous Metal Research, Xi'an,710016, China
[3] School of Material Science and Engineering, Chang'an University, Xi'an,710064, China
关键词
Titanium alloys;
D O I
暂无
中图分类号
学科分类号
摘要
To achieve preferable impact performance of a newly designed high strength Ti-5321 alloy, samples with three kinds of microstructures, i.e., bimodal microstructure (BM), tri-modal microstructure (TM) and lamellar microstructure (LM) were prepared for instrument Charpy tests at room temperature. Results of impact tests indicated that LM presented the higher impact toughness of 37.5 J/cm2 than that of BM (11.25 J/cm2) and TM (25 J/cm2). Moreover, both crack initiation energy and crack propagation energy of LM were obviously raised. Further analysis containing fracture surfaces and the cross-sectional microstructures of the impact samples by the usage of SEM and EBSD provided insights into the influence of microstructure on crack initiation and propagation during impact process. The largely plastic deformation of primary α near the V-notch tip impeded crack initiation and enhanced the crack initiation energy. The interweaved α colonies with high angle boundaries deflected the crack propagation direction and thus increased the crack propagation energy. Besides, TEM analysis showed that the typical deformation characteristic under impact test with high strain rate. Except for dislocation lines, the pile-up of highly dense dislocations, twinning, dislocation cells, sub-grains, shear bands and fragmentation of α phase can be found. These approaches presented in this study could provide certain insights into fabricating typical microstructure in the high strength titanium alloys to ameliorate impact properties. © 2021 Elsevier Inc.
引用
收藏
相关论文
共 50 条
  • [31] Effect of cyclic heat treatment on microstructure and mechanical properties of Ti-5Al-5Mo-5V-3Cr-1Zr alloy
    Gong-Ye, Fan-Jiao
    Zhou, Jie
    Zhang, Qian
    Long, Shuai
    Zhou, Yu-Ting
    Li, Shi-shan
    Peng, Shi-Xin
    Deng, He-Ping
    Zhang, Jian-Sheng
    MATERIALS RESEARCH EXPRESS, 2021, 8 (07)
  • [32] Microstructure Evolution during High-Temperature Deformation of Ti-5Al-5V-2Mo-1Cr-1Fe Alloy under Compression
    Anil Kumar, V.
    Sarkar, Aditya
    Gupta, R. K.
    Prasad, M. J. N. V.
    Murty, S. V. S. N.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (05) : 3258 - 3272
  • [33] Microstructure Evolution during High-Temperature Deformation of Ti-5Al-5V-2Mo-1Cr-1Fe Alloy under Compression
    V. Anil Kumar
    Aditya Sarkar
    R. K. Gupta
    M. J. N. V. Prasad
    S. V. S. N. Murty
    Journal of Materials Engineering and Performance, 2021, 30 : 3258 - 3272
  • [34] Melting and Microstructure Analysis of β-Ti Alloy Ti-5Al-5Mo-5V-1Cr-1Fe With and Without Boron
    Kumar, V. Anil
    Murty, S. V. S. N.
    Gupta, R. K.
    Babu, R. Ramesh
    Prasad, M. J. N. V.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2015, 68 : S207 - S215
  • [35] Microstructure and high cycle fatigue fracture surface of a Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy
    Wu, G. Q.
    Shi, C. L.
    Sha, W.
    Sha, A. X.
    Jiang, H. R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 575 : 111 - 118
  • [36] High-Temperature Oxidation of Ti-48Al-2Nb-2Cr and Ti-25Al-10Nb-3V-1Mo
    Rajendra U. Vaidya
    Young Soo Park
    Jin Zhe
    George T. Gray
    Darryl P. Butt
    Oxidation of Metals, 1998, 50 : 215 - 240
  • [37] High-temperature oxidation of Ti-48Al-2Nb-2Cr and Ti-25Al-10Nb-3V-1Mo
    Vaidya, RU
    Park, YS
    Zhe, J
    Gray, GT
    Butt, DP
    OXIDATION OF METALS, 1998, 50 (3-4): : 215 - 240
  • [38] Microstructure Evolution in Adiabatic Shear Band in Ti-5Mo-5V-2Cr-3Al Alloy
    You Zhenping
    Mi Xujun
    Hui Songxiao
    Ye Wenjun
    Yu Yang
    Wang Bo
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 (07) : 1184 - 1187
  • [39] Effect of Cooling Rate on Microstructure of Alloy Ti3Al-10Nb-3V-1Mo
    张启海
    周光爵
    邬彦如
    Rare Metals, 1997, (04) : 48 - 53
  • [40] Room-Temperature Compressive Deformation Behavior of High-Strength Ti-15V-3Al-3Cr-3Sn-1Nb-1Zr Alloy
    Zhaohui Zhang
    Quanming Liu
    Haiying Yang
    Shifeng Liu
    Journal of Materials Engineering and Performance, 2017, 26 : 3368 - 3375