Deformation Mechanisms of (100) and (110) Single-Crystal BCC Gum Metal Studied by Nanoindentation and Micropillar Compression

被引:0
|
作者
Jarzabek, Dariusz M. [1 ,2 ]
Wloczewski, Mateusz [2 ]
Milczarek, Michal [1 ]
Jenczyk, Piotr [1 ]
Takesue, Naohisa [3 ]
Golasinski, Karol M. [4 ]
Pieczyska, Elzbieta A. [1 ]
机构
[1] Polish Acad Sci, Inst Fundamental Technol Res, PL-02106 Warsaw, Poland
[2] Warsaw Univ Technol, PL-00661 Warsaw, Poland
[3] Fukuoka Univ, Fukuoka 8140180, Japan
[4] Cardinal Stefan Wyszynski Univ Warsaw, Multidisciplinary Res Ctr, PL-05092 Dziekanow Lesny, Poland
关键词
STRAIN-RATE SENSITIVITY; ELASTIC-MODULUS; ALLOY; PHASE; INDENTATION; STRENGTH; BEHAVIOR; BETA;
D O I
10.1007/s11661-024-07605-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, small-scale testing techniques-nanoindentation and micropillar compression-were used to investigate the deformation mechanisms, size effects, and strain rate sensitivity of (100) and (110) single-crystal Gum Metal at the micro/nanoscale. It was observed that the (100) orientation exhibits a significant size effect, resulting in hardness values ranging from 1 to 5 GPa. Conversely, for the (110) orientation, this effect was weaker. Furthermore, the yield strength obtained from the micropillar compression tests was approximately 740 MPa for the (100) orientation and 650 MPa for the (110) orientation. The observed deformations were consistent with the established features of the deformation behavior of body-centered cubic (bcc) alloys: significant strain rate sensitivity with no depth dependence, pile-up patterns comparable to those reported in the literature, and shear along the {112}<111> slip directions. However, the investigated material also exhibited Gum Metal-like high ductility, a relatively low modulus of elasticity, and high yield strength, which distinguishes it from classic bcc alloys. (C) The Author(s) 2024
引用
收藏
页码:4954 / 4964
页数:11
相关论文
共 50 条
  • [31] OXYGEN-CHEMISORPTION AND CORROSION ON CR(100) AND CR(110) SINGLE-CRYSTAL SURFACES
    FOORD, JS
    LAMBERT, RM
    SURFACE SCIENCE, 1985, 161 (2-3) : 513 - 520
  • [32] EMISSION CHARACTERISTICS OF SINGLE-CRYSTAL LAB6 CATHODES WITH (100) AND (110) ORIENTATIONS
    FURUKAWA, Y
    YAMABE, M
    ITOH, A
    INAGAKI, T
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1982, 20 (02): : 199 - 203
  • [33] LEED STUDY OF INTERACTION OF OXYGEN WITH COPPER SINGLE-CRYSTAL FACES (110), (100) AND (111)
    OUSTRY, A
    LAFOURCA.L
    ESCAUT, A
    SURFACE SCIENCE, 1973, 40 (03) : 545 - 554
  • [34] THE DEPOSITION OF SILICON ON METAL SINGLE-CRYSTAL SURFACES, STUDIED BY RAIRS, LEED AND AES
    CHESTERS, MA
    HORN, AB
    JOURNAL OF PHYSICS-CONDENSED MATTER, 1991, 3 : S251 - S256
  • [35] RADIATION-DAMAGE IN SINGLE-CRYSTAL ICE STUDIED BY 100 KEV PROTON CHANNELING
    GOLECKI, I
    JACCARD, C
    SURFACE SCIENCE, 1979, 90 (02) : 357 - 358
  • [36] Deformation mechanisms in single crystal Ni-based concentrated solid solution alloys by nanoindentation
    Yang, Liuqing
    Chen, Youxing
    Miller, Jimmie
    Weber, William J.
    Bei, Hongbin
    Zhang, Yanwen
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 856
  • [37] Deformation twinning to dislocation slip transition in single-crystal tantalum under dynamic compression
    Tang, M. X.
    Li, C.
    Cai, Y.
    Luo, S. N.
    JOURNAL OF MATERIALS SCIENCE, 2022, 57 (10) : 6026 - 6038
  • [38] Plastic Deformation of ⟨001⟩ Single-Crystal SrTiO3 by Compression at Room Temperature
    Yang, Kai-Hsun
    Ho, New-Jin
    Lu, Hong-Yang
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2011, 94 (09) : 3104 - 3111
  • [39] Deformation twinning to dislocation slip transition in single-crystal tantalum under dynamic compression
    M. X. Tang
    C. Li
    Y. Cai
    S. N. Luo
    Journal of Materials Science, 2022, 57 : 6026 - 6038
  • [40] Plastic deformation of 〈001〉 single-crystal SrTiO3 by compression at room temperature
    Department of Materials Science, Center for NanoScience and Technology, National Sun Yat-Sen University, Kaohsiung 80424, Taiwan
    J Am Ceram Soc, 1600, 9 (3104-3111):