Impact of surface ultrasonic rolling on cavitation erosion behavior of 304 stainless steel

被引:0
|
作者
Key Laboratory of Coal Processing and Efficient Utilization of Ministry of Education, China University of Mining and Technology, Xuzhou, Jiangsu, 221116, China [1 ]
School of Chemical Engineering and Technology, China University of Mining and Technology, Xuzhou, Jiangsu, 221116, China
机构
来源
基金
中国国家自然科学基金;
关键词
Cavitation - Erosion - Austenitic stainless steel - Corrosive effects - Passivation - Steel corrosion - Electrochemical corrosion - Energy transfer - Microstructure - Pitting - Corrosion resistance - Sodium chloride - Electrochemical impedance spectroscopy - Grain size and shape;
D O I
暂无
中图分类号
学科分类号
摘要
Surface ultrasonic rolling process (SURP) is a prior self-nano-technology of surface strengthening to improve the cavitation resistance of metal materials. In the paper, the 304 stainless steel (304SS) specimens were processed into 5 times, 10 times, 15 times and 20 times by SURP, then were cut into pieces along the SURP surface. In order to investigate impact of SURP on cavitation erosion behavior of 304SS, microstructure, mechanical properties and phase distribution of 304SS with difference SURP times were characterized firstly. Subsequently, ultrasonic cavitation erosion process and electrochemical measurements was experimented respectively: the specimens with different SURP times were subjected to 3 h in ore pulp solution (The mass fraction of 3.5% NaCl and 5% plumbum-zinc) by ultrasonic cavitation erosion process (UCEP), meanwhile, the electrochemical behaviors of the 304SS specimens with difference SURP times, such as open circuit potential (OCP), polarization curves and electrochemical impedance spectroscopy (EIS) were measured successively. Finally, the influences of the mechanical properties and corrosion characteristics of the 304SS with different microstructures after SURP on cavitation corrosion resistance were discussed in details, in the meantime, the microscopic mechanisms of the cavitation resistance for 304SS with different SURP times were investigated. The result shows that SURP is significantly beneficial to protect 304SS from the cavitation erosion behavior via introduction of deformation layers, transformation between martensite and austenitic, formation of passivation film, grain refinement and the surface hardness as well as residual stress of the 304SS were enhanced accordingly. However, the energy transfer of SURP is not only used to surface hardening, grain refinement, slip bands establishment but also defects formation, overmuch energy transfer plays the opposite role. Therefore SURP 10 times is a suitable SURP times that makes 304SS achieved optimal cavitation resistance. © 2019 Elsevier B.V.
引用
收藏
相关论文
共 50 条
  • [41] Inverse surface integrity problem in ultrasonic impact-treated AISI 304 stainless steel components
    Wang, G. Q.
    Zhu, X. P.
    Lei, M. K.
    Guo, D. M.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2016, 87 (5-8): : 2033 - 2040
  • [42] Inverse surface integrity problem in ultrasonic impact-treated AISI 304 stainless steel components
    G. Q. Wang
    X. P. Zhu
    M. K. Lei
    D. M. Guo
    The International Journal of Advanced Manufacturing Technology, 2016, 87 : 2033 - 2040
  • [43] Cavitation erosion behavior of WC coatings on CrNiMo stainless steel by laser alloying
    Zhang, Xiao-bin
    Liu, Chang-sheng
    Liu, Xiao-dong
    Dong, Jiang
    Yu, Bo
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2009, 16 (02) : 203 - 207
  • [44] Cavitation Erosion Behavior of Nb Strengthened Duplex Stainless Steel Surfacing Layer
    Yefeng Bao
    Chong Cao
    Bingqi Xie
    Zirui Wang
    Linpo Guo
    Ke Yang
    Qining Song
    Journal of Materials Engineering and Performance, 2022, 31 : 10367 - 10377
  • [45] Cavitation Erosion Behavior of Nb Strengthened Duplex Stainless Steel Surfacing Layer
    Bao, Yefeng
    Cao, Chong
    Xie, Bingqi
    Wang, Zirui
    Guo, Linpo
    Yang, Ke
    Song, Qining
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (12) : 10367 - 10377
  • [46] Mechanical and electrochemical behavior of nanocrystalline surface of 304 stainless steel
    Wang, XY
    Li, DY
    ELECTROCHIMICA ACTA, 2002, 47 (24) : 3939 - 3947
  • [48] In-situ study on cavitation erosion behavior of super ferritic stainless steel
    Wang, Zhenhua
    Zhang, Bing
    WEAR, 2021, 482
  • [49] INTERGRANULAR CAVITATION IN CREEP OF 304-STAINLESS STEEL
    CHEN, IW
    ARGON, AS
    JOURNAL OF METALS, 1979, 31 (08): : F51 - F51
  • [50] Ultrasonic Cavitation Erosion Behavior of GX40CrNiSi25-20 Cast Stainless Steel through Yb-YAG Surface Remelting
    Cosma, Daniela
    Mitelea, Ion
    Bordeasu, Ilare
    Utu, Ion Dragos
    Craciunescu, Corneliu Marius
    MATERIALS, 2024, 17 (17)