Effect of removing surface hardened layer on the fatigue strength of bearing steel SUJ2 ground specimen in the long life field

被引:11
|
作者
Goto, Masahiro [1 ]
Yamamoto, Takaei [1 ]
Nisitani, Hironobu [2 ]
Sakai, Tatsuo [3 ]
Kawagoishi, Norio [4 ]
机构
[1] Dept. of Mech. Eng., Oita Univ., Dan-noharu, Oita, 870-1192, Japan
[2] Dept. of Mech. Eng., Kyusyu-Sangyo Univ., Higashi-ku, Fukuoka, 813-8503, Japan
[3] Dept. of Mech. Eng., Ritsumeikan Univ., Nojihigashi, Kusatsu, 525-8577, Japan
[4] Dept. of Mech. Eng., Kagoshima Univ., Koorimoto, Kagoshima, 890-0065, Japan
关键词
Bending strength - Electrolytic polishing - Fatigue testing - Grinding (comminution) - Heat treatment - Residual stresses - Scanning electron microscopy - Strain hardening - Stress concentration - Surface roughness;
D O I
10.2472/jsms.49.786
中图分类号
学科分类号
摘要
In order to study the fatigue damage of a high carbon chromium bearing steel SUJ2, rotating bending fatigue tests of smooth specimens (Kt = 1.06, stress concentration factor) were carried out. The specimens were finished by the grinding after the heat-treatment. The fatigue strength of EP-0 (ground) specimen exhibited large scatter and it tended to drop again in the long-life field in excess of 107 cycles. In such a case, fish-eye was left on the fracture surface. In order to study the effect of surface hardened layer due to the grinding, two types of EP (electropolished) specimens, EP-15 specimen whose surface hardened layer and grinding flows were almost removed and EP-3 specimen which has the decreased surface roughness and surface hardened layer, were fatigued. The fatigue strength of EP-15 specimen was dramatically decreased when compared to the EP-0 specimen, and no drop in fatigue strength in the long-life field were observed. This indicates that the drop in fatigue strength in the long-life field results from the surface strengthened layer due to the grinding. On the other hand, S-N data of EP-3 specimen exhibit large scatter, but the range of scatter is smaller than that of EP-0 specimen. This narrowed scatter may be related to the decreased surface roughness of EP-3 specimen. Considering the experimental results of EP -15 and -3 specimens, the physical basis of peculiar S-N characteristics of EP-0 specimen was investigated.
引用
收藏
页码:786 / 792
相关论文
共 43 条
  • [41] The effect of SiC powder mixing electrical discharge machining on white layer thickness, heat flux and fatigue life of AISI D2 die steel
    Al-Khazraji, Ahmed
    Amin, Samir Ali
    Ali, Saad Mahmood
    ENGINEERING SCIENCE AND TECHNOLOGY-AN INTERNATIONAL JOURNAL-JESTECH, 2016, 19 (03): : 1400 - 1415
  • [42] Effect of MoS2 additive on electrical pitting mechanism of lubricated surface for Babbitt alloy/bearing steel pair under ac electric field
    Lin, CM
    Chiou, YC
    Lee, RT
    WEAR, 2004, 257 (7-8) : 833 - 842
  • [43] CREEP-FATIGUE STRENGTH OF LONG-TERM POST-SERVICE 2-BULLET-1/4CR-1-BULLET-MO STEEL AND REMAINING LIFE ESTIMATION
    OKAZAKI, M
    HASHIMOTO, M
    MOCHIZUKI, T
    JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 1991, 113 (04): : 549 - 555