Self-field AC power dissipation in high-TC superconducting tapes and a prototype cable

被引:0
|
作者
Awan, S.A. [1 ]
Sali, S. [1 ]
机构
[1] University of Newcastle upon Tyne, Department of Electrical and Electronic Engineering, Merz Court, Newcastle upon Tyne, NE1 7RU, United Kingdom
来源
关键词
Superconducting tapes - Critical current density (superconductivity) - High temperature superconductors - Electric losses;
D O I
10.2528/PIER01060602
中图分类号
学科分类号
摘要
The measured self-field AC power dissipation in superconducting BiSrCaCuO-2223/Ag tapes and a prototype cable is cable is compared with theoretical models. A brief overview of the theoretical background for AC loss calculations in superconductor tapes with different geometrical shapes is also discussed. New models for the harmonic components of the fundamental frequency and the current dependent non-linear inductance are also derived. It is shown that the latter models can be used to estimate current distribution and the variation of flux penetration in superconducting tapes. Two separate experimental apparatus were designed and constructed for measurements on tapes and prototype cable systems. The observed losses in tapes are reasonably well described by models based on the Critical State Model (CSM). In contrast, the measured losses in the prototype cable are found to be a factor of approximately two higher the predicted values. Further investigations showed that this may be due to inhomogeneous contact resistance between individual tapes and the current joints and the variation in critical current density (JC) distribution between tapes. The significance of current dependence of the loss component, inductive quadrature component, phase error in measurements and the definition of the critical current in the prototype cable are also discussed.
引用
收藏
页码:81 / 100
相关论文
共 50 条
  • [41] Blistering phenomenon in BiSCCO-2223 high-Tc superconducting tapes
    Hebrew Univ of Jerusalem, Jerusalem, Israel
    Supercond Sci Technol, 7 (549-554):
  • [42] CURRENT, INDUCTION PROFILES AND HYSTERETIC LOSSES IN HIGH-TC SUPERCONDUCTING TAPES
    LEVILLAIN, C
    MANUEL, P
    THEROND, PG
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 1995, 5 (02) : 705 - 708
  • [43] Materials for classical and high-Tc superconducting tapes and wires at 4.2 K
    Flukiger, R
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 1997, 10 (12): : 872 - 875
  • [44] Electrical insulation characteristics of a high-Tc superconducting DC cable
    Kwag, D. -S.
    Cheon, H. -G.
    Choi, J. -H.
    Kim, H. -J.
    Cho, J. -W.
    Kim, S. -H.
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2008, 18 (02) : 1402 - 1405
  • [45] Advances in Bi-based high-Tc superconducting tapes and wires
    Kitaguchi, H
    Kumakura, H
    MRS BULLETIN, 2001, 26 (02) : 121 - 125
  • [46] The influence of the bending process on the critical current of high-Tc superconducting tapes
    Sosnowski, J
    PHYSICA C-SUPERCONDUCTIVITY AND ITS APPLICATIONS, 2003, 387 (1-2): : 239 - 241
  • [47] LAYERED HIGH-TC SUPERCONDUCTORS IN AN AC FIELD
    SIMONOV, AY
    PHYSICA C, 1993, 211 (3-4): : 455 - 466
  • [48] Advances in Bi-Based High-Tc Superconducting Tapes and Wires
    Hitoshi Kitaguchi
    Hiroaki Kumakura
    MRS Bulletin, 2001, 26 : 121 - 125
  • [49] Ac-loss and time constant measuring techniques of high-Tc tapes and stacks of tapes
    Schmidt, Curt
    PHYSICA C-SUPERCONDUCTIVITY AND ITS APPLICATIONS, 2006, 445 : 694 - 700
  • [50] AC response of the vortex liquid in the high-Tc superconducting cylinder
    Wu, Chien-Jang
    Tseng, Tseung-Yuen
    Physica C: Superconductivity and its Applications, 1996, 260 (1-2): : 8 - 18