Effects of wear speeds on friction-wear behaviours of cathode arc ion plated TiAlSiN coatings at high temperatures

被引:5
|
作者
Chengjian T. [1 ]
Dejun K. [1 ,2 ]
机构
[1] School of Mechanical Engineering, Changzhou University, Changzhou
[2] Jiangsu Key Laboratory of Materials Surface Science and Technology, Changzhou University, Changzhou
来源
Dejun, Kong (djkong@cczu.edu.cn) | 1600年 / Taylor and Francis Ltd.卷 / 11期
关键词
Cathodic arc ion plating (CAIP); high temperature; TiAlSiN coating; wear mechanism; wear speed;
D O I
10.1080/17515831.2017.1302683
中图分类号
学科分类号
摘要
A TiAlSiN coating was deposited on AISI H13 hot work mould steel using a cathodic arc ion plating (CAIP). The microstructures, chemical composition and phases of the obtained coatings were analysed using a field emission scanning electronic microscope, energy dispersive spectrometer (EDS) and X-ray diffractometer, respectively. The high temperature friction-wear properties of TiAlSiN coating at the different wear speeds were investigated, and the wear mechanism was also discussed. The results show that the N of the TiAlSiN coating is not completely released at 800 °C, the diffraction peak of TiN still exists in this coating. In addition, the products of SiO2 and Al2O3 play a role of self-lubricating and wear resistance. The average coefficient of friction (COF) of the coatings at the wear speeds of 400, 600, and 800 r/min is 0.15, 0.22, and 0.17, respectively. The wear mechanism of TiAlSiN coating at 800 °C is primarily adhesive wear, accompanied by oxidation wear and abrasive wear. © 2017 Informa UK Limited, trading as Taylor & Francis Group.
引用
收藏
页码:66 / 74
页数:8
相关论文
共 50 条
  • [21] COATINGS FOR FRICTION AND WEAR CONTROL AT HIGH-TEMPERATURES
    SLINEY, HE
    SURFACE & COATINGS TECHNOLOGY, 1987, 33 (1-4): : 243 - 244
  • [22] Friction-Wear Behaviors of Chemical Vapor Deposited Diamond Films at High Temperatures
    Kong Dejun
    Zhao Wen
    Zhang Ling
    Journal of Superhard Materials, 2019, 41 : 98 - 105
  • [23] WEAR-RESISTANCE OF ARC ION-PLATED CHROMIUM NITRIDE COATINGS
    CHIBA, Y
    OMURA, T
    ICHIMURA, H
    JOURNAL OF MATERIALS RESEARCH, 1993, 8 (05) : 1109 - 1115
  • [24] Friction-Wear Behaviors of Chemical Vapor Deposited Diamond Films at High Temperatures
    Kong Dejun
    Zhao Wen
    Zhang Ling
    JOURNAL OF SUPERHARD MATERIALS, 2019, 41 (02) : 98 - 105
  • [25] Friction-wear behaviours of micro-arc oxidation films in situ grown on 7475 aluminium alloys
    Dejun, K.
    Jing, Z.
    Hao, L.
    MATERIALS TECHNOLOGY, 2017, 32 (12) : 737 - 743
  • [26] Effects of loads on friction-wear properties of HVOF sprayed FeCrBSi coating at elevated temperatures
    Luo Yuntian
    Xu Jianyan
    Kong Dejun
    MATERIALS RESEARCH EXPRESS, 2019, 6 (09)
  • [27] Influence of Y on microstructure and performance of friction and wear of arc ion plated TiAIN film
    Guo, Ce-An
    Zhao, Zong-Ke
    Hu, Ming
    Shang, Guang-Ming
    Zhou, Feng
    Zhang, Jian
    Surface Technology, 2018, 47 (10): : 139 - 144
  • [28] Characterization and friction-wear behaviors of cathodic arc ion plated AlCrTiN coating on HVOF sprayed WC-12Co coating at elevated temperatures (vol 5, 096402, 2018)
    Kong Weicheng
    Shen Hui
    MATERIALS RESEARCH EXPRESS, 2018, 5 (10):
  • [29] The friction and wear characteristics of cathodic arc ion-plated (V, Ti)N coatings in sliding against alumina ball
    Ouyang, JH
    Sasaki, S
    WEAR, 2004, 257 (7-8) : 708 - 720
  • [30] High-Speed Laser Cladded Ni-Based WC Coatings: Microstructure, Friction-Wear Property and Wear Mechanism
    Zhang, Kaiwei
    Kong, Dejun
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2024, 33 (07) : 2367 - 2379