Mechanical properties and life cycle assessment (LCA) of waste glass reinforced concrete

被引:2
|
作者
Jin, Zhipeng [1 ]
Liang, Kaikang [2 ]
Liu, Ce [1 ]
Yang, Guangzhao [3 ]
Cui, Kai [4 ]
Mao, Shihua [1 ]
机构
[1] Southwest Forestry Univ, Sch Civil Engn, Kunming 650224, Peoples R China
[2] City Univ Hong Kong, Dept Architecture & Civil Engn, Hong Kong, Peoples R China
[3] Guangzhou Inst Bldg Sci Co Ltd, Guangzhou 510080, Peoples R China
[4] Hong Kong Polytech Univ, Dept Civil & Environm Engn, Hung Hom, Kowloon, Hong Kong, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
Waste glass power (WGP); Mechanical properties of concrete; Life cycle assessment (LCA); Glass fiber (GF); Energy storage; CEMENT; DURABILITY; POWDER;
D O I
10.1016/j.jobe.2024.110643
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
As global warming continues and construction drains large quantities of natural resources, waste glass, a kind of solid waste that is difficult to degrade naturally, is gradually being used to alleviate the pressure of natural resource shortage. Waste glass powder (WGP) and glass fiber (GF) have been widely used in concrete production. This study aims to use WGP to replace traditional fine aggregates (FAs) and explore the effects of WGP and 1 % GF added alone and mixed at different replacement amounts on the mechanical properties (compressive strength, splitting tensile strength, and flexural strength) of concrete at different ages (7d and 28d) and observe the failure morphology. Water absorption tests are conducted to study their pore structures. While studying their mechanical properties and pore structures, considering the recycling of solid waste, the life cycle assessment (LCA) method is used to explore whether the replacement of WGP can achieve green environmental protection goals. The environmental impact of different types of concrete is evaluated to ensure that the mechanical properties of concrete will be further improved under the premise of green and low carbon. The results show that the mixed use of WGP and GF reduces the compressive strength of concrete, but the splitting tensile strength and flexural strength are improved. At 28 days, compared with ordinary concrete (F0G0), the splitting tensile strength and flexural strength of concrete with only added GF (F1G0) increased by 10.7% and 13.5%, respectively. When GF was mixed with 10 % WGP (F1G10), the flexural strength and splitting tensile strength increased by 21.5 % and 24.6 %, respectively. The main body of the concrete containing GF is intact (F1G0, F1G10, F1G20, F1G30), the crack width is thinner than that of F0G0, and the sound is deeper when it is destroyed. The water absorption rate of glass fiber-waste glass power concrete (F1G20) with a replacement amount of 20 % was the lowest, which was 6.1 % lower than that of F0G0. The LCA results show that concrete has an excellent influence on the environment when preparing concrete. Using alternative materials such as WGP to reduce the amount of FAs can reduce carbon emissions. The carbon emissions of FAs in F1G30 are 30% lower than that of F0G0.
引用
收藏
页数:19
相关论文
共 50 条
  • [31] Abrasion Resistance and Mechanical Properties of Waste-Glass-Fiber-Reinforced Roller-compacted Concrete
    S. A. Yildizel
    O. Timur
    A. U. Ozturk
    Mechanics of Composite Materials, 2018, 54 : 251 - 256
  • [32] Abrasion Resistance and Mechanical Properties of Waste-Glass-Fiber-Reinforced Roller-compacted Concrete
    Yildizel, S. A.
    Timur, O.
    Ozturk, A. U.
    MECHANICS OF COMPOSITE MATERIALS, 2018, 54 (02) : 251 - 256
  • [33] Mechanical and fracture properties of glass fiber reinforced geopolymer concrete
    Midhun, M. S.
    Rao, T. D. Gunneswara
    Srikrishna, T. Chaitanya
    ADVANCES IN CONCRETE CONSTRUCTION, 2018, 6 (01) : 29 - 45
  • [34] MECHANICAL PROPERTIES OF WASTE PLASTIC BANNER FIBER REINFORCED CONCRETE
    Setiawan, Agustinus Agus
    Philip, Fredy Jhon
    Permanasari, Eka
    JURNAL TEKNOLOGI, 2018, 80 (05): : 113 - 119
  • [35] Mechanical Properties of Glass Fiber Reinforced Concrete with Recycled Aggregates
    Garg, Anshul
    Sharma, Pushpendra Kumar
    JOURNAL OF APPLIED SCIENCE AND ENGINEERING, 2021, 24 (06): : 1033 - 1039
  • [36] Life cycle assessment on recycled e-waste concrete
    Goh, Pei Gy
    Maghfouri, Mehdi
    Onn, Chiu Chuen
    Loo, Siaw Chuing
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2022, 17
  • [37] Use of waste glass as coarse aggregate in concrete: mechanical properties
    Yan, Lan-Ian
    Liang, Jiong-Feng
    ADVANCES IN CONCRETE CONSTRUCTION, 2019, 8 (01) : 1 - 7
  • [38] Influence of Replacing Cement with Waste Glass on Mechanical Properties of Concrete
    Zeybek, Ozer
    Ozkilic, Yasin Onuralp
    Karalar, Memduh
    Celik, Ali Ihsan
    Qaidi, Shaker
    Ahmad, Jawad
    Burduhos-Nergis, Dumitru Doru
    Burduhos-Nergis, Diana Petronela
    MATERIALS, 2022, 15 (21)
  • [39] Mechanical and durability properties of concrete incorporating glass and plastic waste
    Abdelli, Houssam Eddine
    Mokrani, Larbi
    Kennouche, Salim
    de Aguiar, J. L. Barroso
    ADVANCES IN CONCRETE CONSTRUCTION, 2021, 11 (02) : 173 - 181
  • [40] Studies on mechanical properties of concrete containing waste glass aggregate
    Park, SB
    Lee, BC
    Kim, JH
    CEMENT AND CONCRETE RESEARCH, 2004, 34 (12) : 2181 - 2189