Experimental and Theoretical Calculation of Bonding Performance between Threaded GFRP Bars and Concrete

被引:0
|
作者
Song Z. [1 ]
Lu C. [1 ]
Xuan G. [1 ]
Cai Q. [1 ]
Bu S. [1 ]
机构
[1] Faculty of Civil Engineering and Mechanics, Jiangsu University, Zhenjiang
关键词
Bonding performance; Glass fiber reinforced polymer(GFRP) bar; Pullout test; Strength prediction; Theoretical model;
D O I
10.3969/j.issn.1007-9629.2021.04.029
中图分类号
学科分类号
摘要
In order to study the bonding performance of the threaded glass fiber reinforced polymer(GFRP) bar and the concrete interface, three groups of pullout specimens were prepared from several GFRP bars of different diameters. A central pullout test was conducted on these specimens after 28d standard curing. Experimental results show that the bonding strength between GFRP bar and concrete increases as the bar diameter increases. The failure modes and bonding stress-slip curves of GFRP bars of different diameters change accordingly. For the GFRP bars with small diameters of 8mm and 12mm, the tested specimens are mainly pulled out and damaged, but the bonding stress-slip curves in the two cases also differ greatly after the stage of elastic rise. The test specimens of the diameter of 8mm tend to fluctuate back and forth, and gradually flatten. While the bonding stress of the pullout specimen with a bar of diameter of 12mm continues to rise and then decreases, showing a hyperbolic mode. When the diameter of GFRP bars becomes larger(16mm), the splitting damage appeares in the specimens tested. After the bonding stress-slip curve rises to the highest point, the bonding stress decreases rapidly. Finally, based on the theoretical model of the thick-walled cylinder of elastic mechanics, the angle of the bonding failure surface of the threaded GFRP bars of different diameters was discussed and the formula for calculating the bonding strength was proposed. The comparative analysis with the relevant test results verifies that the calculation formula has excellent prediction accuracy for specimens with pullout failure. © 2021, Editorial Department of Journal of Building Materials. All right reserved.
引用
收藏
页码:887 / 894
页数:7
相关论文
共 35 条
  • [21] MASMOUDI R, MASMOUDI A, OUEZDOU M B, Et al., Long-term bond performance of GFRP bars in concrete under temperature ranging from 20 C to 80 C, Construction and Building Materials, 25, 2, pp. 486-493, (2011)
  • [22] ZHANG Meizhen, Experimental study on bond-slip behavior between FRP bar and concrete based on intelligent bars, (2014)
  • [23] WANG Yinglai, Experimental study on tensile properties of FRP bars and bond behavior between and concrete after high temperature, (2013)
  • [24] GU Hongxue, Tensile property of FRP tendons and bond behavior between FRP tendons and concrete, (2015)
  • [25] HAO Qingduo, WANG Yanlei, Experimental investigation on bond strength between GFRP rebars and concrete under pullout conditions, Journal of Building Structures, 29, 1, pp. 103-111, (2008)
  • [26] ZHANG Yu, Experimental Study on the bond performance theory between GFRP bar and concrete, (2016)
  • [27] SHI Xiaoquan, ZHANG Zhiqiang, LI Zhiye, Et al., Pulling test study on bonding performance of GFRP bar and concrete, Railway Engineering, 10, pp. 133-136, (2010)
  • [28] WANG Bo, Experimental study on the bond behavior between GFRP bars and concrete, Industrial Construction, pp. 134-137, (2009)
  • [29] KUANG Y C, OU L W, HU J X., Experimental and numerical analysis on the bonding performance of GFRP bolts, Applied Mechanics and Materials, 777, pp. 166-172, (2015)
  • [30] LI S, ZHANG M Z., Experimental research on bond performance between GFRP bar and concrete under single-ended pullout conditions, The 2013 World Congress on Advances in Structural Engineering and Mechanics(ASEM13), pp. 8-12, (2013)