The processability of highly spherical gas-atomized ti-6al-4v alloy powder in laser powder bed fusion

被引:0
|
作者
Nakamura K. [1 ]
Ikeshoji T.-T. [2 ]
Sekimoto K. [3 ]
Okumura T. [3 ]
Kyogoku H. [2 ]
机构
[1] Kindai University Hiroshima Branch, Technology Research Association for Future Additive Manufacturing, 1 Takaya-Umenobe, Higashihiroshima
[2] Fundamental Technology for Next Generation Research Institute, Kindai University, 1 Takaya-Umenobe, Higashihiroshima
[3] Corporate Research & Development Center, Daido Steel Co., Ltd., 30 Daido-cho 2-chome, Minami-ku, Nagoya
关键词
Gas-atomized powder; Laser powder bed fusion; Mechanical properties; Process map; Titanium alloy;
D O I
10.2497/jjspm.67.424
中图分类号
学科分类号
摘要
The powder characteristics are one of the most important factors to affect the processability in additive manufacturing technology, especially in laser powder bed fusion. In this research, the influence of highly spherical gas-atomized Ti-6Al-4V alloy powder on the processability in laser powder bed fusion was investigated. The cubic specimens of highly spherical gas-atomized Ti-6Al-4V alloy powder were fabricated at various laser power and scan-speed using a laser powder bed fusion type machine with 1 kW fiber laser, and examined the density and surface roughness of the cubic specimens. As a result, the optimum fabrication condition was obtained using the process map evaluated by the density and surface roughness of the cubic specimen. The alloy fabricated at a laser power of 150 W and a scan speed of 700 mm/s showed the maximum relative density of 99.94% and the surface roughness, Sa, of about 5 µm. The tensile strength and elongation of the as-built alloy were more than 1300 MPa and 8%, respectively. It was thus found that the use of highly spherical gas-atomized powder greatly improves the density, surface roughness and tensile properties of the as-built alloy. © 2020 Japan Society of Powder and Powder Metallurgy
引用
收藏
页码:424 / 430
页数:6
相关论文
共 50 条
  • [21] Raking process for Powder Bed Fusion of Ti-6Al-4V alloy Powder Analyzed by Discrete Element Method
    Okugawa M.
    Isono Y.
    Koizumi Y.
    Nakano T.
    Keikinzoku/Journal of Japan Institute of Light Metals, 2022, 72 (06): : 291 - 297
  • [22] Dynamic a globularization in laser powder bed fusion additively manufactured Ti-6Al-4V
    Chen, J.
    Fabijanic, D.
    Brandt, M.
    Zhao, Y.
    Ren, S. B.
    Xu, W.
    ACTA MATERIALIA, 2023, 255
  • [23] Investigation of Microstructure and Mechanical Properties for Ti-6Al-4V Alloy Parts Produced Using Non-Spherical Precursor Powder by Laser Powder Bed Fusion
    Varela, Jaime
    Arrieta, Edel
    Paliwal, Muktesh
    Marucci, Mike
    Sandoval, Jose H.
    Gonzalez, Jose A.
    McWilliams, Brandon
    Murr, Lawrence E.
    Wicker, Ryan B.
    Medina, Francisco
    MATERIALS, 2021, 14 (11)
  • [24] Laser surface polishing of Ti-6Al-4V parts manufactured by laser powder bed fusion
    Obeidi, Muhannad Ahmed
    Mussatto, Andre
    Dogu, Merve Nur
    Sreenilayam, Sithara P.
    McCarthy, Eanna
    Ul Ahad, Inam
    Keaveney, Shane
    Brabazon, Dermot
    SURFACE & COATINGS TECHNOLOGY, 2022, 434
  • [25] A study on surface morphology and tension in laser powder bed fusion of Ti-6Al-4V
    Khorasani, Mahyar
    Ghasemi, AmirHossein
    Awan, Umar Shafique
    Hadavi, Elahe
    Leary, Martin
    Brandt, Milan
    Littlefair, Guy
    O'Neil, William
    Gibson, Ian
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2020, 111 (9-10): : 2891 - 2909
  • [26] Interplay of strain and phase evolution of laser powder bed fusion Ti-6Al-4V
    Andrews, C.
    Heo, T. W.
    Shi, R.
    Basgul, C.
    Kurtz, S.
    Matthews, M. J.
    Taheri, M. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 855
  • [27] A study on surface morphology and tension in laser powder bed fusion of Ti-6Al-4V
    Mahyar Khorasani
    AmirHossein Ghasemi
    Umar Shafique Awan
    Elahe Hadavi
    Martin Leary
    Milan Brandt
    Guy Littlefair
    William O’Neil
    Ian Gibson
    The International Journal of Advanced Manufacturing Technology, 2020, 111 : 2891 - 2909
  • [28] Influence of laser post-processing on pore evolution of Ti-6Al-4V alloy by laser powder bed fusion
    Shen, Bingnan
    Li, Hui
    Liu, Sheng
    Zou, Jing
    Shen, Shengnan
    Wang, Yinghe
    Zhang, Tao
    Zhang, Dongqi
    Chen, Yinghua
    Qi, Haiqin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 818 (818)
  • [29] Deciphering the transformation pathway in laser powder-bed fusion additive manufacturing of Ti-6Al-4V alloy
    Chen, J.
    Fabijanic, D.
    Zhang, T.
    Lui, E. W.
    Brandt, M.
    Xu, W.
    ADDITIVE MANUFACTURING, 2022, 58
  • [30] TENSILE AND FATIGUE PROPERTIES OF Ti-6Al-4V ALLOY FABRICATED BY LASER POWDER-BED FUSION PROCESS
    Rahman, M. Shafiqur
    Chakravarty, Uttam K.
    PROCEEDINGS OF THE ASME 2020 INTERNATIONAL MECHANICAL ENGINEERING CONGRESS AND EXPOSITION, IMECE2020, VOL 4, 2020,