Enhanced photocatalytic activity of FeSO4 in a ZnO photocatalyst with H2O2 for dye degradation

被引:5
|
作者
Domínguez-Talamantes D.G. [1 ]
Vargas-Hernández D. [2 ]
Hernández-Oloño J.T. [1 ]
Rodríguez-Castellón E. [3 ]
Arellano-Cortaza M. [4 ]
Castillo S.J. [5 ]
Tánori-Córdova J.C. [1 ]
机构
[1] Departamento de Investigación en Polímeros y Materiales, Universidad de Sonora, Boulevard Luis Encinas Johnson y Rosales S/N, Sonora, Hermosillo
[2] CONAHCYT-Universidad de Sonora, Boulevard Luis Encinas Johnson y Rosales S/N, Sonora, Hermosillo
[3] Departamento de Química Inorgánica, Cristalografía y Mineralogía, Facultad de Ciencias, Universidad de Málaga, Campus de Teatinos, Málaga
[4] Universidad Juárez Autónoma de Tabasco, Avenida Universidad S/n Zona de La Cultura, Colonia Magisterial, CP, Tabasco, Villahermosa Centro
[5] Departamento de Investigación en Física, Universidad de Sonora, Boulevard Luis Encinas Johnson y Rosales S/N, Sonora, Hermosillo
来源
Optik | 2024年 / 304卷
关键词
Heterogeneous photo-Fenton; Photocatalyst; Methyl orange; Methylene blue; Scavengers;
D O I
10.1016/j.ijleo.2024.171753
中图分类号
学科分类号
摘要
In this study, the photocatalytic degradation efficiency of ZnO synthesized by a hydrothermal method and iron-supported ZnO catalysts by an impregnation method, dried (D) and calcined (C), was evaluated, through the degradation of methylene blue (MB) and methyl orange (MO) molecules under UV irradiation. The catalysts were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray photoelectron spectroscopy (XPS), N2 adsorption-desorption, and UV[sbnd]visible diffuse reflectance spectroscopy (DRS). XRD showed that FeSO4 is supported on ZnO, and the XPS study revealed higher concentrations of hydroxyl groups and Fe3+ for the dried catalyst. The bandgap energies were 3.24, 3.23, and 3.19 eV for ZnO, Fe/ZnO D and Fe/ZnO C, respectively. The results revealed that Fe/ZnO D with H2O2 exhibited a higher photocatalytic degradation efficiency than ZnO, achieving 97% and 99% degradation for MB and MO at 10 min, which implies that the integrated iron in ZnO serves as an electron-hole separator. In addition, the catalyst has a larger BET specific area, the presence of hydroxyl groups and sulfate ions on the surface of the catalyst with holes forms hydroxyl radicals (•OH), and the presence of Fe3+ on the surface catalyst with H2O2 produces more •OH radicals. •OH radicals are the major oxidation species in this process, which promotes the degradation of dyes. The photocatalytic dye degradation efficiency was also evaluated for various catalyst doses, dye concentrations and solution pH values. Moreover, the stability of the catalyst over repeated cycles of dye treatment was demonstrated. © 2024 Elsevier GmbH
引用
收藏
相关论文
共 50 条
  • [41] Kinetics of thermal decomposition of FeSO4 center dot 7H(2)O
    Straszko, J
    OlszakHumienik, M
    Mozejko, J
    INZYNIERIA CHEMICZNA I PROCESOWA, 1996, 17 (03): : 517 - 528
  • [42] Crystallization kinetics of FeSO4·7H2O in black titanium solution
    Song, Xingfu, 1600, Materials China (65):
  • [43] 利用H2O2和FeSO4处理环氧大豆油生产的废水
    阮爱珍
    广州化工, 1998, (01) : 46 - 49+36
  • [44] Indanthrene Blue Dye Degradation by UV/H2O2 Process: H2O2 as a Single or Fractioned Aliquot?
    Almeida, Caio Vinicius da S.
    Macedo, Matheus S.
    Eguiluz, Katlin Ivon B.
    Salazar-Banda, Giancarlo R.
    Queissada, Daniel D.
    ENVIRONMENTAL ENGINEERING SCIENCE, 2015, 32 (11) : 930 - 937
  • [45] Synthesis of heterostructured Bi2O3-CeO2-ZnO photocatalyst with enhanced sunlight photocatalytic activity
    Hezam, Abdo
    Namratha, K.
    Drmosh, Q. A.
    Yamani, Z. H.
    Byrappa, K.
    CERAMICS INTERNATIONAL, 2017, 43 (06) : 5292 - 5301
  • [46] H2O2/UV enhanced degradation of pesticides in wastewater
    Kowalska, E
    Janczarek, M
    Hupka, J
    Grynkiewicz, M
    WATER SCIENCE AND TECHNOLOGY, 2004, 49 (04) : 261 - 266
  • [47] Photocatalytic degradation of organic dye and phytohormone by a Cu(II) complex powder catalyst with added H2O2
    Wang, Dawei
    Zhao, Ping
    Yang, Jing
    Xu, Gaofeng
    Yang, Haiyan
    Shi, Zhengjun
    Hu, Qian
    Dong, Binbin
    Guo, Zhanhu
    COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS, 2020, 603
  • [48] Enhanced photocatalytic degradation performance of In2O3/g-C3N4 composites by coupling with H2O2
    Liu, Wei
    Zhang, Jin
    Kang, Qun
    Chen, Hongbing
    Feng, Ru
    ECOTOXICOLOGY AND ENVIRONMENTAL SAFETY, 2023, 252
  • [49] Photocatalytic Degradation of Malachite Green Dye with UV/H2O2 System in presence of Transition Metal Ions
    Waheed-Uz-Zaman
    Dar, Amara
    Anwar, Jamil
    Munir, Ayesha
    JOURNAL OF THE CHEMICAL SOCIETY OF PAKISTAN, 2023, 45 (04): : 302 - 308
  • [50] UV/H2O2 degradation of diclofenac in a photocatalytic fuel cell
    Dhawle, Rebecca
    Mantzavinos, Dionissios
    Lianos, Panagiotis
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2021, 299