Investigations on the machinability performance of Al2O3/TiCN CVD coated carbide tools in sustainable high-speed hard-turning of AISI 4340 alloy steel

被引:0
|
作者
Jouini, Nabil [1 ]
Yaqoob, Saima [2 ]
Ghani, Jaharah A. [3 ]
机构
[1] Prince Sattam bin Abdulaziz Univ, Coll Engn, Mech Engn Dept, Alkharj 11942, Saudi Arabia
[2] NED Univ Engn & Technol, Dept Ind & Mfg Engn, Karachi, Pakistan
[3] Univ Kebangsaan Malaysia, Fac Engn & Built Environm, Dept Mech & Mfg Engn, Bangi 43600, Selangor, Malaysia
关键词
carbide tool; tool life; cutting force; surface roughness; tool wear; INSERTS; WEAR; PVD;
D O I
10.1088/2053-1591/ad7657
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study investigates the effectiveness of CVD coated carbide inserts in turning hardened AISI 4340 steel at high-machining speed V = 300, 350 m min(-1) under sustainable dry cutting environment. Experiments were executed in accordance to Taguchi L-4 orthogonal array and crucial machinability aspects tool life, tool wear progression and mechanism, cutting force, and surface roughness were evaluated in detail. The results of this study revealed that Al2O3/TiCN coating successfully inhibited the faster progression of tool wear at low cutting speed (300 m min(-1)), feed rate (0.05 mm rev(-1)) and depth of cut (0.1 mm), thus delivering the highest tool life of 19.25 min and lowest cutting force of 76.8 N. However, better surface finish of 0.305 mu m was obtained at high cutting speed (350 m min(-1)), low feed rate (0.05 mm rev(-1)), and high depth of cut (0.1 mm). Nevertheless, at high cutting speed (350 m min(-1)) and feed rate (0.1 mm rev(-1)), involvement of intense thermal-mechanical effects suppressed the effectiveness of coating and tool completed its useful life at 9.24 min. Severe flaking on the cutting edge was observed at high machining parameters. Scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) analysis revealed that adhesion, oxidation, and small scale chipping and abrasion were the primary wear mechanisms attributing in competing the tool life criteria (Vb = 300 mu m) in all cutting conditions. Furthermore, it was established that the cutting force and surface roughness increased with increasing tool flank wear due to coating delamination, material adhesion and tool chipping. This research emphasizes the significant potential of adopting Al2O3/TiCN coated carbide inserts for high-speed industrial hard-turning of AISI 4340 steel.
引用
收藏
页数:9
相关论文
共 50 条
  • [31] Machinability investigation of Chromoly steel using TiN/Al2O3/TiCN/TiOCN multilayer coated tungsten carbide tool inserts with artificial neural network methodology
    Singh, Nikhil
    Bharatish, A.
    Rajkumar, G. R.
    Babu, G. Satheesh
    APPLIED RESEARCH, 2023, 2 (04):
  • [32] Multi-objective optimization of cutting parameters when machining cold work steel with CVD-coated carbide (Al2O3/TiC/TiCN)
    Safi, Khaoula
    Yallese, Mohammed A.
    Belhadi, Salim
    Boutabba, Smail
    Mabrouki, Tarek
    UPB Scientific Bulletin, Series D: Mechanical Engineering, 2021, 83 (01): : 149 - 168
  • [33] FRACTURE-RESISTANCE OF AL2O3 REINFORCED HIGH-SPEED STEEL
    QUEENEY, RA
    MILLER, JL
    BELTZ, RJ
    DANKOFF, JD
    1989 ADVANCES IN POWDER METALLURGY, VOLS 1-3, 1989, 1-3 : B345 - B354
  • [34] Dry Machining Performance of AA7075-T6 Alloy Using Uncoated Carbide and MT-CVD TiCN-Al2O3-Coated Carbide Inserts
    Sahoo, Sarthak Prasad
    Datta, Saurav
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2020, 45 (11) : 9777 - 9791
  • [35] Dry Machining Performance of AA7075-T6 Alloy Using Uncoated Carbide and MT-CVD TiCN-Al2O3-Coated Carbide Inserts
    Sarthak Prasad Sahoo
    Saurav Datta
    Arabian Journal for Science and Engineering, 2020, 45 : 9777 - 9791
  • [36] Performance of Al2O3/TiC mixed ceramic inserts coated with TiAlSiN, WC/C and DLC thin solid films during hard turning of AISI 52100 steel
    Kumar, Ch Sateesh
    Patel, Saroj Kumar
    Fernandes, Filipe
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 19 : 3380 - 3393
  • [37] Microstructures and properties of CVD TiN–TiCN–Al2O3 coated WC-8wt%Co-xRu cemented carbide
    Xiuxian Chen
    Ji Xiong
    Zhixing Guo
    Junbo Liu
    Lu Yang
    Qianbing You
    Journal of Materials Science, 2023, 58 : 8317 - 8330
  • [38] Optimization of process parameters in CNC turning process on machining SCM440 steel by uncoated carbide and TiCN/Al2O3/TiN coated carbide tool under dry conditions
    Arunnath, A.
    Masooth, P. Haja Syeddu
    MATERIALS TODAY-PROCEEDINGS, 2021, 45 : 6253 - 6269
  • [39] Experimental Study on High-speed Turning of Free-cutting Steel AISI 12L14 Using Multi-layer Coated Carbide Tools
    Xu, Jinyang
    An, Qinglong
    Chan, Ming
    ADVANCES IN MATERIALS PROCESSING X, 2012, 500 : 3 - +
  • [40] Performance and wear mechanisms of uncoated, TiAlN, and AlTiN-coated carbide tools in high-speed drilling of Al-Si alloy
    Ali Akhavan Farid
    Safian Sharif
    Mohd Hasbullah Idris
    The International Journal of Advanced Manufacturing Technology, 2021, 113 : 2671 - 2684