Effects of CaF2 and La2O3 on the phase structure of rare earth in CaO-SiO2-La2O3-CaF2 slags

被引:0
|
作者
Wang, Jinming [1 ,2 ,3 ]
Liu, Xiangjun [4 ]
Guo, Wentao [2 ,3 ,5 ]
Zhao, Zengwu [2 ,3 ,6 ]
Sun, Zuolin [5 ]
机构
[1] Inner Mongolia Univ Sci & Technol, Sch Rare Earth Ind, Baotou, Peoples R China
[2] Inner Mongolia Univ Sci & Technol, Inner Mongolia Autonomous Reg Carbon Neutral Colla, Baotou, Peoples R China
[3] Inner Mongolia Univ Sci & Technol, Key Lab Green Extract & Efficient Utilizat Light R, Baotou, Peoples R China
[4] Inner Mongolia Univ Sci & Technol, Sch Mech Engn, Baotou, Peoples R China
[5] Inner Mongolia Univ Sci & Technol, Sch Mat Sci & Engn, Baotou, Peoples R China
[6] Inner Mongolia Univ Technol, Sch Mat Sci & Engn, Hohhot, Peoples R China
关键词
CaF2; La2O3; rare earth phase; structure; viscosity; CRYSTALLIZATION BEHAVIOR;
D O I
10.1177/03019233241283594
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The rare earth in the rare earth slag can be separated and enriched by heating and melting the rare earth slag and then slowly cooling crystallisation. In this process, it is of great significance to study the effect of chemical composition on the crystallisation of rare earth phase in slag and the effect of slag viscosity on crystal growth. The rare earth slag melt samples were prepared according to the main chemical composition of rare earth slag by using an analytical pure reagent. The effects of CaF2 and La2O3 contents on the phase structure and morphology of rare earth phase in CaO-SiO2-La2O3-CaF2 slags were studied by SEM-EDS and XRD. The relationship between the viscosity of the slag and the crystal growth behaviour was studied by measuring the melt viscosity with the cylinder rotation method. The results show that the rare earth in CaO-SiO2-La2O3-CaF2 slags exists in the form of CaLa4(SiO4)(3)O. The change of CaF2 and La2O3 content has no effect on the structure of rare earth phase, but the size of rare earth crystal phase changes obviously. With the increase of CaF2 and La2O3 content, the size of rare earth crystal phase increases gradually. CaF2 and La2O3 can reduce the viscosity transition temperature of slag melt and increase the crystallisation temperature range of rare earth phase to promote crystal growth.
引用
收藏
页数:7
相关论文
共 50 条
  • [31] DETERMINATION OF THE VISCOSITY OF CaF2-CaO-La2O3 TERNARY SLAGS AND AN INVESTIGATION OF PHASE CHARACTERISTICS.
    Peng Yujiang
    Hong Yanruo
    Zhu Yuankai
    Jinshu Xuebao/Acta Metallurgica Sinica, 1982, 18 (04): : 456 - 462
  • [32] MASS-SPECTROMETRY MEASUREMENTS OF CAF2 AND CAO ACTIVITIES IN CAF2-CAO-AL2O3 SLAGS AT 1700 K
    ALLIBERT, M
    CHATILLON, C
    CANADIAN METALLURGICAL QUARTERLY, 1979, 18 (03) : 349 - 354
  • [33] Activity of SiO2 in CaO-SiO2-Al2O3-CaF2 slags.
    Gzielo, Antoni
    Jowsa, Jan
    Archiwum Hutnictwa, 1984, 29 (02): : 319 - 331
  • [34] Activity of SiO2 in CaO-SiO2-Al2O3 Molten Slags Containing CaF2 or B2O3 at 1450 °C
    Chen, Jian-Bin
    Pan, Wen-Bo
    Huang, Hong-Hong
    Chen, Zhi-Yu
    Zhao, Ming-Hui
    Sun, Ya-Qin
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2022, 53 (03): : 1526 - 1537
  • [35] Effects of B2O3 and CaF2 on melting properties of CaO-based slags
    Wang, Hong-ming
    Fu, De
    Li, Gui-rong
    Zhu, Xiang
    Zhao, Zhao
    Zhao, Yu-tao
    Zhu, Hua
    ADVANCED MATERIALS AND PROCESS TECHNOLOGY, PTS 1-3, 2012, 217-219 : 511 - 514
  • [36] Nitrogen Dissolution in CaO-SiO2-Al2O3-MgO-CaF2 Slags
    Baek, Seoung bae
    Lim, Jong ho
    Jung, Woo jin
    Lee, Seoung won
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2014, 24 (02): : 81 - 86
  • [37] MINERALOGY OF CaO-SiO2-FetO-P2O5(-MO, CaF2) SLAGS
    Diao, Jiang
    Xie, Bing
    METALURGIA INTERNATIONAL, 2012, 17 (10): : 65 - 71
  • [38] Stability of cuspidine (3CaO•2SiO2•CaF2) and phase relations in the CaO-SiO2-CaF2 system
    Watanabe, T
    Fukuyama, H
    Nagata, K
    ISIJ INTERNATIONAL, 2002, 42 (05) : 489 - 497
  • [39] Fluoride vaporization and crystallization of CaF2-CaO-Al2O3-(La2O3) slag for vacuum electroslag remelting
    Li, Tengfei
    Li, Guangqiang
    Zhang, Zhan
    Liu, Yu
    Wang, Xijie
    VACUUM, 2022, 196
  • [40] Activity of SiO2 in CaO–SiO2–Al2O3 Molten Slags Containing CaF2 or B2O3 at 1450 °C
    Jian-Bin Chen
    Wen-Bo Pan
    Hong-Hong Huang
    Zhi-Yu Chen
    Ming-Hui Zhao
    Ya-Qin Sun
    Metallurgical and Materials Transactions B, 2022, 53 : 1526 - 1537