Thermal cycling on microstructure and mechanical properties of laser powder bed fusion manufactured IN738LC alloy

被引:2
|
作者
Hu, Yong [1 ,2 ]
Jia, Hui-Bin [1 ,2 ]
Hu, Yong-Qi [1 ,2 ]
Chu, Cheng [1 ,2 ]
Zhang, Xu [1 ,2 ]
Wang, Li-Hua [1 ,2 ]
Zhang, Dong [3 ]
机构
[1] Lanzhou Univ Technol, Sch Mat Sci & Engn, Lanzhou 730050, Peoples R China
[2] Lanzhou Univ Technol, State Key Lab Adv Proc & Recycling Nonferrous Met, Lanzhou 730050, Peoples R China
[3] State Key Lab Nickel & Cobalt Resources Comprehens, Jinchang 737100, Peoples R China
关键词
Laser powder bed fusion (L-PBF); IN738LC alloy; Thermal cycling; Microstructure; Mechanical properties; MELTING SLM; PROCESS PARAMETERS; ENERGY DENSITY; HEAT-TREATMENT; EVOLUTION; TEMPERATURE; STRESS; STRENGTH; CARBIDES; POWER;
D O I
10.1007/s12598-024-02851-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study investigated the impact of thermal cycling effects on the microstructure and mechanical properties of IN738LC alloy manufactured by laser powder bed fusion, considering different volumetric energy densities (VEDs) and interlayer times (ILTs) as part of the experimental parameters. The results show that low VED and long ILT samples displayed superior quality, with an average grain size of 10.97 mu m and relatively low strain accumulation level. In contrast, samples with high VED and long ILT exhibit increased cracking and porosity, the average grain size is 14.63 mu m and present higher strain accumulation degree. The nano-primary MC phase within the alloy transformed into a spherical secondary MC phase inside the grain and a polygonal secondary MC phase on the grain boundary. In the low VED and long ILT, the mean equivalent diameter (MED) of MC carbide within the grain and on the grain boundary was 63 and 140 nm, respectively, the tensile strength was 1072 +/- 21 MPa. By contrast, for the high VED and long ILT, the MED of MC carbide in the grain and on the grain boundary were 47 and 105 nm, respectively, and the tensile strength was 794 +/- 31 MPa. The tensile strength of high VED and long ILT decreased by 26% compared with low VED and long ILT.
引用
收藏
页码:6649 / 6672
页数:24
相关论文
共 50 条
  • [31] Effect of processing parameters on the microstructure, mechanical properties and thermal expansion behavior of Invar 36 alloy manufactured by laser powder bed fusion
    Huang, Guoliang
    He, Gongming
    Peng, Xiaoqiang
    He, Yong
    Chen, Huan
    Huang, Ke
    Liu, Ying
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 897
  • [32] Fabrication and strengthening mechanism of crack-free nano-TiC reinforced IN738LC with enhanced mechanical properties by laser powder bed fusion
    Shu, Chang
    Chen, Siyuan
    Zheng, Zhiyu
    Lu, Xuben
    Li, Weining
    De Lisi, Michele
    Bidare, Prveen
    Shu, Xuedao
    Essa, Khamis
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 27 : 3835 - 3848
  • [33] Effect of adding IN718 on crack inhibition, microstructure, and mechanical properties of selective laser melted IN738LC alloy
    Wang, Chunxue
    Huang, Guoqiang
    Liang, Zhenkui
    Chen, Xin
    Wu, Jianhui
    Sun, Tao
    Meng, Fanqiang
    Mironov, Sergey
    Gao, Jicheng
    Zhao, Lin
    Feng, Xiaomei
    Shen, Yifu
    OPTICS AND LASER TECHNOLOGY, 2025, 185
  • [34] Microstructure and mechanical properties of crack-free Inconel 738 fabricated by laser powder bed fusion
    Jena, Ashutosh
    Atabay, Sila Ece
    Brochu, Mathieu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 850
  • [35] Effects of Y2O3 nanoparticles on the high-temperature oxidation behavior of IN738LC manufactured by laser powder bed fusion
    Guo, Chuan
    Yu, Zhengrong
    Liu, Chang
    Li, Xinggang
    Zhu, Qiang
    Ward, R. Mark
    CORROSION SCIENCE, 2020, 171
  • [36] Microstructure, mechanical properties and strengthening mechanisms of IN738LC alloy produced by Electron Beam Selective Melting
    Li, Yang
    Kan, Wenbin
    Zhang, Yanming
    Li, Mingzhi
    Liang, Xiaoyu
    Yu, Yefeng
    Lin, Feng
    ADDITIVE MANUFACTURING, 2021, 47
  • [37] Mechanical Properties of AlSi12 Alloy Manufactured by Laser Powder Bed Fusion Technique
    Masaaki Kimura
    Akihiro Hirayama
    Junya Yoshioka
    Hosei Maekawa
    Masahiro Kusaka
    Koichi Kaizu
    Tsuyoshi Takahashi
    Journal of Failure Analysis and Prevention, 2020, 20 : 1884 - 1895
  • [38] Mechanical Properties of AlSi12 Alloy Manufactured by Laser Powder Bed Fusion Technique
    Kimura, Masaaki
    Hirayama, Akihiro
    Yoshioka, Junya
    Maekawa, Hosei
    Kusaka, Masahiro
    Kaizu, Koichi
    Takahashi, Tsuyoshi
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2020, 20 (06) : 1884 - 1895
  • [39] Effect of Solid Solution Treatment on the Microstructure and Mechanical Properties of IN738LC Superalloy
    Kim, Jeong-Min
    Park, Joon-Sik
    Yun, Ho-Seob
    Lee, Seung-Jin
    An, Seong-Uk
    APPLIED MATERIALS AND ELECTRONICS ENGINEERING, PTS 1-2, 2012, 378-379 : 744 - +
  • [40] Nanoalloyed Al5254 alloy manufactured by powder bed fusion-laser beam: microstructure and mechanical properties analysis
    Stopyra, Wojciech
    Smolina, Irina
    Grochowska, Emilia
    Kobiela, Karol
    Karoluk, Michal
    Kasprowicz, Marcin
    Gruber, Konrad
    PROGRESS IN ADDITIVE MANUFACTURING, 2025, 10 (03) : 1701 - 1706