The negative effect of V content on high temperature oxidation resistance of austenitic stainless steels at 850 °C

被引:3
|
作者
Wang, Fan [1 ,2 ]
Zou, Dening [1 ]
Wang, Quansheng [2 ]
Zhang, Xiaoming [2 ]
Tong, Libo [1 ]
Liang, Xinliang [2 ]
Li, Yang [3 ]
Jiang, Yicheng [2 ]
机构
[1] Xian Univ Architecture & Technol, Sch Met & Engn, Xian 710055, Peoples R China
[2] Shaanxi Special Equipment Inspect & Testing Inst, Xian 710048, Peoples R China
[3] Taiyuan Iron & Steel Grp Co Ltd, Technol Ctr, Taiyuan 030003, Peoples R China
基金
中国国家自然科学基金;
关键词
Austenitic stainless steel; Vanadium content; High temperature oxidation; STRESS-CORROSION CRACKING; Z-PHASE; BEHAVIOR; MN; AL; 304-STAINLESS-STEEL; PRECIPITATION; MECHANISM; ALLOYS; NB;
D O I
10.1016/j.matchar.2024.113967
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of V on the high -temperature oxidation performance of austenitic stainless steel has been investigated by the constant -temperature oxidation weight gain approach, while the morphology, composition and elemental distribution of the oxide film are further analyzed by scanning electron microscopy and energy dispersive spectrum, transmission electron microscope and X-ray powder diffractometer as well as X-ray photoelectron spectroscopy, revealing the mechanism of the effect of V on the high -temperature oxidation performance of austenitic stainless steel. As a result, the addition of V has a significant adverse effect on the oxidation resistance of steel. Noteworthy, vanadium pentoxide generated during the oxidation process increases the internal stress of the surface oxide layer, reduces the integrity of the oxide layer and promotes oxygen penetration into the matrix. Simultaneously, the Z -phase formed at the grain boundaries of the matrix inhibits the diffusion of Cr ions, resulting in the inability to form an effective protective layer of Cr 2 O 3 oxidation on the surface.
引用
收藏
页数:9
相关论文
共 50 条
  • [31] Effect of TiN inclusions on oxidation behavior of austenitic stainless steels
    Zhu, Jia-Jie
    Jiang, Li
    Zhai, Li-Hong
    Zhou, Jian-Ming
    Ding, Xiang-Bin
    Li, Zhi-Jun
    MATERIALS LETTERS, 2023, 335
  • [32] Effect of Molybdenum on the Corrosion Resistance of Austenitic Stainless Steels.
    Defranoux, J.M.
    Materials Technology, 1974, 62 (03) : 137 - 143
  • [33] EFFECT OF CR ON PITTING RESISTANCE OF AUSTENITIC STAINLESS-STEELS
    BRIGHAM, RJ
    CORROSION SCIENCE, 1975, 15 (09) : 579 - 580
  • [34] ON THE INFLUENCE OF COLD WORK ON THE OXIDATION BEHAVIOR OF SOME AUSTENITIC STAINLESS-STEELS - HIGH-TEMPERATURE OXIDATION
    LANGEVOORT, JC
    FRANSEN, T
    GELLINGS, PJ
    OXIDATION OF METALS, 1984, 21 (5-6): : 271 - 284
  • [35] The effect of boron on cavitation resistance of FeCrMnSiB austenitic stainless steels
    Cruz, Juliane R.
    Henke, Sergio Luiz
    Pukasiewicz, Anderson G. M.
    d'Oliveira, Ana Sofia C. M.
    WEAR, 2019, 436
  • [36] Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels
    Zheng Chun
    Liu Jiabin
    Jiang Laizhu
    Yang Cheng
    Jiang Meixue
    ACTA METALLURGICA SINICA, 2022, 58 (02) : 193 - 205
  • [37] High temperature oxidation of duplex stainless steels
    Riquier, Y
    Zhang, H
    REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 2004, 101 (10): : 855 - +
  • [38] Oxidation protective barrier coatings for austenitic stainless steels at 1100°C
    Zhang, Zhong-li
    Wei, Peng-yao
    Zhang, Nan-nan
    Wang, Qi-shen
    Gong, Xue
    ADVANCED MATERIALS AND PROCESSES III, PTS 1 AND 2, 2013, 395-396 : 726 - 731
  • [39] Developing new cast austenitic stainless steels with improved high-temperature creep resistance
    Maziasz, Philip J.
    Shingledecker, John P.
    Evans, Neal D.
    Pollard, Michael J.
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE 2007, VOL 9, 2008, : 73 - 80
  • [40] STRESS CORROSION CRACKING RESISTANCE OF COMMERCIAL AUSTENITIC STAINLESS STEELS IN HIGH TEMPERATURE WATER.
    Kowaka, Masamichi
    Kobayashi, Taiki
    Kudo, Takeo
    Sumitomo Metals, 1978, 30 (01): : 93 - 101