Quantitative piezoelectric measurements of partially released Pb(Zr, Ti)O3 structures

被引:0
|
作者
Tipsawat, Pannawit [1 ]
Zheng, Xiaojun [2 ]
Tran, Quyen T. [2 ]
Jackson, Thomas N. [2 ]
Trolier-McKinstry, Susan [1 ]
机构
[1] Penn State Univ, Mat Res Inst, Dept Mat Sci & Engn, University Pk, PA 16802 USA
[2] Penn State Univ, Mat Res Inst, Ctr Thin Film Devices, Sch Elect Engn & Comp Sci, University Pk, PA 16802 USA
基金
美国国家航空航天局;
关键词
CRYSTAL ORIENTATION DEPENDENCE; BEAM LASER INTERFEROMETER; FERROELECTRIC THIN-FILMS; LEAD-ZIRCONATE-TITANATE; ETCHING DAMAGE; ELECTRIC-FIELD; PZT CERAMICS; TEMPERATURE; DISPLACEMENTS; PERFORMANCE;
D O I
10.1063/5.0215677
中图分类号
O59 [应用物理学];
学科分类号
摘要
The effective large signal longitudinal piezoelectric coefficient (d(33,f)(& lowast;)) of piezoelectric thin films on rigid substrates has been widely investigated. Unclamped piezoelectric thin films are predicted to have a higher d(33,f)(& lowast;) coefficient due to reduced constraints on piezoelectric strain, domain reorientation, and domain wall motion, but quantitative measurements of this coefficient have been limited. This study uses microfabrication techniques along with double-beam laser interferometry (DBLI) to accurately determine the longitudinal piezoelectric coefficient of Pb(Zr,Ti)O-3 thin films in partially released piezomicroelectro mechanical structures. A two-step backside release process was used: first, deep reactive ion etching to create backside vias and second, wet etching of the ZnO sacrificial layer to release the area beneath the Pb(Zr,Ti)O-3 thin films. Post wet etching, optical profilometry showed concavely deformed diaphragms resulting from asymmetrical stress profiles through the diaphragm thickness. DBLI was then used to examine diaphragm deflection under an applied unipolar voltage ranging from 0 to 10 V. Devices with 50% and 75% of the area beneath the top electrode released exhibited large signal d(33,f)(& lowast;) values of 410 +/- 6 and 420 +/- 8 pm/V, respectively, more than three times higher than the d(33,f)(& lowast;) value of the clamped samples: 126 +/- 13 pm/V. The reasons contributing to the large d(33,f)(& lowast;) include (i) the change in stress levels due to the release process, (ii) the elimination of mechanical constraints from substrate clamping, and (iii) enhanced domain reorientation. These findings confirm that substrate declamping significantly boosts the piezoelectric coefficient, bringing d(33,f)(& lowast;) closer to the bulk longitudinal piezoelectric coefficient (d(33)).
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Enhanced figure of merit in Pb(Zr,Ti)O3 nanorods for piezoelectric energy harvesting
    Song, Jundong
    Yamada, Tomoaki
    Okamoto, Kazuki
    Yoshino, Masahito
    Nagasaki, Takanori
    AIP ADVANCES, 2020, 10 (10)
  • [32] Piezoelectric properties and conductivity of Pb(Zr,Ti)O3 with SrO-WO3 additive
    Reichmann, Klaus
    Voelkl, Elmar
    Ahrens, Martin
    Fleig, Juergen
    Voetsch, Juergen
    JOURNAL OF MATERIALS SCIENCE, 2010, 45 (06) : 1473 - 1477
  • [33] Piezoelectric properties and conductivity of Pb(Zr,Ti)O3 with SrO–WO3 additive
    Klaus Reichmann
    Elmar Völkl
    Martin Ahrens
    Jürgen Fleig
    Jürgen Vötsch
    Journal of Materials Science, 2010, 45 : 1473 - 1477
  • [34] Compressive stress effect on the loss mechanism in a soft piezoelectric Pb(Zr,Ti)O3
    Daneshpajooh, H.
    Choi, M.
    Park, Y.
    Scholehwar, T.
    Hennig, E.
    Uchino, K.
    REVIEW OF SCIENTIFIC INSTRUMENTS, 2019, 90 (07):
  • [35] PROPERTIES OF PB(TI,ZR)O3 PIEZOELECTRIC CERAMICS AND NATURE OF THEIR ORIENTATIONAL DIELECTRIC POLARIZATION
    ISUPOV, VA
    SOVIET PHYSICS SOLID STATE,USSR, 1968, 10 (04): : 989 - +
  • [36] Fabrication and piezoelectric properties of Pb(Zr,Ti)O3 cubes synthesized by hydrothermal method
    Takada, Yoko
    Mimura, Ken-ichi
    Kato, Kazumi
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2018, 126 (05) : 326 - 330
  • [37] Ferroelectric performances and crystal structures of (Pb, La)(Zr, Ti, Nb)O3
    Kitamura, Naoto
    Mizoguchi, Takuma
    Itoh, Takanori
    Idemoto, Yasushi
    JOURNAL OF SOLID STATE CHEMISTRY, 2014, 210 (01) : 275 - 279
  • [38] Piezoelectric and ferroelectric properties in Ba(Zr,Ti)O3 and CuO-Ba(Zr,Ti)O3 ceramics
    Shin, Dong-Jin
    Kim, Jinhwan
    Jeong, Soon-Jong
    Koh, Jung-Hyuk
    MATERIALS RESEARCH BULLETIN, 2016, 82 : 7 - 10
  • [39] Pb loss in Pb(Zr,Ti)O3 ceramics observed by in situ ionic conductivity measurements
    Donnelly, Niall J.
    Randall, Clive A.
    JOURNAL OF APPLIED PHYSICS, 2011, 109 (10)
  • [40] Study of dielectric and piezoelectric properties of Pb(Ni,Nb)O3–Pb(Zr,Ti)O3 ceramics using mechanically activated powder
    O. P. Thakur
    Chandra Prakash
    Rakesh Kumar Sharma
    Journal of Materials Science, 2007, 42 : 6246 - 6251