Synergistic Leaching of Titanium, Aluminum, and Magnesium Components during Dilute Acid Pressure Treatment of High-Titanium Blast Furnace Slag

被引:1
|
作者
Yuan, Ke [1 ]
He, Siqi [1 ]
Yu, Bo [1 ]
Qian, Shiyi [1 ]
Wu, Xueyu [1 ]
Li, Wenyi [1 ]
Zhao, Chunmeng [1 ]
机构
[1] Mianyang Normal Univ, Sch Resources & Environm Engn, Mianyang 621000, Peoples R China
来源
MOLECULES | 2024年 / 29卷 / 14期
关键词
high-titanium blast furnace slag; dilute sulfuric acid; pressure; acid digestion; filtration; FUSION; FE; AL;
D O I
10.3390/molecules29143336
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
This study focuses on an improved leaching process through the combination of pressurized conditions and direct filtration of acid leaching slurry, which is conductive to improving the filterability of acid leaching systems and the extraction rates of Ti, Al, and Mg components. The effects of sulfuric acid concentration, reaction temperature, particle size of materials, acid-slag ratio, and reaction time on the leaching efficiency were systematically investigated. The results showed that pressurization significantly enhances the filtration efficiency of the reaction slurry. Under the same filtration time, the filtration efficiency increased from 46% under ordinary pressure to 78% under pressurized conditions. Moreover, under the optimal reaction conditions, the extraction rates of Ti, Al, and Mg components were more than 88.21%, 97.8%, and 96.31%, respectively. Additionally, XRD and FTIR showed that titanium oxide sulfate hydrate crystals were produced in the acid-leached residues when the reaction temperature exceeded 190 degrees C, thereby reducing the extraction rate of Ti component. And the XRD pattern shows that when the reaction temperature is maintained at 190 degrees C and the reaction time is extended to 150 min, titanium oxide sulfate hydrate crystals will be formed to reduce the extraction rate of the Ti component. In summary, this study not only provides important theoretical support for the resource utilization of high-titanium blast furnace slag but also offers a feasible solution for efficient extraction and convenient filtration, thus holding significant academic and practical implications.
引用
收藏
页数:17
相关论文
共 50 条
  • [1] Recovery of titanium, aluminum, magnesium and separating silicon from titanium-bearing blast furnace slag by sulfuric acid curing–leaching
    Long Wang
    Liang Chen
    Weizao Liu
    Guoquan Zhang
    Shengwei Tang
    Hairong Yue
    Bin Liang
    Dongmei Luo
    InternationalJournalofMinerals,MetallurgyandMaterials, 2022, (09) : 1705 - 1714
  • [2] Recovery of titanium, aluminum, magnesium and separating silicon from titanium-bearing blast furnace slag by sulfuric acid curing—leaching
    Long Wang
    Liang Chen
    Weizao Liu
    Guoquan Zhang
    Shengwei Tang
    Hairong Yue
    Bin Liang
    Dongmei Luo
    International Journal of Minerals, Metallurgy and Materials, 2022, 29 : 1705 - 1714
  • [3] Recovery of titanium, aluminum, magnesium and separating silicon from titanium-bearing blast furnace slag by sulfuric acid curing-leaching
    Wang, Long
    Chen, Liang
    Liu, Weizao
    Zhang, Guoquan
    Tang, Shengwei
    Yue, Hairong
    Liang, Bin
    Luo, Dongmei
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2022, 29 (09) : 1705 - 1714
  • [4] Leaching of Carbothermic Reduced Titanium-bearing Blast Furnace Slag by Acid
    ZHEN Yulan
    ZHANG Guohua
    CHOU Kuochih
    Journal of the Chinese Ceramic Society, 2016, 3 (01) : 1 - 8
  • [5] Preparation of Ti-rich Feedstock by Hydrochloric Acid Leaching of High Titanium Blast Furnace Slag
    Huo, Hong-ying
    Zou, Min
    2ND INTERNATIONAL CONFERENCE ON APPLIED MATHEMATICS, SIMULATION AND MODELLING (AMSM 2017), 2017, 162 : 523 - 526
  • [6] Effect of electric furnace steel slag powder on the strength of green low-carbon concrete with high-titanium blast furnace slag
    Liang, Yuehua
    Wang, Jie
    JOURNAL OF CO2 UTILIZATION, 2024, 89
  • [7] Effect of Basicity on the Viscosity and Phase Structure of Chromium-containing High-titanium Blast Furnace Slag
    Tian, Zhenyun
    Kang, Jialong
    Yang, Liu
    Wang, Jian
    Qiu, Guibao
    ISIJ INTERNATIONAL, 2025, 65 (03)
  • [8] Extraction of Valuable Metals from Titanium-bearing Blast Furnace Slag by Acid Leaching
    Liu, Yan
    Chen, Xuegui
    Mao, Shuaidong
    Xiao, Yadong
    Li, Jiacong
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2024, 39 (02): : 376 - 385
  • [9] Extraction of Valuable Metals from Titanium-bearing Blast Furnace Slag by Acid Leaching
    刘燕
    CHEN Xuegui
    MAO Shuaidong
    XIAO Yadong
    LI Jiacong
    JournalofWuhanUniversityofTechnology(MaterialsScience), 2024, 39 (02) : 376 - 385
  • [10] An approach towards utilization of water-quenched blast furnace slag for recovery of titanium, magnesium, and aluminum
    Ju, Jinrong
    Feng, Yali
    Li, Haoran
    Wu, Ruifeng
    Wang, Ben
    JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING, 2022, 10 (04):