Flatness warping of CRTS III track slabs during curing phase

被引:0
|
作者
Liu, Ran [2 ]
Wu, Jun [4 ]
Song, Li [1 ,2 ]
Cao, Jiwei [3 ]
Yu, Zhiwu [1 ,2 ]
机构
[1] Natl Engn Res Ctr High speed Railway Construct Tec, Changsha 410075, Peoples R China
[2] Cent South Univ, Sch Civil Engn, Changsha 410075, Peoples R China
[3] China Railway 9 Grp Co Ltd, Shenyang 110013, Liaoning, Peoples R China
[4] China Railway Grp Ltd, Beijing 100039, Peoples R China
基金
中国国家自然科学基金;
关键词
Excessive flatness warping deformation; Track slab curing; Improvement designs; The CRTS III track slab for high-speed railways; CEMENTITIOUS MATERIALS; MOISTURE DISTRIBUTION; AUTOGENOUS SHRINKAGE; DRYING SHRINKAGE; CONCRETE; ADSORPTION; DIFFUSION;
D O I
10.1016/j.conbuildmat.2024.137311
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
At present, there is a problem of excessive flatness warping in high-speed railway CRTS III type ballastless track slabs on certain railway lines. To analyze the evolution of flatness warping in track slabs and propose effective solutions, this study measured the compressive strength of the concrete used in track slabs, and the flatness warping of track slabs during the water curing and wet curing stages. A comparative experiment was also conducted to evaluate six improvement designs of track slabs. A model was developed to calculate the flatness warping of track slabs during the natural curing stage. The primary findings are as follows: (1) After the demoulding of the track slab, central upward arching deformation occurs at all stages due to the combined effects of drying shrinkage, thermal shrinkage, prestressing, and creep. The flatness warping generated during steam curing stage is a prerequisite; (2) During the curing phase, the primary factors causing excessive flatness warping in track slabs are drying shrinkage and thermal shrinkage; (3) The issue of excessive flatness warping of track slabs can be effectively resolved by employing secondary water spraying and setting a 0.5 mm reverse arch. Additionally, when the temperature is below 0degree celsius and the relative humidity is less than 0.55, it is necessary to apply insulation and moisturizing measures to the track slabs during the natural curing stage.
引用
收藏
页数:15
相关论文
共 50 条
  • [41] Calculation of reasonable-longitudinal-continuous length for bed plate of CRTS III slab ballastless track
    Cai, Xiao-Pei
    Zhao, Lei
    Gao, Liang
    Zhong, Yang-Long
    Lau, Albert
    Jiaotong Yunshu Gongcheng Xuebao/Journal of Traffic and Transportation Engineering, 2016, 16 (01): : 55 - 62
  • [42] Experimental study on evolution of mechanical properties of CRTS III ballastless slab track under fatigue load
    Zeng Zhi-ping
    Wang Jun-dong
    Shen Shi-wen
    Li Ping
    Shuaibu, Abdulmumin Ahmed
    Wang Wei-dong
    CONSTRUCTION AND BUILDING MATERIALS, 2019, 210 : 639 - 649
  • [43] A further understanding on the strength development of cement pastes in the presence of triisopropanolamine used in CRTS III slab track
    Zhang, Yanrong
    Zhang, Xuesong
    Cai, Xiaopei
    Gao, Liang
    Li, Qiangqiang
    Kong, Xiangming
    CONSTRUCTION AND BUILDING MATERIALS, 2022, 315
  • [44] Study on the time-varying tensile reliability of CRTS III ballastless track plate in cold region
    Li, Longxiang
    Ren, Juanjuan
    Deng, Shijie
    Zhang, Yichi
    Zhao, Huawei
    Journal of Railway Science and Engineering, 2024, 21 (10) : 4027 - 4039
  • [45] Durability study of CRTS III slab ballastless track under the combined effects of fatigue damage and carbonation
    Song, Li
    Chen, Libing
    Zhu, Maodong
    Wang, Lian
    Hou, Jian
    CONSTRUCTION AND BUILDING MATERIALS, 2025, 469
  • [46] Insights of the vehicle-track-girder system dynamic response changes caused by the thermal deformation of CRTS III ballastless track in the natural environment
    Zhou, Li
    Zhang, Tianqi
    Luo, Yanyun
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 400
  • [47] Study on the effect of CRTS III ballastless track caused by angular settlement in transition section between bridge and subgrade
    Lou P.
    Huang G.
    Journal of Railway Science and Engineering, 2023, 20 (04) : 1292 - 1303
  • [48] Research on Target Localization Method of CRTS-III Slab Ballastless Track Plate Based on Machine Vision
    Liu, Xinjun
    Wu, Wenjiang
    Zheng, Liaomo
    Wang, Shiyu
    Zhang, Qiang
    Wang, Qi
    ELECTRONICS, 2021, 10 (23)
  • [49] Temperature field and thermal effect analysis of CRTS III ballastless track structure under the outdoor natural environment
    Liu, Hubing
    Song, Li
    Liu, Ran
    Yu, Zhiwu
    CONSTRUCTION AND BUILDING MATERIALS, 2022, 358
  • [50] Dynamic effects and structure optimization of damping layers of CRTS III slab ballastless track for high speed railway
    Xin T.
    Zhang Q.
    Gao L.
    Zhao L.
    Qu J.
    Zhongguo Tiedao Kexue/China Railway Science, 2016, 37 (05): : 1 - 7