Mechanism of Directional Reduction Strengthening of Nickel Laterite Ore Under Fluidization Condition

被引:0
|
作者
Zheng, Siqi [1 ,2 ]
Wang, Xiaofang [1 ,2 ]
Qin, Guotao [1 ,2 ]
Zhu, Zhiping [1 ,2 ]
机构
[1] Chinese Acad Sci, Inst Engn Thermophys, State Key Lab Coal Convers, 11 North Fourth Ring Rd West, Beijing 100190, Peoples R China
[2] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
关键词
MAGNETIC SEPARATION; SELECTIVE REDUCTION; SODIUM-SULFATE; IRON; TRANSFORMATION; FERRONICKEL; KINETICS; OXIDE;
D O I
10.1007/s11663-024-03311-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The nickel laterite ore-fluidized reduction roasting technology is a clean and efficient metallurgical. To achieve the nickel enrichment effect, accomplish the controlled reduction of nickel and iron, and reduce nickel to the metallic state while controlling the metallization rate of iron, it is necessary to carry out experimental studies on the directional selective reduction of it. This study investigated the effects of temperature, additive amount, and reductant type on the selective reduction effect of nickel-iron oxides in nickel laterite ore with an iron grade of 24.30 pct and nickel grade of 1.45 pct. The physical phase, micro-morphology, and valence changes of nickel-iron elements of the reduced samples were also analyzed in depth by combining XRD, SEM-EDS, XPS, et al. The results showed that the best reduction effect of H2 was achieved at the reduction temperature of 800 degrees C and the reduction time of 60 minutes, and the metallization rates of nickel and iron were 95.96 and 14.85 pct, respectively, under this condition. The selective reduction of nickel laterite by Na2SO4 was apparent. The appropriate amount of Na2SO4 has a more significant increase in the metallization rate of nickel in the mixed gas atmosphere, roasting at 800 degrees C for 60 minutes. When the addition of Na2SO4 is 6 pct, the metallization rate of nickel reaches a maximum of 92.05 pct; when the Na2SO4 increases from 0 to 8 pct, the nickel grade reaches a maximum of 3.65 pct, and the recovery of nickel reaches a maximum of 87.78 pct. The XRD results show that the addition of Na2SO4 destroys the olivine phase in nickel laterite ore, which allows the nickel stored therein to be released to participate in the reaction, thus increasing the rate of nickel metallization. This study provides theoretical support for the further application of fluidized roasting technology on nickel laterite ore smelting.
引用
收藏
页码:4929 / 4941
页数:13
相关论文
共 50 条
  • [41] Carbothermic Selective Reduction of Laterite Nickel Ore by Addition of Sulfur and Sodium Hydroxide to Produce Ferronickel
    Setiawan, Iwan
    Triana, Tiara
    Febriana, Eni
    Firdiyono, F.
    PROCEEDINGS OF THE 3RD INTERNATIONAL SEMINAR ON METALLURGY AND MATERIALS (ISMM 2019): EXPLORING NEW INNOVATION IN METALLURGY AND MATERIALS, 2020, 2232
  • [42] Carbothermic Reduction Roasting of a Low-Grade Nickel Laterite Ore in the Modified Caron Process
    Ilyas, Sadia
    Kim, Hyunjung
    Srivastava, Rajiv Ranjan
    5TH INTERNATIONAL SYMPOSIUM ON NICKEL AND COBALT (NI-CO 2021), 2021, : 317 - 328
  • [43] Carbothermal Reduction of Stainless Steel Dust and Laterite Nickel Ore: Slag Phase Behavior Regulation and Self-pulverization Control Mechanism
    Liu, Peijun
    Liu, Zhenggen
    Chu, Mansheng
    Yan, Ruijun
    Li, Feng
    Tang, Jue
    ISIJ INTERNATIONAL, 2023, 63 (03) : 586 - 595
  • [44] The reduction of nickel from low-grade nickel laterite ore using a solid-state deoxidisation method
    Li, Bo
    Wang, Hua
    Wei, Yonggang
    MINERALS ENGINEERING, 2011, 24 (14) : 1556 - 1562
  • [45] Influence mechanism of different types of coal on selective nickle reduction in nickel laterite reduction roasting
    Sun, Ti-Chang
    Ji, Ya-Na
    Jiang, Man
    Beijing Keji Daxue Xuebao/Journal of University of Science and Technology Beijing, 2011, 33 (10): : 1197 - 1203
  • [46] Separation and recovery of iron and nickel from low-grade laterite nickel ore by microwave carbothermic reduction roasting
    Zhang, Junhong
    Gao, Lihua
    He, Zhijun
    Hou, Xinmei
    Zhan, Wenlong
    Pang, Qinghai
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (06): : 12223 - 12235
  • [47] Sulfur Removal and Iron Extraction from Natrojarosite Residue of Laterite Nickel Ore Processing by Reduction Roasting
    Zulhan, Zulfiadi
    Adzana, Zhahrina
    Munawaroh, Mona
    Yusro, Achmad Haerul
    Christian, Jonathan Dwiputra
    Saputri, Aura Dwi
    Hidayat, Taufiq
    METALS, 2023, 13 (01)
  • [48] Multiobjective collaborative optimization of novel carbothermal reduction process of stainless steel dust and laterite nickel ore
    Liu, Pei-jun
    Liu, Zheng-gen
    Chu, Man-sheng
    Yan, Rui-jun
    Li, Feng
    Tang, Jue
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2023, 33 (06) : 1919 - 1931
  • [49] Influence of laterite nickel ore on extracting iron from Bayer red mud by carbothermal smelting reduction
    Ao-ping He
    Jian-min Zeng
    Shi-hong Liu
    Journal of Iron and Steel Research International, 2021, 28 : 661 - 668
  • [50] Kinetic study of the reduction reaction of red mud and CO under fluidization condition
    Kong, Hao
    Zhou, Tuo
    Wang, Zhe
    Li, Chaoran
    Zhang, Man
    Yang, Hairui
    ASIA-PACIFIC JOURNAL OF CHEMICAL ENGINEERING, 2024, 19 (03)