In the present investigation a wrought magnesium alloy (AZ31) has been processed applying the accumulative back extrusion (ABE) method. This was performed through different thermomechanical processing routes (different ABE deformation passes at temperatures of 80-380 degrees C). The results indicate that AZ31 alloy may successfully be deformed through ABE processing even at temperatures as low as 80 degrees C. Following the ABE processing a sophisticated microhardness testing was conducted and thorough microstructural observations were undertaken using optical microscopy. The results show that the equiaxed submicron size grains have been achieved. As the number of passes was increased, a more homogeneous microstructure with finer mean grain size was obtained. It was also found that increasing the temperature resulted in larger mean grain size and also higher microstructural homogeneity. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:1334 / 1339
页数:6
相关论文
共 50 条
  • [21] Deformation mechanisms of AZ31 magnesium alloy
    Ebeling, T.
    Hartig, Ch.
    Laser, T.
    Nuernberg, M. R.
    Bormann, R.
    MAGNESIUM TECHNOLOGY 2008, 2008, : 41 - +
  • [22] DEFORMATION BEHAVIOUR OF AZ31 MAGNESIUM ALLOY
    Lukac, Pavel
    Balik, Jaroslav
    Trojanova, Zuzanka
    METAL 2011: 20TH ANNIVERSARY INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2011, : 915 - 919
  • [23] The effect of deformation processing on tensile ductility of magnesium alloy AZ31
    Zuberova, Z.
    Sabirov, I.
    Estrin, Y.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2011, 49 (01): : 29 - 36
  • [24] Influence of different deformation processing on the AZ31 magnesium alloy sheets
    Su-Qin Zhu
    Hong-Ge Yan
    Wei-Jun Xia
    Ji-Zi Liu
    Jun-Feng Jiang
    Journal of Materials Science, 2009, 44 : 3800 - 3806
  • [25] Influence of different deformation processing on the AZ31 magnesium alloy sheets
    Zhu, Su-Qin
    Yan, Hong-Ge
    Xia, Wei-Jun
    Liu, Ji-Zi
    Jiang, Jun-Feng
    JOURNAL OF MATERIALS SCIENCE, 2009, 44 (14) : 3800 - 3806
  • [26] EXPERIMENTAL STUDY OF ULTRAFINE-GRAINED COMMERCIAL MAGNESIUM ALLOY AZ31 PREPARED BY SEVERE PLASTIC DEFORMATION METHOD
    Vratna, Jitka
    Janecek, Milos
    METAL 2013: 22ND INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2013, : 1603 - 1607
  • [27] Effect of Severe Plastic Deformation on Microstructure of Squeeze-cast Magnesium Alloy AZ31 Plate
    Fong, Kai Soon
    Tan, Ming Jen
    Atsushi, Danno
    Chua, Beng Wah
    Ho, Meng Kwong
    PROCEEDINGS OF THE 19TH INTERNATIONAL ESAFORM CONFERENCE ON MATERIAL FORMING (ESAFORM 2016), 2016, 1769
  • [28] Effect of grain refinement on the strength and corrosion of AZ31 magnesium alloy following severe plastic deformation
    Eliezer, D.
    Ben Hamu, G.
    Cross, C. E.
    Bollinghaus, Th.
    Magnesium Technology 2006, Proceedings, 2006, : 261 - 264
  • [29] A new Approach for Inverse Parameter Calculations of the Plastic Deformation Behavior of AZ31 Magnesium Alloy
    Ebeling, T.
    Hartig, Ch.
    Bormann, R.
    MAGNESIUM TECHNOLOGY 2009, 2009, : 531 - 535
  • [30] Thermal microstructural stability of AZ31 magnesium after severe plastic deformation
    Young, J. P.
    Askari, H.
    Hovanski, Y.
    Heiden, M. J.
    Field, D. P.
    MATERIALS CHARACTERIZATION, 2015, 101 : 9 - 19