- [43] Effect of joining temperature and holding time on microstructure and shear strength of Ti2AlC/Cu joints brazed using Ag-Cu filler alloy MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 567 : 58 - 64
- [44] Effect of in-situ synthesized TiB whiskers on interfacial microstructure and shear strength of γ-TiAl joint vacuum brazed with TiH2-Ni-TiB2 fillers MATERIALS TODAY COMMUNICATIONS, 2024, 38
- [45] The effect of temperature on microstructureu and mechanical behavior of the vacuum brazed joint of Ti-46.5Al-5Nb alloy and 42CrMo steel PRICM 5: THE FIFTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-5, 2005, 475-479 : 829 - 832
- [46] Effect of brazing temperature on microstructure and mechanical properties of Si3N4/Si3N4 joints brazed with Ag–Cu–Ti + Mo composite filler Journal of Materials Science, 2011, 46 : 2796 - 2804