Numerical and experimental investigation on flexural properties of selective laser melting (SLM) manufactured strut lattices structures from Ti-6Al-4V and Inconel 625

被引:0
|
作者
Condruz, Mihaela Raluca [1 ]
Badea, Teodor Adrian [1 ]
Paraschiv, Alexandru [1 ]
机构
[1] Romanian Res & Dev Inst Gas Turbines COMOTI, 220D Iuliu Maniu Ave, Bucharest 061126, Romania
来源
关键词
Lattice structures; Three-point bending; Finite element analysis; Microstructure; Selective laser melting; MICROSTRUCTURE EVOLUTION; HEAT-TREATMENTS; ALLOY; BEHAVIOR;
D O I
10.1016/j.mtcomm.2024.110150
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Lattice structures hold a significant importance in the aerospace industry due to their ability to tailor the physical, thermal, and mechanical properties of complex components for optimal performance. This study is focused on evaluating the flexural properties of four lattice configurations - re-entrant, truncated octahedron, Kelvin, and octet cells - through static finite element analysis (FEA) and experimental three-point bending tests, as well as examining their microstructural features (as they affect the materials' mechanical properties). Highperformance alloys used for gas turbines components manufacturing, Ti-6Al-4 V and Inconel 625, were fabricated using selective laser melting (SLM) process. The necessity of this research resulted from the lack of information in the scientific literature regarding flexural properties of various additive manufactured cell types and metallic materials. The aim was to compile data that could be used to create a comprehensive database for various industrial applications. Findings from both simulations and experimental analyses indicated that the octet cell had the highest performance, with experimentally measured flexural strengths of 878 MPa for Ti-6Al4V, respective 674 MPa for Inconel 625. Contrarily, the re-entrant cell exhibited the lowest performance, with flexural strengths of 125 MPa for Ti-6Al-4V and 116 MPa for Inconel 625. Failure in the re-entrant cells was attributed to the bending fracture of vertical rods at the connecting nodes or lattice struts, while other cell types experienced damage through a combination of bending and shear mechanisms. Dimensional deviations observed in all specimens were attributed to defects such as surface roughness, the stair-stepping effect, and internal stresses.
引用
收藏
页数:16
相关论文
共 50 条
  • [21] Additive Manufactured Ti-6Al-4V Alloy with Graded Microstructure by Selective Laser Melting
    利用选区激光熔化技术制备梯度结构的Ti-6Al-4V合金
    Chen, Chao (pkhqchenchao@126.com), 1600, Science Press (50): : 3543 - 3549
  • [22] Investigation of Ti-6Al-4V alloy in situ manufactured using selective laser melting from elemental powder mixture
    Polozov I.
    Sufiiarov V.
    Popovich A.
    Solid State Phenomena, 2020, 299 : 646 - 651
  • [23] Microstructure, Mechanical Properties, and Constitutive Models for Ti-6Al-4V Alloy Fabricated by Selective Laser Melting (SLM)
    Tao, Pan
    Zhong, Jiangwei
    Li, Huaixue
    Hu, Quandong
    Gong, Shuili
    Xu, Qingyan
    METALS, 2019, 9 (04):
  • [24] The Transverse Rupture Strength in Ti-6Al-4V Alloy Manufactured by Selective Laser Melting
    Lai, Pang-Hsin
    Chen, Jhewn-Kuang
    Wu, Ming-Wei
    2015 4TH INTERNATIONAL CONFERENCE ON ENGINEERING AND INNOVATIVE MATERIALS (ICEIM 2015), 2015, 27
  • [25] Optimisation of single contour strategy in selective laser melting of Ti-6Al-4V lattices
    Cao, Xue
    Carter, Luke Nelson
    Villapun, Victor Manuel
    Cantaboni, Francesco
    De Sio, Giulia
    Lowther, Morgan
    Louth, Sophie Elizabeth Thompson
    Grover, Liam
    Ginestra, Paola
    Cox, Sophie Constance
    RAPID PROTOTYPING JOURNAL, 2022, 28 (05) : 907 - 915
  • [26] A Numerical Study on the Mesoscopic Characteristics of Ti-6Al-4V by Selective Laser Melting
    Ao, Xiaohui
    Liu, Jianhua
    Xia, Huanxiong
    Yang, Ye
    MATERIALS, 2022, 15 (08)
  • [27] Investigation on influence of selective laser melting parameters on mechanical properties of Ti-6Al-4V alloy
    Kumar, Mandeep
    Nabi, Jahangir
    Singh, Harsimran Jeet
    Kaundal, Hemant
    Bera, Tarun Kumar
    Singh, Ratnesh Kumar Raj
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART C-JOURNAL OF MECHANICAL ENGINEERING SCIENCE, 2025, 239 (01) : 117 - 128
  • [28] Microstructure and tensile properties of Ti-6Al-4V alloys manufactured by selective laser melting with optimized processing parameters
    Wang, L.
    Ma, C.
    Huang, J.
    Ding, H. Y.
    Chu, M. Q.
    2017 INTERNATIONAL CONFERENCE ON MATERIAL ENGINEERING AND MANUFACTURING (ICMEM 2017), 2017, 265
  • [29] Evaluation of fatigue crack propagation behaviour in Ti-6Al-4V manufactured by selective laser melting
    Walker, K. F.
    Liu, Q.
    Brandt, M.
    INTERNATIONAL JOURNAL OF FATIGUE, 2017, 104 : 302 - 308
  • [30] Microstructure and Mechanical Properties of Ti-6Al-4V Fabricated by Selective Laser Melting
    Simonelli, Marco
    Tse, Yau Yau
    Tuck, Christopher
    TMS 2012 141ST ANNUAL MEETING & EXHIBITION - SUPPLEMENTAL PROCEEDINGS, VOL 1: MATERIALS PROCESSING AND INTERFACES, 2012, : 863 - 870