Mechanical and Corrosion Properties of Super Austenitic Stainless Steel Joint for Double-Sided Synchronous TIP TIG Arc Butt Welding

被引:1
|
作者
Wang, Lulu [1 ]
Lang, Zeyu [1 ]
Tan, Long [1 ]
机构
[1] Qingdao Univ Sci & Technol, Coll Electromech Engn, Qingdao 266061, Shandong, Peoples R China
关键词
254SMO super austenitic stainless steel; corrosion resistance; double-sided double-arc synchronous TIP TIG butt welding; mechanical properties; CHI-PHASE; 10CRNI3MOV STEEL; SIGMA-PHASE; MICROSTRUCTURE; ALUMINUM; BEHAVIOR; PASSIVATION;
D O I
10.1002/srin.202400295
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Super austenitic stainless steel 254SMO (254SMO SASS) plates are joined by double-sided double-arc synchronous TIP TIG butt welding (DSSTTABW) using ER NiCrMo3 wire, and the micro-structure, mechanical and corrosion properties of 254SMO SASS joints are investigated subsequently. Results show that solidification grain boundary and solidification sub-grain boundary can be observed in fusion zone. A small amount of sigma phase precipitates in the weld, while chi phase is found in the transition zone, but no solidification crack occurs in weld and heat affected zone (HAZ). 254SMO SASS joint has higher micro-hardness and lower tensile strength and elongation compared to base metal. During transverse tensile process, 254SMO SASS joints fail in the weld zone in a ductile mode. Electrochemical corrosion performance tests indicate that 254SMO SASS joint achieve equivalent pitting corrosion resistance and similar passive mechanism to base metal in 3.5 wt% NaCl solution. The passivation film on the surface of both joint and base metal display as n-p semi-conductive character, but the film stability of 254SMO joint surface is slightly poorer compared to base material. The surface passivation film of 254SMO joint primarily consists of oxides of Fe, Cr, and Mo before potentiodynamic polarization, while hydroxides of Fe and Cr are also observed after polarization. Double-sided synchronous TIP TIG arc welding was introduced to butt joint 4 mm thick 254SMO super austenitic stainless steel without groove. Sound joint with excellent appearance, mechanical and corrosion properties was achieved. The passive film of 254SMO joint and base metal both display as n-p semi-conductive character, which consists of metal oxides and hydroxides of Cr and Mo.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:10
相关论文
共 50 条
  • [41] Influence of heat input on the intermetallic compound characteristics and fracture mechanisms of titanium-stainless steel MIG-TIG double-sided arc welding joints
    Cheng, Zhi
    Ye, Zheng
    Huang, Jihua
    Yang, Jian
    Chen, Shuhai
    Zhao, Xingke
    INTERMETALLICS, 2020, 127
  • [42] Effects of TIG Process on Corrosion Resistance of 321 Stainless Steel Welding Joint
    Hu, Dan
    Li, Shulin
    Lu, Sheng
    MATERIALS PERFORMANCE, MODELING AND SIMULATION, 2013, 749 : 173 - 179
  • [43] Effect of shielding gases on microstructure and mechanical properties of super austenitic stainless steel by hybrid welding
    Sathiya, P.
    Mishra, Mahendra Kumar
    Shanmugarajan, B.
    MATERIALS & DESIGN, 2012, 33 : 203 - 212
  • [44] Effect of multipass TIG welding on the corrosion resistance and microstructure of a super duplex stainless steel
    Hosseini, V. A.
    Hurtig, K.
    Karlsson, L.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2017, 68 (04): : 405 - 415
  • [45] Effect of axial misalignment on the microstructure, mechanical, and corrosion properties of magnetically impelled arc butt welding joint
    Lv, Shanhui
    Liu, Hongbing
    Wang, Fei
    Liu, Xu
    Peng, Mingjian
    Wei, Yinjin
    Li, Chunsi
    MATERIALS TODAY COMMUNICATIONS, 2024, 40
  • [46] Microstructures and Hardness Profile of Asymmetric Double-sided Double Arc Welding for High Strength Steel
    Huang, Gen-zhe
    Liu, Shuang-yu
    Liu, Feng-de
    Zhang, Hong
    2015 INTERNATIONAL CONFERENCE ON MATERIALS AND ENGINEERING AND INDUSTRIAL APPLICATIONS (MEIA 2015), 2015, : 91 - 97
  • [47] Microstructure and mechanical properties of flash butt welding high carbon martensitic stainless steel M390 and austenitic stainless steel 304
    Cao R.
    Qiao L.
    Che H.
    Li S.
    Wang T.
    Dong H.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2022, 43 (02): : 27 - 33
  • [48] Thermal cycle and microstructure of backing weld in double-sided TIG arc horizontal welding of high-strength steel thick plate
    Xiong, Jun
    Liu, Shuyi
    Zhang, Guangjun
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2015, 81 (9-12): : 1939 - 1947
  • [49] Microstructure and mechanical properties of a thick-section high-strength steel welded joint by novel double-sided hybrid fibre laser-arc welding
    Chen, Yanbin
    Feng, Jiecai
    Li, Liqun
    Chang, Shuai
    Ma, Guolong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 582 : 284 - 293
  • [50] Thermal cycle and microstructure of backing weld in double-sided TIG arc horizontal welding of high-strength steel thick plate
    Jun Xiong
    Shuyi Liu
    Guangjun Zhang